# US 2002/0000601 A1 · Semiconductor device having self-aligned contact and landing pad structure and method of forming same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0000601 A1
- Document ID: US20020000601A1
- Status: Published application
- Kind: A1
- Application number: 09/451,054
- Filed: 1999-11-30
- Published: 2002-01-03
- Earliest claimed: 1999-11-30
- Assignees: Agere Systems Guardian Corp.
- Inventors: SEUNGMOO CHOI
- Web page: https://patentgrep.com/patent/US20020000601A1

## CPC

- H10W 20/069: {by forming self-aligned vias or self-aligned contact plugs}
- H10B 41/00: Electrically erasable-and-programmable ROM [EEPROM] devices comprising floating gates
- H10W 20/0698: {Local interconnections}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor integrated circuit device and method of forming same is disclosed and includes a silicon substrate having a field oxide region and spaced active region. First and second self-aligned contact window openings are associated with a respective field oxide region and active region. A dummy polysilicon landing pad is formed over the field oxide region and formed below the first self-aligned contact window opening. An operative polysilicon landing pad is formed above the dummy landing pad. A silicon nitride barrier layer is also formed during the process.

## Claims

### Claim 1

A semiconductor integrated circuit device comprising:
a silicon substrate having a field oxide region and a spaced active region formed therein;
first and second self-aligned contacts formed in respective first and second self-aligned contact window openings that are associated with the respective field oxide region and active region;
a dummy polysilicon landing pad formed over said field oxide region and formed below said first self-aligned contact window opening; and
an operative polysilicon landing pad formed above said dummy landing pad.

### Claim 2 (depends on 1)

The device according to claim 1, wherein said second self-aligned contact window opening comprises a first, upper portion that is formed during a first self-aligned contact etch step and a second, lower portion that is formed during a second self-aligned contact etch step.

### Claim 3 (depends on 2)

The device according to claim 2, wherein said first self-aligned contact window opening is formed during the first self-aligned contact etch step.

### Claim 4 (depends on 3)

The device according to claim 3, and further comprising a silicon nitride layer that is formed before a self-aligned contact etch step.

### Claim 5 (depends on 1)

The device according to claim 1, wherein said dummy landing pad is formed during a floating gate fabrication process.

### Claim 6 (depends on 1)

The device according to claim 1, and further comprising a thin oxide layer positioned below said second self-aligned contact window opening.

### Claim 7 (depends on 1)

The device according to claim 1, and further comprising a polysilicon landing pad overlying a portion of the active region.

### Claim 8 (depends on 1)

The device according to claim 1, and further comprising sidewall spacers formed on the ends of the polysilicon landing pad overlying a portion of the active region.

### Claim 9 (depends on 1)

The device according to claim 1, and further comprising sidewall spacers formed on the ends of the operative polysilicon landing pad.

### Claim 10

A method of forming a semiconductor integrated circuit device comprising the steps of:
forming a field oxide region and a spaced active region within a semiconductor substrate;
forming first and second self-aligned contact window openings that are associated with the respective field oxide region and active region;
forming a dummy polysilicon landing pad over the field oxide region and below the first self-aligned contact window opening; and
forming an operative polysilicon landing pad above the dummy landing pad.

### Claim 11 (depends on 10)

A method according to claim 10, and further comprising the step of forming a first, upper portion of the second self-aligned contact window opening during a first self-aligned contact etch step and a second, lower portion during a second self-aligned contact etch step.

### Claim 12 (depends on 11)

A method according to claim 11, and further comprising the step of forming the first self-aligned contact window during the first self-aligned contact etch step.

### Claim 13 (depends on 12)

A method according to claim 12, and further comprising the step of forming a silicon nitride layer before any self-aligned contact etch step.

### Claim 14 (depends on 10)

A method according to claim 10, and further comprising the step of forming the dummy landing pad during a floating gate fabrication process.

### Claim 15 (depends on 10)

A method according to claim 10, and further comprising the step of forming a thin oxide layer such that the second self-aligned contact window opening is positioned over the thin oxide layer.

### Claim 16 (depends on 10)

A method according to claim 10, and further comprising the step of forming a polysilicon landing pad overlying a portion of the active region.

### Claim 17 (depends on 10)

A method according to claim 10, and further comprising the step of forming sidewall spacers on the ends of the polysilicon landing pad overlying a portion of the active region.

### Claim 18 (depends on 10)

A method according to claim 10, and further comprising the step of forming sidewall spacers on the ends of the operative polysilicon landing pad.