# US 2002/0001858 A1 · Method of manufacturing a capacitor in a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0001858 A1
- Document ID: US20020001858A1
- Status: Published application
- Kind: A1
- Application number: 09/852,602
- Filed: 2001-05-10
- Published: 2002-01-03
- Earliest claimed: 2000-06-28
- Assignees: Hyundai Electronics Industries Co., Ltd.
- Inventors: Kyong Min Kim; Han Sang Song; Dong Jun Kim
- Web page: https://patentgrep.com/patent/US20020001858A1

## CPC

- H10D 1/684: {the dielectrics comprising multiple layers, e.g. comprising buffer layers, seed layers or gradient layers}
- H10D 1/042: {using deposition processes to form electrode extensions}
- H10D 1/716: {having vertical extensions}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6538: {by exposure to UV light}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10P 14/69397: {the material containing two or more metal elements}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing a capacitor in a semiconductor device uses a metal as an upper electrode and a lower electrode, and forms a dielectric film in a double structure of a titanium-containing tantalum oxide film and an amorphous tantalum oxide film. Therefore, the invention can secure a sufficient capacitance while improving an electrical characteristic of the capacitor.

## Claims

### Claim 1

A method of manufacturing a capacitor in a semiconductor device, comprising the steps of:
providing a semiconductor substrate in which a predetermined structure is formed;
forming a plug and a diffusion prevention film on said substrate to form an entire structure;
depositing a Ru film on the entire structure;
thereafter patterning said Ru film to form a lower electrode;
forming a titanium-containing tantalum oxide film on the entire structure;
thereafter performing an annealing process;
forming an amorphous tantalum oxide film on said titanium-containing tantalum oxide film; and
depositing a metal layer on the entire structure to form an upper electrode.

### Claim 2 (depends on 1)

The method of claim 1, wherein said Ru film has a thickness of about 100 Å to about 500Å, and is formed by introducing gaseous tris (2,4-octanedionato) ruthenium into a reaction furnace within which a pressure of about 0.1 Torr to about 10 Torr is maintained, said furnace containing a wafer, and heating the wafer to about 200° C. to about 350° C.

### Claim 3 (depends on 2)

The method of claim 2, comprising the steps of introducing oxygen or NH3 to the furnace at a rate of about 5 sccm to about 1000 sccm as the reaction gas for forming said Ru film.

### Claim 4 (depends on 1)

The method of claim 1, wherein said titanium-containing tantalum oxide film is formed by providing gaseous tantalum ethylate and introducing oxygen or titanium at a rate of about 1 sccm to about 200 sccm, to a reaction furnace containing a wafer, and heating the wafer to a temperature of about 300° C. to about 400° C.

### Claim 5 (depends on 4)

The method of claim 4, comprising the step of maintaining said reaction furnace at a pressure of about 0.1 Torr to about 1.2 Torr.

### Claim 6 (depends on 4)

The method of claim 4, comprising the step of introducing oxygen at a flow rate of about 10 sccm to about 1000 sccm.

### Claim 7 (depends on 4)

The method of claim 4, comprising the step of introducing titanium at a flow rate of about 1 sccm to about 200 sccm.

### Claim 8 (depends on 1)

The method of claim 1, wherein said annealing process comprises a step of performing a N2O plasma or UV/03 process at a temperature of about 300° C. to about 500° C., and a step of performing a rapid annealing process or a reaction furnace annealing process using N2 gas and 02 gas at a temperature of about 500° C. to about 700° C.

### Claim 9 (depends on 1)

The method of claim 1, comprising the step of forming said amorphous tantalum oxide film by introducing gaseous tantalum ethylate (Ta(OC2H5)5) and oxygen at a flow rate of about 10 sccm to about 1000 sccm to a reaction furnace containing a wafer, and heating the wafer to a temperature of about 300° C. to about 400° C.

### Claim 10 (depends on 1, 9)

The method of claim 9, comprising the step of maintaining said reaction furnace at a pressure of about 0. 1 Torr to about 1.2 Torr. 11. The method of claim 1, wherein said upper electrode comprises a Ru film or aTiN film.