# US 2002/0055252 A1 · Method for shrinking critical dimension

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0055252 A1
- Document ID: US20020055252A1
- Status: Published application
- Kind: A1
- Application number: 09/903,667
- Filed: 2001-07-13
- Published: 2002-05-09
- Earliest claimed: 2000-11-09
- Assignees: Macronix International Co., Ltd.
- Inventors: Ching-Yu Chang
- Web page: https://patentgrep.com/patent/US20020055252A1

## CPC

- H10P 76/4085: {characterised by the processes involved to create the masks}
- G03F 7/40: Treatment after imagewise removal, e.g. baking
- H10P 76/2041: {Photolithographic processes}
- H10P 76/4088: {Processes for improving the resolution of the masks}
- H10W 20/089: {using processes for implementing desired shapes or dispositions of the openings, e.g. double patterning}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In accordance with the present invention, a method is provided for shrinking critical dimension in semiconductor processes. This method comprises a step of performing an over-exposure process to a photosensitive layer to form a patterned photosensitive layer on a substrate by using a patterned reticle. Due to the unexposed region of the photosensitive layer being diminished by over-exposure the critical dimension is shrunk. Then, a sacrificial layer is applied for the purpose of pattern reverse-transferring. Next, the patterned photosensitive layer is removed such that the pattern is transferred to the sacrificial layer with a shrunk critical dimension. In cooperation of the present exposure technology with the present invention, the shrinkage of a critical dimension is accomplished, for example, using an I-line exposure light source in a critical dimension of 0.25 μm process, or using a deep UV (ultraviolet) exposure light source in a critical dimension of 0.13 μm process.

## Claims

### Claim 1

A method for shrinking a critical dimension by over-exposure, said method comprising:
forming a photosensitive layer on a substrate;
providing a patterned reticle with a pattern to align with said substrate;
performing an over-exposure process to said photosensitive layer to form a patterned photosensitive layer by using said patterned reticle;
forming a sacrificial layer on said substrate and said patterned photosensitive layer;
anisotropically etching said sacrificial layer to expose said patterned photosensitive layer; and
removing said patterned photosensitive layer to reverse transferring said pattern to said sacrificial layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said photosensitive layer is formed by spin coating.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said pattern is selected from the group consisting of a spacing, a line width, and a contact hole.

### Claim 4 (depends on 1)

The method according to claim 1, wherein said step of performing said over-exposure process increases an exposed region and shrinks an unexposed region of said photosensitive layer.

### Claim 5 (depends on 4)

The method according to claim 4, wherein said unexposed region is a region of shrinking said critical dimension.

### Claim 6 (depends on 1)

The method according to claim 1, wherein said photosensitive layer is selected from the group consisting of a positive photoresist and a negative photoresist.

### Claim 7 (depends on 1)

The method according to claim 1, wherein said sacrificial layer is selected from the group consisting of an oxide layer, a nitride layer, a phosphosilicate glass (PSG) layer, a borophosphosilicate glass (BPSG) layer, a photosensitive material layer, and a polymer layer.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said step of forming said sacrificial layer is selected from the group consisting of spin coating said sacrificial layer, depositing said sacrificial layer, and sputtering said sacrificial layer.

### Claim 9

A method for shrinking a critical dimension by over-exposure, said method comprising:
forming a photosensitive layer on a substrate;
providing a patterned reticle with a pattern to align with said substrate;
performing an over-exposure process to said photosensitive layer to form a patterned photosensitive layer by using said patterned reticle, wherein said over-exposure process increases an exposed region and shrinks an unexposed region of said photosensitive layer, wherein said unexposed region is a region of shrinking said critical dimension;
forming a sacrificial layer on said substrate and said patterned photosensitive layer;
anisotropically etching said sacrificial layer to expose said patterned photosensitive layer; and
removing said patterned photosensitive layer to reverse transferring said pattern to said sacrificial layer.

### Claim 10 (depends on 9)

The method according to claim 9, wherein said pattern is selected form the group consisting of a spacing, a line width, and a contact hole.

### Claim 11 (depends on 9)

The method according to claim 9, wherein said photosensitive layer is selected from the group consisting of a positive photoresist and a negative photoresist.

### Claim 12 (depends on 9)

The method according to claim 9, wherein said sacrificial layer is selected from the group consisting of an oxide layer, a nitride layer, a phosphosilicate glass (PSG) layer, a borophosphosilicate glass (BPSG) layer, a photosensitive material layer, and a polymer layer.

### Claim 13 (depends on 9)

The method according to claim 9, wherein said step of forming said sacrificial layer is selected from the group consisting of spin coating said sacrificial layer, depositing said sacrificial layer, and sputtering said sacrificial layer.

### Claim 14

A method for shrinking a critical dimension in semiconductor process, said method comprising:
spin-coating a photosensitive layer on a substrate;
providing a reticle to align with said substrate, wherein said reticle has a pattern;
performing an over-exposure process to transfer said pattern to said photosensitive layer to form an exposed region and an unexposed region in said photosensitive layer, wherein said exposed region of said photosensitive layer is increased and said unexposed region of said photosensitive layer is shrunk;
performing a development process to form a patterned photosensitive layer;
forming a sacrificial layer on said substrate and said patterned photosensitive layer;
etching back said sacrificial layer to expose said patterned photosensitive layer; and
removing said patterned photosensitive layer to reverse transferring said pattern to said sacrificial layer.

### Claim 15 (depends on 14)

The method according to claim 14, wherein said photosensitive layer is selected from the group consisting of a positive photoresist and a negative photoresist.

### Claim 16 (depends on 14)

The method according to claim 14, wherein said pattern is selected from the group consisting of a spacing, a line width, and a contact hole.

### Claim 17 (depends on 14)

The method according to claim 14, wherein said sacrificial layer is selected from the group consisting of an oxide layer, a nitride layer, a phosphosilicate glass (PSG) layer, a borophosphosilicate glass (BPSG) layer, a photosensitive material layer, and a polymer layer.

### Claim 18 (depends on 14)

The method according to claim 14, wherein said step of forming said sacrificial layer is selected from the group consisting of spin coating said sacrificial layer, depositing said sacrificial layer, and sputtering said sacrificial layer.

### Claim 19 (depends on 14)

The method according to claim 14, wherein said step of etching back said sacrificial layer comprises anisotropically etching said sacrificial layer.