Solder ball and method for producing same
AssigneeHitachi Metals, Ltd.
InventorsKoji Sato, Takeshi Kuboi, Masayoshi Date
Life of this patent
Estimating the term…
Loading patent…
AssigneeHitachi Metals, Ltd.
InventorsKoji Sato, Takeshi Kuboi, Masayoshi Date
Estimating the term…
A solder ball having a diameter of 1.2 mm or less, a dispersion of a diameter distribution of 5% or less and sphericity of 0.95 or more, an area ratio of the maximum dendrite being 80% or less of a cross section including a center of the solder ball, comprises a first additional element of 0.5-8 mass% of Ag and/or 0.1-3 mass % of Cu, and 0.006-10 mass %, in total, of at least one second additional element selected from the group consisting of Bi, Ge, Ni, P, Mn, Au, Pd, Pt, S, In and Sb, the balance being substantially Sn. The solder ball is produced by a uniform droplet-spraying method comprising the steps of vibrating a melt of a solder alloy in a crucible under pressure to force the melt to drop through orifices of the crucible; permitting the melt dropping through the orifices to become spherical droplets in a non-oxidizing gas atmosphere; and rapidly solidifying them.
A solder ball prepared by a uniform droplet-spraying method, said solder ball has a carbon-concentrated layer of 1 nm or less in thickness and an oxygen-concentrated layer of 5 nm or less in thickness on a surface thereof.
A solder ball, wherein an area ratio of the maximum dendrite is 80% or less of a cross section including a center of said solder ball.
A method for producing solder balls comprising the steps of vibrating a melt of a solder alloy in a crucible under pressure to force said melt to drop through orifices of said crucible;