# US 2001/0055820 A1 · Ferroelectric thin film device and method of producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0055820 A1
- Document ID: US20010055820A1
- Status: Published application
- Kind: A1
- Application number: 09/773,987
- Filed: 2001-02-01
- Published: 2001-12-27
- Earliest claimed: 1997-09-22
- Assignees: Murata Manufacturing Co., Ltd.
- Inventors: Atsushi Sakurai; Xiao-Min Li; Kosuke Shiratsuyu
- Web page: https://patentgrep.com/patent/US20010055820A1

## CPC

- H10D 1/684: {the dielectrics comprising multiple layers, e.g. comprising buffer layers, seed layers or gradient layers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A ferroelectric thin film device comprises an Si substrate; a TiN thin film whose Ti component is partially replaced with Al, the TiN thin film being formed on the Si substrate; and a ferroelectric thin film of an oxide with a perovskite structure formed on the TiN thin film, wherein the amount of Al atoms present at Ti sites of the TiN thin film after partially replacing Ti with Al is within the range from about 1% to 30% and the oxygen atomic content of the TiN thin film is equal to or less than about 5%.

## Claims

### Claim 1

A ferroelectric thin film device comprising:
an Si substrate;
a TiN thin film whose Ti component is partially replaced with Al, on said Si substrate; and
a ferroelectric thin film of a perovskite oxide on said TiN thin film,
wherein the amount of Al atoms present at Ti sites of said TiN thin film is within the range from about 1% to 30% and the oxygen atomic content of said TiN thin film is equal to or less than about 5%.

### Claim 2 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein the amount of Al atoms present at Ti sites of said TiN thin film is within the range from about 5% to 20% and the oxygen atomic content of said TiN thin film is equal to or less than about 1%.

### Claim 3 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein the thickness of said TiN thin film is about 100 to 500 nm and the thickness of said ferroelectric thin film is about 400 to 800 nm.

### Claim 4 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein said TiN thin film is epitaxially grown and said ferroelectric thin film is orientationally ordered.

### Claim 5 (depends on 4)

A ferroelectric thin film device according to claim 4, wherein said ferroelectric thin film is a Pb-based perovskite.

### Claim 6 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein said ferroelectric thin film is a Pb-based perovskite.

### Claim 7 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein said ferroelectric thin film is a perovskite represented by the formula of ABO3, where A is Pb or Pb and at least La and B is at least one element selected from the group consisting of Ti, Zr, Mg and Nb.

### Claim 8 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein said ferroelectric thin film is epitaxial.

### Claim 9 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein said TiN thin film is a laser deposition film.

### Claim 10 (depends on 1)

A ferroelectric thin film device according to claim 1, wherein said ferroelectric thin film is a chemical vapor deposition film.

### Claim 11

A method of producing a ferroelectric thin film device, comprising the steps of:
epitaxially forming a TiN thin film whose Ti component is partially replaced with Al; and
forming a ferroelectric thin film of a perovskite oxide in an orientationally ordered fashion on said TiN thin film, wherein
the amount of Al atoms present at Ti sites of said TiN thin film is within the range from about 1% to 30% and the oxygen atomic content of said TiN thin film is equal to or less than about 5%.

### Claim 12 (depends on 11)

A method of producing a ferroelectric thin film device according to claim 11, wherein the amount of Al atoms present at Ti sites of said TiN thin film is within the range from about 5% to 20% and the oxygen atomic content of said TiN thin film is equal to or less than about 1%.

### Claim 13 (depends on 11)

A method of producing a ferroelectric thin film device according to claim 11, wherein said ferroelectric thin film is a Pb-based perovskite.

### Claim 14 (depends on 11)

A method of producing a ferroelectric thin film device according to claim 11, wherein said ferroelectric thin film is a perovskite represented by the formula of ABO3, where A is Pb or Pb and at least La and B is at least one element selected from the group consisting of Ti, Zr, Mg and Nb.

### Claim 15 (depends on 11)

A method of producing a ferroelectric thin film device according to claim 11, wherein said ferroelectric thin film is formed by an epitaxial growth process.

### Claim 16 (depends on 11)

A method of producing a ferroelectric thin film device according to claim 11, wherein said TiN thin film Ti is formed by a laser deposition process at a pressure equal to or lower than about 1×10−6 Torr using a target material whose Ti component is partially replaced with Al.

### Claim 17 (depends on 11)

A method of producing a ferroelectric thin film device according to claim 11, wherein said ferroelectric thin film is formed by a chemical vapor deposition process.