# US 2002/0001948 A1 · Method of manufacturing a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0001948 A1
- Document ID: US20020001948A1
- Status: Published application
- Kind: A1
- Application number: 09/875,624
- Filed: 2001-06-06
- Published: 2002-01-03
- Earliest claimed: 2000-06-28
- Assignees: Hyundai Electronics Industries Co., Ltd.
- Inventors: In Haeng Lee
- Web page: https://patentgrep.com/patent/US20020001948A1

## CPC

- H10D 64/259: {Source or drain electrodes being self-aligned with the gate electrode and having bottom surfaces higher than the interface between the channel and the gate dielectric}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of manufacturing a semiconductor device in a salicide process to lower a contact resistance between a junction and a metal wiring, wherein a TiSi2 layer is formed on the junction at the same time when Ti is deposited by means of a plasma vapor deposition method using TiCl4 gas and H2 gas. Therefore, the method can simplify the process and reduce the amount of consumption of silicon atoms in the junction, compared to the conventional salicide process by which a TiSi2 layer is formed by annealing process after Ti is deposited, thus realizing a stable leakage current characteristic.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, comprising the steps of:
providing a semiconductor substrate for forming a TiSi2 layer; and
simultaneously forming a TiSi2 layer on said substrate and depositing Ti on said substrate by a plasma vapor deposition method using TiCl4 gas and H2 gas.

### Claim 2 (depends on 1)

The method of claim 1, comprising the step of forming said TiSi2 layer under a power of about 100 Watts to about 500 Watts, a pressure in the range of about 2 Torr to about 20 Torr, and a temperature of the semiconductor device is in the range of about 400° C. to about 700° C.

### Claim 3 (depends on 1)

The method of claim 1, comprising the step of flowing the TiCl4 gas at a rate of about 10 mg/min to about 100 mg/min and flowing the H2 gas at a rate of about 1000 sccm to about 3000 sccm, to form said TiSi2 layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein said plasma vapor deposition method employs Ar as an inert gas at a flow rate of about 100 sccm to about 5000 sccm, in addition to said TiCl4 and H2 gases used to form said TiSi2 layer.

### Claim 5

A method of manufacturing a semiconductor device, comprising the steps of:
providing a semiconductor substrate defining a device separation film, a gate having two sidewalls, and a junction having an exposed surface;
forming a mask insulating film on said gate and forming a gate spacer at both sidewalls of said gate;
forming a silicon layer on the exposed surface of said junction;
forming a TiSi2 layer on said silicon layer and substantially simultaneously depositing Ti on the silicon layer by a plasma vapor deposition method using TiCl4 gas and H2 gas; and
removing any unreacted Ti layer after said TiSi2 layer is formed.

### Claim 6 (depends on 5)

The method of claim 5, comprising the step of forming said silicon layer by a selective epitaxial growth method.

### Claim 7 (depends on 5)

The method of claim 5, comprising the step of using at least one of SiH4, SiH2Cl2, SiHCl3, and SiCl4 as a reaction gas in said selective epitaxial growth method.

### Claim 8 (depends on 5)

The method of claim 5, comprising the step of forming said TiSi2 layer under a power of about 100 Watts to about 500 Watts, a pressure in the range of about 2 Torr to about 20 Torr, and a temperature of the semiconductor substrate is in the range of about 400° C. to about 700° C.

### Claim 9 (depends on 5)

The method of claim 5, comprising the step of flowing the TiCl4 gas at a rate of about 10 mg/min to about 100 mg/min and flowing the H2 gas at a rate of about 1000 sccm to about 3000 sccm, to form said TiSi2 layer.

### Claim 10 (depends on 5)

The method of claim 5, wherein said plasma vapor deposition method employs Ar as an inert gas at a flow rate of about 100 sccm to about 5000 sccm, in addition to said TiCl4 and H2 gases used to form said TiSi2 layer.

### Claim 11 (depends on 11)

The method of claim 11, further including a step of annealing said TiSi2 layer after removing the unreacted Ti layer.

### Claim 12 (depends on 11)

The method of claim 11, comprising the step of performing the annealing at a temperature of about 700° C. to about 900° C. to change the phase of said TiSi2 layer into C54 phase.