# US 2002/0000643 A1 · Devices related to electrode pads for p-type group iii nitride compound semiconductors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0000643 A1
- Document ID: US20020000643A1
- Status: Published application
- Kind: A1
- Application number: 08/866,129
- Filed: 1997-05-30
- Published: 2002-01-03
- Earliest claimed: 1996-05-31
- Assignees: Toyoda Gosei Co., Ltd.
- Inventors: TOSHIYA UEMURA; NAOKI SHIBATA; SHIZUYO NOIRI; SHIGEMI HORIUCHI
- Web page: https://patentgrep.com/patent/US20020000643A1

## CPC

- H10D 62/85: being Group III-V materials, e.g. GaAs
- H10D 64/62: Electrodes ohmically coupled to a semiconductor
- H10W 72/019: {of bond pads}
- H10W 72/90: Bond pads, in general
- H10W 72/923: {Bond pads having multiple stacked layers}
- H10W 72/952: {comprising metals or metalloids, e.g. PbSn, Ag or Cu}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

An electrode pad for a Group III nitride compound semiconductor having p-type conduction includes a triple layer structure having first, second, and third metal layers, formed on an electrode layer. A protection film with a window exposing a central portion of the third metal layer is formed by etching on the third metal layer and covers the sides of the first, second, and third metal layers. The second metal layer is made of gold (Au). The first metal layer is made of an element which has ionization potential lower than gold (Au). The third metal is made of an element which has adhesiveness to the protection film stronger than that of gold (Au). Consequently, this structure of the electrode pad improves the adhesive strength between the protection layer and the third meal layer and prevents the etching of the sides of the protection film. Furthermore, the contact resistance between the semiconductor and the electrode pad is lowered and, thus, ohmic characteristic of the electrode pad is improved.

## Claims

### Claim 1

An electrode pad for a Group III nitride compound semiconductor having p-type conduction, comprising:
a first metal layer formed on at least one of said semiconductor and an electrode layer formed on said semiconductor, a second metal layer formed on said first metal layer, and a third metal layer formed on said second metal layer;
a protection film covering over said third metal layer and exposing central portion of said third metal layer; and
wherein said second metal layer is made of gold (Au), said first metal layer comprises a material that has an ionization potential lower than gold (Au), and said third metal layer comprises a material that has an adhesiveness to said protection film which is stronger than gold (An).

### Claim 2 (depends on 1)

An electrode pad according to claim 1, wherein said material of said first metal layer includes at least one of nickel (Ni), iron (Fe), copper (Cu), chromium (Cr), tantalum (Ta), vanadium (V), manganese (Mn), aluminum (Al), and silver (Ag).

### Claim 3 (depends on 1)

An electrode pad according to claim 1, wherein said material of said third metal layer includes at least one of aluminum (Al), nickel (Ni), and titanium (Ti).

### Claim 4 (depends on 1)

An electrode pad according to claim 1, wherein said protection film is made of silicon oxide (SiO2).

### Claim 5 (depends on 1)

An electrode pad according to claim 1, wherein said material of said first metal layer is nickel (Ni) and said material of said third metal layer is aluminum (Al).

### Claim 6 (depends on 1)

An electrode pad according to claim 1, wherein said electrode layer has a multi-layer structure at least having a first electrode layer formed on said semiconductor and a second electrode layer formed on said first electrode layer, wherein said first electrode layer comprises material having an ionization potential that is lower than that of said second electrode layer, said material of said second electrode layer has an ohmic characteristic to said semiconductor better than that of said first electrode layer, and said material of said second electrode layer being distributed more deeply into said semiconductor than that of said first electrode layer by heat treatment.

### Claim 7 (depends on 6)

An electrode pad according to claim 6, wherein said material of said first electrode layer includes at least one of nickel (Ni), iron (Fe), copper (Cu), chromium (Cr), tantalum (Ta), vanadium (V), manganese (Mn), aluminum (Al), and silver (Ag), and said material of said second electrode layer includes at least one of palladium (Pd), gold (Au), iridium (Ir), and platinum (Pt).

