# US 2002/0000667 A1 · Method of manufacturing an insulation film in a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0000667 A1
- Document ID: US20020000667A1
- Status: Published application
- Kind: A1
- Application number: 09/880,348
- Filed: 2001-06-13
- Published: 2002-01-03
- Earliest claimed: 2000-06-30
- Assignees: Hyundai Electronics Industries Co., Ltd.
- Inventors: Sang Tae Ahn; Jung Gyu Song
- Web page: https://patentgrep.com/patent/US20020000667A1

## CPC

- C23C 16/45523: {Pulsed gas flow or change of composition over time}
- C23C 16/402: {Silicon dioxide}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10W 20/074: {of dielectric parts comprising thin functional dielectric layers, e.g. dielectric etch-stop, barrier, capping or liner layers}
- H10W 20/096: {by contacting with gases, liquids or plasmas}
- H10W 20/48: Insulating materials thereof
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of manufacturing an insulating film in a semiconductor device is disclosed. The method comprises the steps of forming a SOD film on the entire structure to fill any distance between conductive layer patterns and after performing a curing process, forming a hard mask film on the SOD film, wherein the silicon oxide film is deposited by plasma deposition method using SiH4 and N2O as a reaction gas at a low-temperature and at a low-pressure and wherein in a stabilization step, the supply amount of SiH4 is greater than that of N2O and in a deposition step, the supply amount of N2O is greater than that of SiH4.

## Claims

### Claim 1

A method of manufacturing an insulating film in a semiconductor device, comprising:
forming a SOD film on an entire structure that comprises at least two conductive layer patterns with a distance therebetween to fill the distance between said conductive layer patterns;
performing a curing process; and
forming a hard mask film on said SOD film.

### Claim 2 (depends on 1)

The method of manufacturing an insulating film in a semiconductor device according to claim 1, wherein said SOD film is selected from the group consisting of a polymer film made of C, H and 0 components, a MSQ film and a HSQ film.

### Claim 3 (depends on 1)

The method of manufacturing an insulating film in a semiconductor device according to claim 1, wherein said curing process is performed at a temperature ranging from about 300° C. to about 650° C. in a reaction furnace.

### Claim 4 (depends on 1)

The method of manufacturing an insulating film in a semiconductor device according to claim 1, wherein said hard mask film is a silicon oxide film.

### Claim 5 (depends on 4)

The method of manufacturing an insulating film in a semiconductor device according to claim 4, wherein said silicon oxide film is formed by plasma deposition method using SiH4 and N2O as a reaction gas under a low-temperature ranging from about 20° C. to about 650° C. and a low-pressure, and
wherein in a stabilization step before plasma is generated, a supply amount of SiH4 is greater than a supply amount of N2O and, in a deposition step after plasma is generated, a supply amount of N2O is greater than a supply amount of SiH4.

### Claim 6 (depends on 5)

The method of manufacturing an insulating film in a semiconductor device according to claim 5, wherein a RF power for generating said plasma is supplied for a time period ranging from about 1 second to about 100 seconds with a low power ranging from about 10 W to about 1000 W at an earlier stage of generating said plasma, and the power is then increased to a range from about 100 W to about 3000 W for a time period ranging from about 10 seconds to about 200 seconds.

### Claim 7

A method of manufacturing an insulating film in a semiconductor device, comprising the steps of:
forming a first SOD film on a semiconductor device for which a given process is performed and then performing a curing process;
forming a hard mask film on said first SOD film and then performing a surface process in-situ; and
forming a second SOD film on said first SOD film and then performing a curing process, and then forming a second hard mask film on said second SOD film.

### Claim 8 (depends on 7)

The method of manufacturing an insulating film in a semiconductor device according to claim 7, wherein said first and second SOD films are selected from the group consisting of a polymer film made of C, H and 0 components, a MSQ film and a HSQ film.

### Claim 9 (depends on 7)

The method of manufacturing an insulating film in a semiconductor device according to claim 7, wherein said curing process is performed at a temperature ranging from about 300° C. to about 650° C. in a reaction furnace.

### Claim 10 (depends on 7)

The method of manufacturing an insulating film in a semiconductor device according to claim 7, wherein said first and second hard masks are silicon oxide films.

### Claim 11 (depends on 10)

The method of manufacturing an insulating film in a semiconductor device according to claim 10, wherein said silicon oxide film is formed by plasma deposition method using SiH4 and N2O as a reaction gas under a low-temperature ranging from about 20° C. to about 650° C. and a low-pressure, wherein in a stabilization step before plasma is generated, a supply amount of SiH4 is greater than a supply amount of N2O and, in a deposition step after plasma is generated, a supply amount of N2O is greater than a supply amount of SiH4.

### Claim 12 (depends on 11)

The method of manufacturing an insulating film in a semiconductor device according to claim 11, wherein a RF power for generating said plasma supplied for a time period ranging from about 1 second to about 100 seconds with a low power ranging from about 10 W to about 1000 W at an earlier stage of generating said plasma, and is then increased to a range from about 100 W to about 3000 W for a time period ranging from about 10 seconds to about 200 seconds.

### Claim 13 (depends on 7)

The method of manufacturing an insulating film in a semiconductor device according to claim 7, wherein said surface process is a plasma process, and
wherein said plasma employs a reaction gas selected from the group consisting of N2, NH3, N2O O2, Ar, He, and is generated by supplying a RF power of a range from about 10 W to about 100 W.

### Claim 14 (depends on 1)

A semiconductor device comprising an insulating film and manufactured in accordance with the method of claim 1.

### Claim 15 (depends on 7)

A semiconductor device comprising an insulating film and manufactured in accordance with the method of claim 7.