# US 2002/0012746 A1 · High throughput high-yield vacuum deposition system for thin film based dense wavelength division multiplexers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0012746 A1
- Document ID: US20020012746A1
- Status: Published application
- Kind: A1
- Application number: 09/902,250
- Filed: 2001-07-10
- Published: 2002-01-31
- Earliest claimed: 2000-07-10
- Assignees: Atomic Telecom
- Inventors: Gerald T. Mearini; Laszlo Takacs
- Web page: https://patentgrep.com/patent/US20020012746A1

## CPC

- C23C 14/546: {using crystal oscillators}
- B82Y 10/00: Nanotechnology for information processing, storage or transmission, e.g. quantum computing or single electron logic
- C23C 14/22: characterised by the process of coating
- C23C 14/505: {for rotation of the substrates}
- G02B 6/29361: {Interference filters, e.g. multilayer coatings, thin film filters, dichroic splitters or mirrors based on multilayers, WDM filters}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS

## Abstract

A vacuum deposition system has been designed to produce thin film based demultiplexers with high throughput and production yields of greater than 25% for use in Dense Wavelength Division Multiplexer (DWDM) systems. The system employs a dense array of high yield fixtures and an ion assisted movable dual electron beam evaporation system. The fixture array increases acceptable yields of narrow band pass filters to 25-75% compared to less than 5% in conventional coating systems used for DWDM. The movable e-beam system allows critical symmetry to be maintained while eliminating significant delays resulting from deposition of two materials from a single electron gun. The vacuum deposition system will enable production of more than 15,000 50-200 GHZ filters which meet specifications for DWDM demultiplexers every 48 hours.

## Claims

### Claim 1

An ion-assisted electron beam evaporation process, the process comprising the steps of:
positioning multiple high yield fixtures in an array;
adjusting a vertical position of each of the fixtures to compensate for variations in deposition rate versus chamber location;
providing two electron guns;
mounting the guns to a movable track;
positioning the first gun at a source deposition location;
rotating the fixtures at greater than 2400 rpm;
performing ion assisted evaporation with the first gun, the second gun being kept in a stand-by location in pre-heat mode;
ceasing deposition prior to achieving target thickness;
shuttering each of the fixtures at different times;
independently reopening the fixtures to a low rate pulsed deposition to achieve the target thickness;
closing clam shutters on the fixtures;
moving the first gun to a stand-by position;
moving the second gun to the source deposition location;
sampling evaporation with a quartz crystal thickness monitor;
opening a shutter on the second gun;
performing ion assisted evaporation with the second gun, the first gun being kept in a stand-by location in pre-heat mode;
ceasing deposition prior to achieving target thickness;
shuttering each of the fixtures at different times;
independently reopening the fixtures to a low rate pulsed deposition to achieve the target thickness;
closing clam shutters on the fixtures; and,
repeating the process until desired filter is obtained.

### Claim 2

A method for producing an optical filter utilizing line-of-sight deposition, the method comprising the steps of:
providing multiple substrates;
providing a fixed ion source;
providing at least one selectively movable evaporator;
positioning the at least one evaporator at a source deposition location; and,
depositing material onto the substrates.

### Claim 3 (depends on 2)

The method of claim 2, wherein the method further comprises the step of:
shuttering the substrates as necessary to ensure uniform deposition on the substrates.

### Claim 4 (depends on 3)

The method of claim 3, where in the method further comprises the step of:
rotating the substrates at approximately greater than 500 revolutions per minute.

### Claim 5 (depends on 4)

The method of claim 4, wherein shuttering the substrates as necessary to ensure uniform deposition on the substrates comprises the steps of:
ceasing deposition of a layer prior to achieving target thickness;
shuttering the substrates at different times;
independently unshuttering the substrates; and,
achieving the target thickness.

### Claim 6 (depends on 2)

The method of claim 2, wherein the at least one evaporator is at least two selectively movable evaporators, the method further comprising the steps of:
moving the first evaporator to a stand-by position;
opening a shutter on the second evaporator;
positioning the second evaporator at the source deposition location; and,
performing ion assisted evaporation with the second evaporator.

### Claim 7 (depends on 6)

The method of claim 6, wherein the method further comprises the steps of:
ceasing deposition of a layer prior to achieving target thickness;
shuttering the substrates at different times;
independently unshuttering the substrates; and,
achieving the target thickness.

### Claim 8 (depends on 7)

The method of claim 7, wherein after moving the second evaporator into the source deposition location, the method comprises the step of:
sampling evaporation with a quartz crystal thickness monitor.

### Claim 9 (depends on 8)

The method of claim 8, wherein the method further comprises the steps of:
closing clam shutters on the substrates; and,
repeating the process until desired filter is obtained.

### Claim 10 (depends on 9)

The method of claim 9, wherein providing multiple substrates comprises the step of:
providing a dense high yield fixture array having multiple, independently shutterable fixtures, each of the fixtures containing multiple substrates.

### Claim 11

A system for producing optical filters, the system comprising:
multiple substrates;
an ion source;
at least two selectively movable evaporators; and,
a source deposition location.

### Claim 12 (depends on 11)

The system of claim 11, wherein the system further comprises:
shuttering means for shuttering the substrates; and,
a vacuum chamber.

### Claim 13 (depends on 12)

The system of claim 12, wherein the substrates are rotated at approximately greater than 500 revolutions per minute.

### Claim 14 (depends on 13)

The system of claim 13, wherein the substrates are attached to high yield fixtures, the fixtures being independently shutterable.

### Claim 15 (depends on 14)

The system of claim 14, wherein the fixtures rotate and are adjustable.

### Claim 16 (depends on 15)

The system of claim 15, wherein the system further comprises:
a quartz crystal thickness monitor.

### Claim 17 (depends on 16)

The system of claim 16, wherein the evaporators are connected to a movable track, the movable track being opposite the fixtures in the vacuum chamber.

### Claim 18 (depends on 17)

The system of claim 17, wherein the vacuum chamber is approximately 60 inches by 80 inches.

### Claim 19 (depends on 2)

An optical filter produced by the method of claim 2.

### Claim 20 (depends on 4)

The method of claim 4, wherein rotating the substrates at greater than 500 revolutions per minute comprises the step of:
rotating the substrates at greater than 2400 revolutions per minute.

### Claim 21 (depends on 13)

The system of claim 13, wherein the substrates are rotated at greater than 2400 revolutions per minute.