# US 2002/0001564 A1 · Aluminosilicate compositions, preparation and use

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0001564 A1
- Document ID: US20020001564A1
- Status: Published application
- Kind: A1
- Application number: 09/776,023
- Filed: 2001-02-02
- Published: 2002-01-03
- Earliest claimed: 1999-10-22
- Inventors: Gerardo Vitale-Rojas; Andres Miguel Quesada Perez
- Web page: https://patentgrep.com/patent/US20020001564A1

## CPC

- C01B 39/065: {Galloaluminosilicates; Group IVB- metalloaluminosilicates; Ferroaluminosilicates}
- C01B 39/06: Preparation of isomorphous zeolites characterised by measures to replace the aluminium or silicon atoms in the lattice framework by atoms of other elements {, i.e. by direct or secondary synthesis}
- Y10S 423/22: MFI, e.g. ZSM-5. silicalite, LZ-241
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for preparing a metalloaluminosilicate, includes the steps of: providing a solution containing a silica source; providing a solution containing an alumina source; providing an aqueous acid solution containing a metal other than silicon or aluminum; mixing the silica source solution with the aqueous acid solution so as to form a silica source-metal containing mixture; mixing the silica source-metal containing mixture with the alumina source solution so as to provide a gel mixture; and hydrothermally crystallizing the gel mixture so as to provide a metalloaluminosilicate material having an aluminosilicate framework and having the metal incorporated into the aluminosilicate framework. A method for preparing aluminosilicate, and specific compositions, are also provided.

## Claims

### Claim 1

A method for preparing a metalloaluminosilicate, comprising the steps of:
providing a solution containing a silica source;
providing a solution containing an alumina source;
providing an aqueous acid solution containing a metal other than silicon or aluminum;
mixing the silica source solution with the aqueous acid solution so as to form a silica source-metal containing mixture;
mixing the silica source-metal containing mixture with the alumina source solution so as to provide a gel mixture; and
hydrothermally crystallizing the gel mixture so as to provide a metalloaluminosilicate material having an aluminosilicate framework and having the metal incorporated into the aluminosilicate framework.

### Claim 2 (depends on 1)

A method according to claim 1, wherein the metal comprises at least one metal selected from the group consisting iron, zinc, zirconium, chromium, nickel, cobalt, magnesium, phosphorous, gallium and mixtures thereof.

### Claim 3 (depends on 1)

A method according to claim 1, wherein the metal is selected from the group consisting of iron, zinc and mixtures thereof.

### Claim 4 (depends on 1)

A method according to claim 1, wherein the gel mixture has a composition in molar ratios as follows:
SiO2/Al2O3 from 5 to 80,
SiO2/DOx from 10 to 1500,
SiO2/(Al2O3+DOx) from 5 to 70,
Na2O/SiO2 from 0.22 to 2.20,
OH/SiO2 from 0.01 to 2.00,
H2O/SiO2 from 14 to 40,
where D is the metal.

### Claim 5 (depends on 1)

A method according to claim 1, wherein the metalloaluminosilicate has a composition expressed in mole ratios of oxides according to an equation selected from the following:
25 1. - a(M2/nO) : b(Al2O3) : c(E2O3) : d(SiO2) : e(H2O) 2. - a(M2/nO) : b(Al2O3) : c(FO2) : d(SiO2) : e(H2O) 3. - a(M2/nO) : b(Al2O3) : c(GO) : d(SiO2) : e(H2O) 4. - a(M2/nO) : b(Al2O3) : c(H2O5) : d(SiO2) : e(H2O)
where M is at least one ion-exchangeable cation having a valence of n; E is an element with valence 3+; F is an element with valence 4+; G is an element with valence 2+; H is an element with valence 5+; a is from >0 to 6; b is equal to 1, c is from >0 to 10; d is from 10 to 80; d/c is from 10 to 1500; e is from 0 to 100; a/(b+c) is from >0 to 5; and d/(b+c) is from 10 to 70.

### Claim 6 (depends on 1)

A method according to claim 1, wherein the hydrothermally crystallizing step is carried out at a temperature of between about 150° C. and about 220° C. under autogenous pressure for a period of at least about 24 hours.

### Claim 7 (depends on 1)

A method according to claim 1, wherein the hydrothermally crystallizing step is carried out at a temperature of between about 165° C. and about 185° C. under autogenous pressure for a period of at least about 24 hours.

### Claim 8 (depends on 1)

A method according to claim 1, wherein the step of hydrothermally crystallizing further comprises the steps of filtering and washing the metalloaluminosilicate material to provide a separated metalloaluminosilicate and drying the separated metalloaluminosilicate to provide a metalloaluminosilicate product.

