# US 2001/0054388 A1 · Single-substrate-film-forming method and single-substrate-heat-processing apparatus

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0054388 A1
- Document ID: US20010054388A1
- Status: Published application
- Kind: A1
- Application number: 09/859,388
- Filed: 2001-05-18
- Published: 2001-12-27
- Earliest claimed: 2000-05-22
- Assignees: Tokyo Electron Limited
- Inventors: Shao Shou Qian
- Web page: https://patentgrep.com/patent/US20010054388A1

## CPC

- H10P 14/6336: {in the presence of a plasma [PECVD]}
- C23C 16/405: {of refractory metals or yttrium}
- C23C 16/56: After-treatment
- H01J 37/3244: {Gas supply means}
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/6519: {the substance being oxygen}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6544: {to change the morphology of the insulating materials, e.g. transformation of an amorphous layer into a crystalline layer}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/69392: {the material containing hafnium, e.g. HfO2}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A heat-processing apparatus for deposition and reformation for forming a tantalum oxide film on a semiconductor substrate includes an airtight process chamber for accommodating the wafer and a worktable for supporting the wafer thereon. A heater for heating the wafer is disposed in the worktable. The process chamber is connected to an exhaust section for exhausting the process chamber. The process chamber is also connected to a section for supplying pentoethoxytantalum as a precursor of the tantalum oxide, a line for supplying an oxidizing gas, and a section for supplying a reforming gas for the tantalum oxide. The reforming gas consists of an excited oxygen gas containing no ions or electrons.

## Claims

### Claim 1

A single-substrate-processing-film-forming method comprising the steps of:
performing a deposition process of depositing a film consisting essentially of an amorphous metal oxide on a target substrate by means of CVD; and
performing a reformation process of removing an organic impurity contained in the film,
wherein the reformation process comprises a step of supplying an excited oxygen gas as a reforming gas into a process chamber accommodating the target substrate, while exhausting the process chamber, the reforming gas being set to have a concentration of ions and electrons not more than 105/cm3.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising steps of:
exciting oxygen gas until generating plasma by an exciting mechanism disposed outside the process chamber; and
preparing the reforming gas by mixing the excited oxygen gas with a non-excited oxygen gas to reduce a concentration of ions and electrons in the excited oxygen gas.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the reforming gas contains a catalytic gas for accelerating activation of the oxygen gas at a concentration of from 0 to 15 flow-rate %.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the catalytic gas consists of N2.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the reformation process comprises a step of heating the film to a temperature lower than a crystallization temperature of the metal oxide.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the reformation process comprises a step of heating the film to a temperature higher than a crystallization temperature of the metal oxide, to perform a crystallization process of crystallizing the film at the same time.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the deposition process is performed in the process chamber, and comprises a step of supplying a raw material gas, which offers a metal of the metal oxide by decomposition, and an oxidizing gas into the process chamber accommodating the target substrate, while exhausting the process chamber.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the raw material gas consists of a metal alkoxide.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the raw material gas consists of pentoethoxytantalum, and the oxidizing gas consists of a substance selected from the group consisting of O2, O3, N2O, NO, NO2, and a vaporized alcohol.

### Claim 10 (depends on 7)

The method according to claim 7, wherein the steps of performing the deposition process and the reformation process are repeated a plurality of times.

### Claim 11

A single-substrate-processing-film-forming method comprising the steps of:
performing a deposition process of depositing a film consisting essentially of an amorphous metal oxide on a target substrate by means of CVD; and
performing a reformation process of removing an organic impurity contained in the film,
wherein the deposition process comprises a step of supplying a raw material gas, which offers a metal of the metal oxide by decomposition, and an oxidizing gas into a process chamber accommodating the target substrate, while exhausting the process chamber,
the reformation process comprises a step of supplying an excited oxygen gas as a reforming gas into a process chamber accommodating the target substrate, while exhausting the process chamber, the reforming gas being set to have a concentration of ions and electrons not more than 105/cm3, and
the method comprises a step of performing the deposition process and the reformation process at substantially the same time, by supplying the raw material gas, the oxidizing gas, and the reforming gas into the process chamber at substantially the same time.

### Claim 12 (depends on 11)

The method according to claim 11, further comprising steps of:
exciting oxygen gas until generating plasma by an exciting mechanism disposed outside the process chamber; and
preparing the reforming gas by mixing the excited oxygen gas with a non-excited oxygen gas to reduce a concentration of ions and electrons in the excited oxygen gas.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the reforming gas contains a catalytic gas for accelerating activation of the oxygen gas at a concentration of from 0 to 15 flow-rate %.

### Claim 14 (depends on 13)

The method according to claim 13, wherein the catalytic gas consists of N2.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the deposition and reformation processes comprise a step of heating the film to a temperature lower than a crystallization temperature of the metal oxide.

### Claim 16 (depends on 11)

The method according to claim 11, wherein the raw material gas consists of a metal alkoxide.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the raw material gas consists of pentoethoxytantalum, and the oxidizing gas consists of a substance selected from the group consisting of O2, O3, N2O, NO, NO2, and a vaporized alcohol.

### Claim 18

A single-substrate-processing-film-forming apparatus comprising:
an airtight process chamber configured to accommodate a target substrate having a film consisting essentially of an amorphous metal oxide thereon;
a worktable configured to support a target substrate within the process chamber;
a heater configured to heat the film while the target substrate is placed on the worktable;
an exhaust section configured to exhaust the process chamber; and
a reforming gas supply section configured to supply excited oxygen gas into the process chamber, the excited oxygen gas being used as a reforming gas for performing a reformation process of removing an organic impurity contained in the film, the reforming gas being set to have a concentration of ions and electrons not more than 105/cm3.

### Claim 19 (depends on 18)

The apparatus according to claim 18, wherein the reforming gas supply section comprises:
an exciting mechanism disposed outside the process chamber and configured to excite oxygen gas until generating plasma; and
a mixing mechanism configured to prepare the reforming gas by mixing the excited oxygen gas with a non-excited oxygen gas to reduce a concentration of ions and electrons in the excited oxygen gas.

### Claim 20 (depends on 18)

The apparatus according to claim 18, further comprising a deposition gas supply section configured to supply a raw material gas, which offers a metal of the metal oxide by decomposition, and an oxidizing gas into the process chamber, so as to deposit the film on the target substrate by means of CVD.