# US 2002/0000244 A1 · Enhanced light absorption of solar cells and photodetectors by diffraction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2002/0000244 A1
- Document ID: US20020000244A1
- Status: Published application
- Kind: A1
- Application number: 09/834,308
- Filed: 2001-04-11
- Published: 2002-01-03
- Earliest claimed: 2000-04-11
- Assignees: Gratings, Inc.; Sandia Corporation
- Inventors: Saleem H. Zaidi
- Web page: https://patentgrep.com/patent/US20020000244A1

## CPC

- H10F 77/703: {of the semiconductor bodies, e.g. textured active layers}
- H10F 71/121: {The active layers comprising only Group IV materials}
- Y02E 10/547: Monocrystalline silicon PV cells
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Enhanced light absorption of solar cells and photodetectors by diffraction. Triangular, rectangular, and blazed subwavelength periodic structures are shown to improve performance of solar cells. Surface reflection can be tailored for either broadband, or narrow-band spectral absorption. Enhanced absorption is achieved by efficient optical coupling into obliquely propagating transmitted diffraction orders. Subwavelength one-dimensional structures are designed for polarization-dependent, wavelength-selective absorption in solar cells and photodetectors, while two-dimensional structures are designed for polarization-independent, wavelength-selective absorption therein. Suitable one and two-dimensional subwavelength periodic structures can also be designed for broadband spectral absorption in solar cells and photodetectors. If reactive ion etching (RIE) processes are used to form the grating, RIE-induced surface damage in subwavelength structures can be repaired by forming junctions using ion implantation methods. RIE-induced surface damage can also be removed by post RIE wet-chemical etching treatments.

## Claims

### Claim 1

A method for increasing absorption of light radiation in a photo responsive device which comprises the step of forming a grating on the surface of said photo responsive device upon which light is incident such that higher grating orders are generated within said photo responsive device and the majority of the incident light entering said photo responsive device propagates obliquely to the surface upon which light is incident, thereby increasing light absorption by said photo responsive device close to the surface upon which light is incident.

### Claim 2 (depends on 1)

The method as described in claim 1, wherein said photo responsive device is selected from the group consisting of solar cells and photo detectors.

### Claim 3 (depends on 2)

The method as described in claim 2, wherein the solar cell material comprises silicon.

### Claim 4 (depends on 1)

The method as described in claim 1 further comprising the step of forming a grating on the surface of said photo responsive device opposite to the surface upon which light is incident.

### Claim 5 (depends on 1)

The method as described in claim 1, wherein said photo responsive device comprises silicon having a thickness of <100 μm.

### Claim 6 (depends on 1)

The method as described in claim 1, wherein said step of forming a grating comprises reactive ion etching.

### Claim 7 (depends on 6)

The method as described in claim 6, further comprising the step of selective KOH etching to remove RIE-induced surface damage.

### Claim 8 (depends on 1)

The method as described in claim 1, wherein said step of forming a grating comprises wet chemical etching.

### Claim 9 (depends on 1)

The method as described in claim 1, wherein the grating comprises a rectangular grating.

### Claim 10 (depends on 1)

The method as described in claim 1, wherein the grating comprises a triangular grating.

### Claim 11 (depends on 1)

The method as described in claim 1, wherein the grating comprises a blazed grating.

### Claim 12 (depends on 1)

The method as described in claim 1, wherein the grating is chosen to have optimal performance within solar cell spectrum.

### Claim 13 (depends on 1)

The method as described in claim 1, further comprising the step of anti-reflection coating the grating surface.

### Claim 14 (depends on 2)

The method as described in claim 2, further comprising the step of forming a junction in the solar cell using ion implantation.

### Claim 15

A method for producing a solar cell having increased absorption of light which comprises the steps of: (a) forming a grating on he surface of said solar cell upon which light is incident; (b) removing surface contamination; (c) forming an n-type junction using gas source doping; and (d) forming n- and p-electrical contacts.

### Claim 16 (depends on 15)

The method as described in claim 15, wherein said step of forming a grating comprises reactive ion etching.

### Claim 17 (depends on 16)

The method as described in claim 16, further comprising the step of removing reactive ion etching-induced surface damage using wet-chemical etching.

### Claim 18 (depends on 17)

The method as described in claim 17, wherein said step of wet-chemical etching comprises exposing the surface to KOH and nitric acid solutions.

### Claim 19 (depends on 15)

The method as described in claim 15, wherein said step of forming a grating comprises wet chemical etching.

### Claim 20

A method for producing a solar cell having increased absorption of light which comprises the steps of, (a) forming a grating on the surface of said solar cell upon which light is incident; (b) cleaning the surface to remove surface contamination: (c) forming an n-type junction by ion implantation; (d) annealing the solar cell formed thereby; and (e) forming n- and p-electrical contacts.

### Claim 21 (depends on 20)

The method as described in claim 20, wherein said step of forming a grating comprises reactive ion etching.

### Claim 22 (depends on 20)

The method as described in claim 20, wherein said step of forming an n-type junction comprises ion implantation using 31P+.

### Claim 23 (depends on 20)

The method as described in claim 20, wherein said step of annealing the solar cell comprises heating the solar cell in an oxygen atmosphere.

### Claim 24 (depends on 20)

The method as described in claim 20, wherein said step of forming a grating comprises wet chemical etching.