# US 2002/0001946 A1 · Method and fabricating metal interconnection with reliability using ionized physical vapor deposition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0001946 A1
- Document ID: US20020001946A1
- Status: Published application
- Kind: A1
- Application number: 09/892,536
- Filed: 2001-06-28
- Published: 2002-01-03
- Earliest claimed: 2000-06-30
- Inventors: Won-Jun Lee
- Web page: https://patentgrep.com/patent/US20020001946A1

## CPC

- H10W 20/038: {covering conductive structures (H10W20/037 takes precedence)}
- H10P 14/418: {the conductive layers comprising transition metals}
- H10P 14/43: Chemical deposition, e.g. chemical vapour deposition [CVD]
- H10P 14/44: Physical vapour deposition [PVD]
- H10W 20/045: {for deposition from the gaseous phase, e.g. for chemical vapour deposition [CVD]}
- H10W 20/425: {Barrier, adhesion or liner layers}
- H10W 20/0375: {comprising multiple stacked thin barrier, adhesion or liner layers not being formed in openings in dielectrics}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a multilayer metal thin film capable of improving electromigration reliability. The method includes steps of forming a Ti film having an <002> crystal orientation by using an ionized physical vapor deposition method, forming a TiN film on the Ti film in order to form a multilayer stack, wherein the TiN film has an <111> crystal orientation, and forming an aluminum film on the multilayer stack in an <111> crystal orientation. Accordingly, the aluminum metal interconnection increases the <002> orientation of the Ti film and improves the <111> orientation of the aluminum to control electromigration resistance, by using the IPVD method in forming the Ti film as an underlayer of the aluminum film.

## Claims

### Claim 1

A method for forming a multilayer metal thin film in a semiconductor device, comprising steps of:
forming a Ti film having an <002> crystal orientation by using an ionized physical vapor deposition method;
forming a TiN film on the Ti film in order to form a multilayer stack, wherein the TiN film has an <111> crystal orientation; and
forming an aluminum film on the multilayer stack in an <111> crystal orientation.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the ionized physical vapor deposition method uses any one of a radio frequency coil, a hollow cathode and a magnetron and applies AC bias to a processing chamber in order to increase a directness of the ionized atoms from a Ti target.

### Claim 3 (depends on 2)

The method as recited in claim 2, wherein the JPVD method uses a radio frequency coil.

### Claim 4 (depends on 3)

The method as recited in claim 3, wherein an AC bias of 0 to 500 W is applied to a wafer, on which the multilayer metal thin film is formed, at a pressure of 1 to 100 mtorr and a DC bias of 0.5 to 5 kW is applied to the radio frequency coil.

### Claim 5 (depends on 1)

The method as recited in claim 1, wherein the Ti film is formed at a thickness of approximately 50 to 500 Å.

### Claim 6 (depends on 1)

The method as recited in claim 1, wherein the TiN film is formed by a PVD (Physical Vapor Deposition), MOCVD (Metal Organic Chemical Vapor Deposition) or IPVD method and the TiN film is formed at a thickness of approximately 50 to 500 Å.

### Claim 7 (depends on 1)

The method as recited in claim 1, wherein the aluminum film is formed by a PVD (Physical Vapor Deposition) or CVD (Chemical Vapor Deposition) method.

### Claim 8 (depends on 7)

The method as recited in claim 7, wherein a precursor to form the aluminum film in the CVD method is one of DMAH (CH3)2AlH, DMEAA (AlH3N(CH3)2(C2H5), and their mixtures.

### Claim 9 (depends on 8)

The method as recited in claim 8, wherein the aluminum film is formed at a temperature of 150 to 300° C. and in a processing chamber having a pressure of 1 to 100 torr.

### Claim 10

A method for forming a multilayer metal thin film in a semiconductor device, comprising steps of:
forming a first Ti film using an ionized physical vapor deposition method;
forming a TiN film on the first Ti film;
forming a second Ti film on the TiN film to increase an <111> crystal orientation of a refractory metal to be formed on the second Ti film; and
forming an aluminum film on the second Ti film.

### Claim 11 (depends on 10)

The method as recited in claim 10, wherein the second Ti film has an <002> orientation and wherein the second Ti film is formed by a PVD (Physical Vapor Deposition) or IPVD (Ionized Physical Vapor Deposition) method.

### Claim 12 (depends on 10)

The method as recited in claim 10, wherein the second Ti film is formed at a thickness of approximately 50 to 500 Å.

### Claim 13 (depends on 10)

The method as recited in claim 10, further comprising a step of forming a tungsten film on the TiN film.

### Claim 14 (depends on 10)

The method as recited in claim 10, wherein the ionized physical vapor deposition method uses any one of a radio frequency coil, a hollow cathode and a magnetron and applies AC bias of 0 to 500 W to a processing chamber.

### Claim 15 (depends on 14)

The method as recited in claim 14, wherein the IPVD method uses a radio frequency coil.

### Claim 16 (depends on 15)

The method as recited in claim 15, wherein an AC bias of 0 to 500 W is applied to a wafer, on which the multilayer metal thin film is formed, at a pressure of 1 to 100 mtorr and a DC bias of 0.5 to 5 kW is applied to the radio frequency coil.

### Claim 17 (depends on 10)

The method as recited in claim 10, wherein the first Ti film is formed at a thickness of approximately 50 to 500 Å.

### Claim 18 (depends on 10)

The method as recited in claim 10, wherein the TiN film is formed by a PVD (Physical Vapor Deposition), MOCVD (Metal Organic Chemical Vapor Deposition) or IPVD method and wherein the TiN film is formed at a thickness of approximately 50 to 500 Å.

### Claim 19 (depends on 10)

The method as recited in claim 10, wherein the aluminum film is formed by a PVD or CVD method.

### Claim 20 (depends on 10)

The method as recited in claim 10, wherein a precursor to form the aluminum film in a CVD method is one of DMAH (CH3)2AlH, DMEAA (AlH3N (CH3)2(C2H5), and their mixtures.

### Claim 21 (depends on 20)

The method as recited in claim 20, wherein the aluminum film is formed at a temperature of 150 to 300° C. and in a processing chamber having a pressure of 1 to 100 torr.