# US 2001/0055940 A1 · Control of CMP removal rate uniformity by selective control of slurry temperature

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0055940 A1
- Document ID: US20010055940A1
- Status: Published application
- Kind: A1
- Application number: 09/863,689
- Filed: 2001-05-23
- Published: 2001-12-27
- Earliest claimed: 2000-06-15
- Inventors: Leland Swanson
- Web page: https://patentgrep.com/patent/US20010055940A1

## CPC

- B24B 37/015: Temperature control
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS

## Abstract

A CMP machine (100, 200, 300) and/or process that uses selective heating of the slurry (160) to improve uniformity. A temperature control mechanism (110) is used to heat and/or cool slurry (160) applied to a selected area of the pad or belt (120, 220, 320). Heating in the selected area improves the removal rate in that area, whereas cooling decreases the removal rate in that area. For example, heating along the perimeter of the pad (120, 220) improves the removal rate at the perimeter of the semiconductor wafer (150).

## Claims

### Claim 1

A method of fabricating an integrated circuit, comprising the steps of:
placing a wafer against a moving polishing pad while adding a first slurry to a first location and a second slurry to a second location wherein a temperature of said first slurry is higher than a temperature of said second slurry.

### Claim 2 (depends on 1)

The method of claim 1, wherein said polishing pad is a polishing belt.

### Claim 3 (depends on 1)

The method of claim 1, wherein said temperature of said first slurry is between room temperature and 40° C.

### Claim 4 (depends on 1)

The method of claim 1, wherein said temperature of said second slurry is between 5° C. and room temperature.

### Claim 5 (depends on 1)

The method of claim 1, wherein said second slurry spends a higher percentage of time near a center said wafer than said first slurry.

### Claim 6 (depends on 1)

The method of claim 1, wherein said second slurry penetrates further under said wafer than said first slurry.

### Claim 7

A method of fabricating an integrated circuit, comprising the steps of:
providing a partially fabricated wafer to a wafer carrier of a chemical-mechanical polish (CMP) machine;
moving a polishing pad of said CMP machine;
adding slurry to a surface of said polishing pad from at least two dispense points, wherein there is a slurry temperature gradient between said at least two dispense points; and
placing said wafer against said surface while said polishing pad is moving.

### Claim 8 (depends on 7)

The method of claim 7, wherein said polishing pad is a polishing belt.

### Claim 9 (depends on 7)

The method of claim 7, wherein a first of said at least two dispense points is located near a center of said polishing piece and a second of said at least two dispense points is located near an edge of said polishing piece.

### Claim 10 (depends on 9)

The method of claim 9, wherein a temperature of said slurry from said first dispense point is less than a temperature of said slurry from said second dispense point.

### Claim 11 (depends on 7)

The method of claim 7, wherein slurry from a first of said at least two dispense points penetrates further under the wafer than slurry from a second of said at least two dispense points.

### Claim 12 (depends on 7)

The method of claim 7, wherein slurry from a first of said at least two dispense points has a lower temperature than slurry from a second of said at least two dispense points.

### Claim 13

A chemical-mechanical polish (CMP) machine comprising:
a platen;
a polishing pad located over said platen;
a wafer carrier for holding a wafer against said polishing pad; and
at least two slurry dispense outlets, wherein at least one of said slurry dispense outlets contains a temperature control mechanism for establishing a slurry temperature gradient between said at least two slurry dispense outlets.

### Claim 14 (depends on 13)

The CMP machine of claim 13, wherein said a first of said at least two slurry dispense outlets is located nearer a center of said polishing piece and a second of said at least two slurry dispense outlet is located nearer an edge of said polishing piece.