# US 2002/0001678 A1 · Method for damping noise, vibration and harshness of a substrate and composition therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0001678 A1
- Document ID: US20020001678A1
- Status: Published application
- Kind: A1
- Application number: 09/915,727
- Filed: 2001-07-26
- Published: 2002-01-03
- Earliest claimed: 1998-06-18
- Inventors: Ralph J. Locke; Daniel W. Irvine
- Web page: https://patentgrep.com/patent/US20020001678A1

## CPC

- C08G 18/6685: {with compounds of group C08G18/3225 or polyamines of C08G18/38}
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C08J 7/043: Improving the adhesiveness of the coatings per se, e.g. forming primers (adhesives in the form of films or foils characterised by the primer layers between the polymer carriers and the adhesives C09J7/50)
- C08J 7/046: Forming abrasion-resistant coatings; Forming surface-hardening coatings
- C09D 175/02: Polyureas
- C08G 2350/00: Acoustic or vibration damping material
- C08J 2475/00: Characterised by the use of polyureas or polyurethanes; Derivatives of such polymers
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

A method for damping vibration of a substrate comprises the step of applying a liquid material onto the substrate in an ambient environment, wherein, after application to the substrate, the material cures substantially instantaneously in the ambient environment. The damping composition usable therefor comprises a resin component and an isocyanate component. The resin component includes a polymer(s) for imparting tensile strength, hardness and flexibility; an optional chain extender(s) for imparting tensile strength, weatherability, flexibility, adhesion to specific substrates, and hardness; and an optional filler for imparting hardness, flexibility, and specific noise, vibration and harshness blocking characteristics to the after-application, cured surface. The isocyanate component of the composition includes an isocyanate quasi-prepolymer(s) based on a uretonimine modified MDI and a high molecular weight polyether polyol having an isocyanate equivalent content of 15.8% and a 2,4′-isomer content of less than about 15%; and an optional plasticizer(s) for imparting flexibility.

## Claims

### Claim 1

A method for damping vibration of a substrate comprising the steps of:
providing a substrate;
mixing at least two components to form a liquid material, wherein the first component consists essentially of at least one amine-terminated polymer present in an amount sufficient to impart a predetermined amount of tensile strength, hardness and flexibility, and the second component consists essentially of at least one isocyanate compound, the first and second components reacting upon mixing; and
applying the liquid material to the substrate at ambient temperature.

### Claim 2 (depends on 1)

The method as defined in claim 1 wherein the ambient environment has a temperature ranging between about 35° F. (1.7° C.) and about 160° F. (71.1° C.).

### Claim 3 (depends on 2)

The method as defined in claim 2 wherein the ambient environment has a temperature ranging between about 50° F. (10° C.) and about 120° F. (48.9° C.).

### Claim 4 (depends on 1)

The method as defined in claim 1 wherein the ambient environment has a pressure ranging between about 730 mm Hg and about 800 mm Hg.

### Claim 5 (depends on 4)

The method as defined in claim 4 wherein the ambient environment has a pressure ranging between about 750 mm Hg and about 780 mm Hg.

### Claim 6 (depends on 1)

The method as defined in claim 1 wherein the material cures in an interval ranging between about 2 seconds and about 30 minutes.

### Claim 7 (depends on 6)

The method as defined in claim 6 wherein the material cures in an interval ranging between about 15 seconds and about 20 seconds.

### Claim 8 (depends on 1)

The method as defined in claim 1 wherein the substrate is at least one of a metal stamping, a body in white, carbon graphite composites, fiberglass, polycarbonates, ABS, and structural polymeric materials.

### Claim 9 (depends on 8)

The method as defined in claim 8 wherein the substrate is a body in white.

### Claim 10 (depends on 1)

The method as defined in claim 1 wherein the applying step is performed by at least one of spraying, dipping and brushing.

### Claim 11 (depends on 10)

The method as defined in claim 10 wherein the applying step is performed by a high pressure, impingement mix spray system.

### Claim 12 (depends on 9)

The method as defined in claim 9 wherein the vibration damped includes at least one of noise, vibration and harshness.

### Claim 13

A method for damping vibration of a substrate comprising the steps of:
providing a substrate;
mixing at least two components to form a liquid material, wherein the first component consists essentially of at least one polyoxalene polymer present in an amount sufficient to impart a predetermined amount of tensile strength, hardness and flexibility, and the second component consists essentially of at least one isocyanate compound, the first and second components reacting upon mixing; and
applying the liquid material to the substrate at ambient temperature.

### Claim 14 (depends on 13)

The method as defined in claim 13 wherein the first component further consists essentially of:
at least one chain extender present in an amount sufficient to impart a predetermined amount of tensile strength, weatherability, flexibility, adhesion to specific substrates, and hardness; and
at least one filler present in an amount sufficient to impart a predetermined amount of hardness, flexibility, and specific vibration blocking characteristics to the substrate.

### Claim 15 (depends on 14)

The method as defined in claim 14 wherein the first component further consists essentially of:
a colorant compound selected from the group consisting of carbon black, titanium dioxide, iron oxide, organic pigments, dyes, and mixtures thereof, and
a catalyst selected from the group consisting of tertiary amines, organometallic catalysts, and mixtures thereof.

### Claim 16 (depends on 13)

The method as defined in claim 13 wherein the at least one polyoxalene polymer is selected from the group consisting of polyoxypropylene diols, polyoxypropylene triols, di-, tri-, quad- or penta-functional polyester polyols, di-, tri-, quad- or penta-functional polyether polyols, and mixtures thereof.