### Claim 9 (depends on 8)

A method according to claim 8, wherein the drying step is carried out at a temperature of between about 80° C. and about 140° C.

### Claim 10 (depends on 1)

A method according to claim 1, wherein the step of providing the silica source solution comprises dissolving sodium silicate in distilled water.

### Claim 11 (depends on 1)

A method according to claim 1, wherein the step of providing the alumina source solution comprises dissolving sodium aluminate in distilled water.

### Claim 12 (depends on 1)

A method according to claim 1, wherein the step of providing the aqueous acid solution comprises the steps of providing an acid solution and dissolving a metal salt in the acid solution.

### Claim 13 (depends on 12)

A method according to claim 12, wherein the acid solution comprises an aqueous solution of an acid selected from the group consisting of sulfuric acid, nitric acid, hydrochloric acid and mixtures thereof.

### Claim 14 (depends on 1)

A method according to claim 1, further comprising the step of mixing the gel mixture so as to provide a substantially homogeneous gel mixture, and hydrothermally crystallizing the substantially homogeneous gel mixture.

### Claim 15 (depends on 1)

A method according to claim 1, wherein the step of mixing the silica source solution with the aqueous acid solution is carried out under continuous mixing so as to provide a substantially homogeneous silica source-metal containing mixture and wherein the step of mixing the silica source-metal containing mixture is carried out under continuous mixing for a period of time sufficient to provide a substantially homogeneous gel mixture.

### Claim 16 (depends on 1)

A method according to claim 1, further comprising the step of converting the metalloaluminosilicate material to protonic form.

### Claim 17 (depends on 16)

A method according to claim 16, wherein the converting step is an ion exchange step.

### Claim 18

A method for preparing an aluminosilicate composition comprising the steps of:
providing a solution containing a silica source;
providing a solution containing an alumina source; mixing the silica source solution with the aqueous acid solution so as to form a silica source acid mixture;
mixing the silica source acid mixture with the alumina source solution so as to provide a gel mixture; and
hydrothermally crystallizing the gel mixture so as to provide an aluminosilicate composition having an aluminosilicate composition having an aluminosilicate framework, wherein the composition is formed without organic additives.

### Claim 19

A method for preparing an aluminosilicate composition consisting essentially of the steps of:
providing a solution containing a silica source;
providing a solution containing an alumina source; mixing the silica source solution with the aqueous acid solution so as to form a silica source acid mixture;
mixing the silica source acid mixture with the alumina source solution so as to provide a gel mixture; and
hydrothermally crystallizing the gel mixture so as to provide an aluminosilicate composition having an aluminosilicate framework, wherein the composition is formed without organic additives.

### Claim 20

A metalloaluminosilicate composition comprising an aluminosilicate composition having an aluminosilicate framework and containing at least one metal incorporated into the aluminosilicate framework.

### Claim 21 (depends on 20)

A composition according to claim 20, wherein the metal comprises at least one metal selected from the group consisting of iron, zinc, zirconium, chromium, nickel, cobalt, magnesium, phosphorous, gallium and mixtures thereof.

### Claim 22 (depends on 20)

A composition according to claim 20, wherein the metal comprises at least one metal selected from the group consisting of iron, zinc and mixtures thereof.

### Claim 23 (depends on 20)

A composition according to claim 20, which is prepared from a gel mixture having the following molar ratios:
SiO2/Al2O3 from 5 to 80,
SiO2/DOx from 10 to 1500,
SiO2/(Al2O3+DOx) from 5 to 70,
Na2O/SiO2 from 0.22 to 2.20,
OH/SiO2 from 0.01 to 2.00,
H2O/SiO2 from 14 to 40,
where D is the metal.

### Claim 24 (depends on 20)

A composition according to claim 20, wherein the composition has mole ratios of oxides according to an equation selected from the following:
26 1. - a(M2/nO) : b(Al2O3) : c(E2O3) : d(SiO2) : e(H2O) 2. - a(M2/nO) : b(Al2O3) : c(FO2) : d(SiO2) : e(H2O) 3. - a(M2/nO) : b(Al2O3) : c(GO) : d(SiO2) : e(H2O) 4. - a(M2/nO) : b(Al2O3) : c(H2O5) : d(SiO2) : e(H2O)
where M is at least one ion-exchangeable cation having a valence of n; E is an element with valence 3+; F is an element with valence 4+; G is an element with valence 2+; H is an element with valence 5+; a is from >0 to 6; b is equal to 1, c is from >0 to 10; d is from 10 to 80; d/c is from 10 to 1500; e is from 0 to 100; a/(b+c) is from >0 to 5; and d/(b+c) is from 10 to 70.