### Claim 8 (depends on 6)

An electrode pad according to claim 6, wherein said material of said first electrode layer is nickel (Ni) and said material of said second electrode layer is gold (Au).

### Claim 9 (depends on 6)

An electrode pad according to claim 6, wherein said heat treatment is carried out in the range of 400° C. to 700° C.

### Claim 10 (depends on 1)

A Group III nitride compound semiconductor device having the electrode pad of claim 1 and further comprising:
semiconductor layers having Group III nitride compound semiconductor and satisfying the formula, AlxGayIn1−x−yN, wherein 0≦x≦1, 0≦y≦1, and 0≦x+y≦1.

### Claim 11 (depends on 10)

A semiconductor device of claim 10, wherein said device is one of a light-emitting diode (LED), a light-emitting laser diode (LD) and a transistor.

### Claim 12

A light-emitting semiconductor device of a Group III nitride compound semiconductor with p-type conduction, comprising:
a surface layer;
a multi-layered electrode layer comprising a first electrode layer formed on said surface layer and a second electrode layer formed on said first electrode layer;
an electrode pad covering a portion of said second electrode layer and leaving another portion of said second electrode layer uncovered; and
wherein said first electrode layer comprises a material which has an ionization potential lower than that of said second electrode layer,
said second electrode layer comprises a material which has an ohmic characteristic to said semiconductor better than that of said first electrode layer, and
the portion of said material of said second electrode layer which is uncovered by said electrode pad is distributed more deeply into said surface layer than that of said first electrode layer by heat treatment and provides a contact resistance between said elect rode layer and said surface layer lower than said portion covered with said electrode pad.

### Claim 13 (depends on 12)

A semiconductor device according to claim 12, wherein said material of said first electrode layer includes at least one of nickel (Ni), iron (Fe), copper (Cu), chromium (Cr), tantalum (Ta), vanadium (V), manganese (Mn), aluminum (Al), and silver (Ag) and said material of said second electrode layer includes at least one of palladium (Pd), gold (Au), iridium (Ir), and platinum (Pt).

### Claim 14 (depends on 12)

A semiconductor device according to claim 12, wherein said material of said first electrode layer is nickel (Ni) and said material of said second electrode layer is gold (Au).

### Claim 15

A method for manufacturing a light-emitting semiconductor device of Group III nitride compound semiconductor with p-type conduction, said method comprising:
providing a surface layer;
forming a multi-layered electrode layer comprising a first electrode layer formed on said surface layer and a second electrode layer formed on said first electrode layer, said first electrode layer comprising a material having ionization potential lower than that of said second electrode layer and said second electrode layer comprising a material having an ohmic characteristic to said semiconductor better than that of said first electrode layer;
forming an electrode pad covering a portion of said second electrode layer and leaving another portion of said second electrode layer uncovered; and
providing a heat treatment so that the portion of said material of said second electrode layer which is uncovered by said electrode pad is distributed more deeply into said surface layer than that of said first electrode layer and provides a contact resistance between said electrode layer and said surface layer lower than said portion covered with said electrode pad.

### Claim 16 (depends on 15)

A method according to claim 15, wherein said material of said first electrode layer includes at least one of nickel (Ni), iron (Fe), copper (Cu), chromium (Cr), tantalum (Ta), vanadium (V), manganese (Mn), aluminum (Al), and silver (Ag) and said material or said second electrode layer includes at least one of palladium (Pd), gold (Au). tridium (Ir), and platinum (Pt).

### Claim 17 (depends on 15)

A method according to claim 15, wherein said material of said first electrode layer is nickel (Ni) and said material of said second electrode layer is gold (Au).

### Claim 18 (depends on 15)

A method according to claim 15, wherein said heat treatment is carried out in the range from about 400° C. to 700° C.

### Claim 19 (depends on 15)

A method according to claim 15, wherein said Group III nitride compound semiconductor satisfies the formula AlxGayIn1−x−yN, wherein 0≦x≦1, 0≦y≦1, and 0≦x+y≦1.