# US 2001/0055863 A1 · Methods for manufacturing soi wafer and soi wafer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0055863 A1
- Document ID: US20010055863A1
- Status: Published application
- Kind: A1
- Application number: 09/324,939
- Filed: 1999-06-03
- Published: 2001-12-27
- Earliest claimed: 1998-06-04
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Inventors: MASATAKE NAKANO; KATSUO YOSHIZAWA
- Web page: https://patentgrep.com/patent/US20010055863A1

## CPC

- H10P 90/1914: {using bonding}
- H10P 90/1922: {using silicon etch back techniques, e.g. BESOI or ELTRAN}
- H10W 10/181: {Semiconductor-on-insulator [SOI] isolation regions, e.g. buried oxide regions of SOI wafers}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The object of the invention is to reduce an outer circumferential edge removing width of the SOI wafer when a bonded SOI wafer is made and prevent deposition of polysilicon at the outer circumference of the SOI layer when an epitaxial layer is grown. An SOI layer is formed by the steps of forming an oxide film on a surface of at least one silicon wafer of two silicon wafers, bonding the other silicon wafer through said oxide film at a room temperature, the wafers are heat treated in oxidizing atmosphere, thereafter an outer periphery of a bond wafer is removed from an outer peripheral edge of the bond wafer up to a region between bonding ends through bonding at a room temperature and heat treatment bonding ends and making the bond wafer into a thin film of desired thickness.

## Claims

### Claim 1

A method for manufacturing an SOI wafer characterized in that an SOI layer is formed by the steps of forming an oxide film on a surface of at least one silicon wafer of two silicon wafers, bonding the other silicon wafer through said oxide film at a room temperature, the wafers are heat treated in oxidizing atmosphere, thereafter an outer periphery of a bond wafer is removed from an outer peripheral edge of the bond wafer up to a region between bonding ends through bonding at a room temperature and heat treatment bonding ends and making the bond wafer into a thin layer of desired thickness.

### Claim 2 (depends on 1)

A method for manufacturing an SOI wafer according to claim 1, wherein after forming said SOI layer, a vapor phase etching is carried out to form a thin film SOI layer.

### Claim 3 (depends on 1)

A method for manufacturing an SOI wafer according to claim 1, wherein after forming either said SOI layer or a thin film SOI layer, said SOI layer or the outer peripheral part of said thin film SOI layer is removed down to an inside part of the bonding end of said bonding at a room temperature.

### Claim 4 (depends on 2)

A method for manufacturing an SOI wafer according to claim 2, wherein after forming either said SOI layer or a thin film SOI layer, said SOI layer or the outer peripheral part of said thin film SOI layer is removed down to an inside part of the bonding end of said bonding at a room temperature.

### Claim 5 (depends on 3)

A method for manufacturing an SOI wafer according to claim 3, wherein a thickness of either said SOI layer or said thin film SOI layer is 1.5 μm or less.

### Claim 6 (depends on 4)

A method for manufacturing an SOI wafer according to claim 4, wherein a thickness of either said SOI layer or said thin film SOI layer is 1.5 μm or less.

### Claim 7

A method for manufacturing an SOI wafer characterized in that an oxide film is formed on a surface of at least one silicon wafer of two silicon wafers, the other silicon wafer is bonded through said oxide film at a room temperature, the wafers are heat treated in oxidizing atmosphere, thereafter an outer periphery of a bond wafer is removed from an outer peripheral edge of the bond wafer up to a first region inside bonding ends through their bonding at a room temperature, a thickness of said bond wafer is reduced to a desired thickness to form an SOI layer, thereafter an outer periphery of said SOI layer is removed down to inside said first region.

### Claim 8 (depends on 5)

A method for manufacturing an SOI wafer according to claim 5, wherein a thickness of said SOI layer is 1.5 μm or less.

### Claim 9

An SOI wafer characterized in that a film thickness of an SOI layer is 1.5 μm or less and an angle formed by a surface near an outer peripheral end of SOI layer and an interface between an buried oxide layer and the SOI layer is approximately 2° or more.

### Claim 10

A thin film SOI wafer etched in vapor phase characterized in that a film thickness of an SOI layer of said thin film SOI wafer is 1.5 μm or less and an outer periphery removing width is 3 mm or less.