# US 2002/0001932 A1 · Method for forming a gate for semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0001932 A1
- Document ID: US20020001932A1
- Status: Published application
- Kind: A1
- Application number: 09/895,268
- Filed: 2001-07-02
- Published: 2002-01-03
- Earliest claimed: 2000-06-30
- Assignees: Hynix Semiconductor Inc.
- Inventors: Heung Jae Cho; Dae Gyu Park; Kwan Yong Lim
- Web page: https://patentgrep.com/patent/US20020001932A1

## CPC

- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10D 64/01344: {in a nitrogen-containing ambient, e.g. N2O oxidation}
- H10D 64/685: {being perpendicular to the channel plane}
- H10D 64/693: {the insulator comprising nitrogen, e.g. nitrides, oxynitrides or nitrogen-doped materials}
- H10P 14/6322: {Formation by thermal treatments (formation by plasma treatment H10P14/6319)}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6538: {by exposure to UV light}
- H10P 14/6544: {to change the morphology of the insulating materials, e.g. transformation of an amorphous layer into a crystalline layer}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention discloses a method for forming a gate for semiconductor devices by depositing a TaOxNy film as a gate oxide film. The method includes the steps of providing a semiconductor substrate where a device isolation film has been formed, growing an SiO2 or SiON film on the semiconductor substrate, depositing an amorphous TaOxNy film on the SiO2 or SiON film, performing a low temperature annealing process to improve quality of the amorphous TaOxNy film, performing a high temperature annealing process ex-situ to remove organic substances and nitrogen in the amorphous TaOxNy film, and crystallize the amorphous TaOxNy film, and depositing a metal barrier film on the crystallized TaOxNy film, and depositing a polysilicon film or metal film for a gate electrode on the metal barrier film.

## Claims

### Claim 1

A method for forming a gate for semiconductor devices, comprising the steps of:
providing a semiconductor substrate;
forming one of a SiO2 film and a SiON film on the semiconductor substrate;
forming an amorphous TaOxNy film on the one of the SiO2 and SiON films;
performing a low temperature annealing process on the amorphous TaOxNy film;
crystallizing the amorphous TaOxNy film by performing a high temperature annealing process; and
forming one of a polysilicon film and a metal film on the crystallized TaOxNy film.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the one of the SiO2 film and the SiON film is formed by performing a rapid thermal process at a temperature between about 700° C. and 1100° C. in an atmosphere of one of O2 gas and N2O gas.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the deposited one of the SiO2 film and the SiON film has a thickness of below about 15 Å.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the amorphous TaOxNy film is deposited at a temperature between about 300° C. and 500° C. by a metal organic chemical vapor deposition using Ta(C2H5O)5 and NH3.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the deposited amorphous TaOxNy film has a thickness between about 20 Å and 500 Å.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the low temperature annealing process is performed at a temperature between about 300° C. and 500° C. by applying about 100 W power, exciting an N2O gas in a chamber using plasma.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the low temperature annealing process is performed by exciting O2 or O3 at a temperature between about 300° C. and 500° C. for about 10 to 30 minutes using UV.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising a step for removing oxygen vacancies and organic substances in the TaOxNy film, by depositing the amorphous TaOxNy film with a thickness of about 20 Å to 150 Å on the amorphous TaOxNy film where the low temperature annealing process has been carried out, and by performing an annealing process by exciting an N2O gas in a chamber, using plasma or exciting O2 or O3 using UV.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the high temperature annealing process is performed ex-situ at a temperature between about 700° C. and 1000° C. for about 60 seconds in an atmosphere of one of N2O and O2 by a rapid thermal process.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the high temperature annealing process is performed ex-situ at a temperature between about 700° C. and 100° C. for about 60 seconds in an atmosphere of one of N2O and O2 in a furnace of an oxidizing atmosphere.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the metal film is one of a TiSi2 film, a WSix film and a W film.

### Claim 12

A method for forming a gate for semiconductor devices, comprising the steps of:
providing a semiconductor substrate;
forming one of a SiO2 film and a SiON film on the semiconductor substrate;
forming an amorphous TaOxNy film on the one of the SiO2 film and the SiON film;
performing a low temperature annealing process on the amorphous TaOxNy film by using plasma or UV;
removing oxygen vacancies and organic substances in the amorphous TaOxNy film;
crystallizing the amorphous TaOxNy film by performing a high temperature annealing process;
forming a metal barrier film on the crystallized TaOxNy film; and
forming one of a polysilicon film and a metal film on the metal barrier film.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the deposited one of the SiO2 film and the SiON film has a thickness of below about 15 Å.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the deposited amorphous TaOxNy film has a thickness between about 20 Å and 500 Å and is deposited at a temperature between about 300° C. and 500° C. by a metal organic chemical vapor deposition using Ta(C2H5O)5 and NH3.

### Claim 15 (depends on 12)

The method according to claim 12, wherein the low temperature annealing process is performed at one of:
a temperature between about 300° C. and 500° C. by applying about 100 W power, exciting an N2O gas in a chamber, and using plasma; and
a temperature between about 300° C. and 500° C. for about 10 to 30 minutes exciting one of O2 or O3 by using UV.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the high temperature annealing process is performed ex-situ at a temperature between about 700° C. and about 1000° C. for about 60 seconds in an atmosphere of one of N2O and O2 by a rapid thermal process and a furnace of an oxidizing atmosphere.

### Claim 17 (depends on 12)

The method according to claim 12, wherein the metal barrier film is one of a TiN film and WN film.

### Claim 18 (depends on 12)

The method according to claim 12, wherein the metal film is elected from one of a TiSi2 film, a WSix film and a W film.

### Claim 19

A method for forming a gate for semiconductor devices, comprising the steps of:
providing a semiconductor substrate;
forming one of a SiO2 film and a SiON film on the semiconductor substrate;
forming an amorphous TaOxNy film on the one of the SiO2 and SiON films;
performing a low temperature annealing process on the amorphous TaOxNy film;
crystallizing the amorphous TaOxNy film by performing a high temperature annealing process; and
forming a metal barrier film on the crystallized TaOxNy film; and
forming one of a polysilicon film and a metal film on the metal barrier film.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the metal barrier film is one of a TiN film and a WN film.