### Claim 17 (depends on 13)

The method as defined in claim 13 wherein the isocyanate compound consists essentially of isocyanate quasi-prepolymers based on a uretonimine modified MDI and a high molecular weight polyether polyol having an isocyanate content of about 15.8% and a 2,4′-isomer content of less than about 10%.

### Claim 18 (depends on 13)

The method as defined in claim 13 wherein the second component further consists essentially of at least one plasticizer present in an amount sufficient to impart a predetermined amount of flexibility.

### Claim 19 (depends on 18)

The method as defined in claim 18 wherein the plasticizer consists essentially of alkylene carbonates selected from the group consisting of ethylene carbonates, propylene carbonates, butylene carbonates, dimethyl carbonates, and mixtures thereof.

### Claim 20

A method for damping vibration of a substrate comprising the steps of:
providing a substrate,
mixing at least two components to form a liquid material, the first and second components reacting upon mixing;
wherein the first component consists essentially of at least one amine terminated polyoxalene polymer present in an amount sufficient to impart a predetermined amount of tensile strength, hardness and flexibility, and the second component consists essentially of at least one isocyanate compound having at least one-NCO radical reactive with the first component; and
applying the liquid material to the substrate at ambient temperature, the liquid material cures substantially instantaneously.

### Claim 21 (depends on 20)

The method as defined in claim 20 wherein the further consists essentially of:
at least one chain extender selected from the group consisting of dialkyl substituted methylene dianilines, diethyltoluene diamines, and mixtures thereof; and
at least one filler is selected from the group consisting of barium sulfate, calcium carbonate, clay, talc, aluminum silicate, titanium dioxide, nitrile rubbers, butyl rubbers, synthetic rubbers, chopped fiberglass, calcium metasilicate, fibers, fumed silica, and mixtures thereof.

### Claim 22 (depends on 20)

The method as defined in claim 20 wherein the amine terminated polyoxalene polymer has a molecular weight between about 1000 and about 6000.

### Claim 23 (depends on 20)

The method as defined in claim 20 wherein the first component of the composition further consists essentially of at least one adhesion promoter, wherein the adhesion promoter comprises an organosilane compound.

### Claim 24

A method for damping vibration of a substrate, the substrate being at least one of a metal stamping, a body in white, carbon graphite composites, fiberglass, polycarbonates, ABS, and structural polymeric materials, the method comprising the step of:
applying substantially organic a liquid material by at least one of spraying, dipping and brushing onto the substrate in an ambient environment, the ambient environment having a temperature ranging between about 35° F. (1.7° C.) and about 160° F. (71. 1° C.), wherein, after application to the substrate, the material cures in an interval ranging between about 15 seconds and about 20 seconds;
wherein the substantially organic liquid material consists essentially of:
a first component, consisting essentially of at least one polymer present in an amount sufficient to impart a predetermined amount of tensile strength, hardness and flexibility; and
a second component, consisting essentially of at least one isocyanate compound and is reactive with the first component.

### Claim 25 (depends on 24)

The method as defined in claim 24 wherein the first component of the liquid material consists essentially of:
at least one polymer present in an amount sufficient to impart a predetermined amount of tensile strength, hardness and flexibility;
at least one chain extender present in an amount sufficient to impart a predetermined amount of tensile strength, weatherability, flexibility, adhesion to specific substrates, and hardness; and
at least one filler present in an amount sufficient to impart a predetermined amount of hardness, flexibility, and specific vibration blocking characteristics to the substrate.

### Claim 26 (depends on 25)

The method as defined in claim 25 wherein the at least one polymer is selected from the group consisting of polyoxypropylene diols, polyoxypropylene triols, di-, tri-, quad- or penta-functional polyester polyols, di-, tri-, quad- or penta-functional polyether polyols, and mixtures thereof.

### Claim 27 (depends on 26)

The method as defined in claim 26 wherein the isocyanate compound consists essentially of isocyanate quasi-prepolymers based on a uretonimine modified MDI and a high molecular weight polyether polyol having an isocyanate content of about 15.8% and a 2,4′-isomer content of less than about 10%.

### Claim 28 (depends on 27)

The method as defined in claim 27 wherein the second component further consists essentially of at least one plasticizer present in an amount sufficient to impart a predetermined amount of flexibility.

### Claim 29 (depends on 28)

The method as defined in claim 28 wherein the plasticizer consists essentially of alkylene carbonates selected from the group consisting of ethylene carbonates, propylene carbonates, butylene carbonates, dimethyl carbonates, and mixtures thereof.

### Claim 30 (depends on 25)

The method as defined in claim 25 wherein the at least one polymer comprises amine-terminated polyoxypropylene diols of about 2000 molecular weight;
wherein the at least one chain extender is selected from the group consisting of dialkyl substituted methylene dianilines, diethyltoluene diamines, and mixtures thereof; and
wherein the at least one filler is selected from the group consisting of barium sulfate, calcium carbonate, clay, talc, aluminum silicate, titanium dioxide, nitrile rubbers, butyl rubbers, synthetic rubbers, chopped fiberglass, calcium metasilicate, fibers, fumed silica, and mixtures thereof.

### Claim 31 (depends on 30)

The method as defined in claim 30 wherein the first component further consists essentially of:
a colorant compound selected from the group consisting of carbon black, titanium dioxide, iron oxide, organic pigments, dyes, and mixtures thereof, and
a catalyst selected from the group consisting of tertiary amines, organometallic catalysts, and mixtures thereof.

### Claim 32 (depends on 31)

The method as defined in claim 31 wherein the first component of the composition further consists essentially of at least one adhesion promoter, wherein the adhesion promoter comprises epoxy silane compounds.