# US 2001/0044373 A1 · Method for forming a membrane electrode diffusion assembly for use in an ion exchange membrane fuel cell

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0044373 A1
- Document ID: US20010044373A1
- Status: Published application
- Kind: A1
- Application number: 09/792,085
- Filed: 2001-02-23
- Published: 2001-11-22
- Earliest claimed: 2000-05-17
- Assignees: Avista Laboratories, Inc.
- Inventors: David R. Lott; P. David DeVries
- Web page: https://patentgrep.com/patent/US20010044373A1

## CPC

- H01M 8/0258: characterised by the configuration of channels, e.g. by the flow field of the reactant or coolant
- H01M 8/0247: characterised by the form (characterised by a channel configuration H01M8/0258)
- H01M 8/04007: related to heat exchange
- H01M 8/04089: of gaseous reactants
- H01M 8/1004: characterised by membrane-electrode assemblies [MEA] (H01M8/12 takes precedence)
- H01M 8/247: Arrangements for tightening a stack, for accommodation of a stack in a tank or for assembling different tanks
- Y02E 60/50: Fuel cells
- Y10S 429/90: Fuel cell including means for power conditioning, e.g. conversion to AC
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for forming a membrane electrode diffusion assembly for use in an ion exchange membrane fuel cell is described and which includes, providing an ion conducting electrolyte membrane having opposite sides; and applying a first diffusion layer to one of the opposite sides of the ion conducting electrolyte membrane by the application of force sufficient to fabricate a resulting membrane electrode diffusion assembly which has an optimal operational temperature range when utilized in an ion exchange membrane fuel cell of less than about 95 degrees C.

## Claims

### Claim 1

A method for forming a membrane electrode diffusion assembly for use in an ion exchange membrane fuel cell, comprising:
providing an ion conducting electrolyte membrane having opposite sides; and
applying a first diffusion layer to one of the opposite sides of the ion conducting electrolyte membrane by the application of force sufficient to fabricate a resulting membrane electrode diffusion assembly which has an optimal operational temperature range when utilized in an ion exchange membrane fuel cell of less than about 95 degrees C.

### Claim 2 (depends on 1)

A method as claimed in claim 1, and further comprising:
before applying the first diffusion layer, and after providing the ion conducting electrolyte membrane, providing anode and cathode electrodes which are individually located in covering relation on the opposite sides of the ion conducting electrolyte membrane, and wherein the first diffusion layer is located in covering relation relative to the anode and cathode electrodes.

### Claim 3 (depends on 1)

A method as claimed in claim 1, wherein the first diffusion layer is applied with a force of at least about 400 pounds to about 10,000 pounds per square inch.

### Claim 4 (depends on 1)

A method as claimed in claim 1, and further providing anode and cathode electrodes individually disposed on the opposite sides of the ion conducting electrolyte membrane, and wherein the first diffusion layer is applied to the side of the ion conducting electrolyte membrane bearing the anode electrode with a force of at least about 400 pounds to about 10,000 pounds per square inch.

### Claim 5 (depends on 1)

A method as claimed in claim 1, and further providing anode and cathode electrodes individually disposed on the opposite sides of the ion conducting electrolyte membrane, and wherein the first diffusion layer is applied to the side of the ion conducting electrolyte membrane bearing the cathode electrode with a force of at least about 400 pounds to about 10,000 pounds per square inch.

### Claim 6 (depends on 1)

A method as claimed in claim 1, and further providing anode and cathode electrodes individually disposed on the opposite sides of the ion conducting electrolyte membrane, and wherein the first diffusion layer is applied concurrently to both sides of the ion conducting electrolyte membrane with a force of at least about 400 pounds to about 10,000 pounds per square inch.

### Claim 7 (depends on 1)

A method as claimed in claim 1, and further comprising:
providing anode and cathode electrodes individually disposed on the opposite sides of the ion conducting electrolyte membrane, and wherein the first diffusion layer comprises carbon and a fluropolymer which is applied to both sides of the ion conducting electrolyte membrane, and in covering relation relative the respective anode and cathode electrodes with a force of at least about 400 to about 10,000 pounds per square inch.

### Claim 8 (depends on 6)

A method as claimed in claim 6, and further comprising:
after the step of providing the ion conducting electrolyte membrane and applying the first diffusion layer thereto, providing a permeable substrate; and
applying a porous layer to the porous substrate to form a second diffusion layer.

### Claim 9 (depends on 6)

A method as claimed in claim 6, and further comprising:
after the step of applying the first diffusion layer, providing a permeable substrate; and
applying a porous layer to the permeable substrate and which comprises at least about 20% to about 90% by weight of particulate carbon and a hydrophobic binding resin which forms a second diffusion layer.

### Claim 10 (depends on 9)

A method as claimed in claim 9, wherein the step of applying the porous layer to the permeable substrate to form the second diffusion layer further comprises:
applying the porous layer to the permeable substrate in the form of a slurry which is applied in successive coats to form a hydrophobic gradient.

### Claim 11 (depends on 1)

A method as claimed in claim 1, and further comprising:
before the step of applying the first diffusion layer, providing a permeable substrate; and
applying a porous layer thereto in the form of a slurry which comprises carbon and a hydrophobic binding resin to form a second diffusion layer which has a hydrophobic gradient; and
applying the first diffusion layer to the ion conducting electrolyte membrane with a force of at least about 400 pounds to about 10,000 pounds per square inch, and wherein following the step of applying force to the first diffusion layer, positioning the second diffusion layer in covering relation relative to the first diffusion layer.

### Claim 12 (depends on 1)

A method as claimed in claim 1, and further comprising:
before the step of applying the first diffusion layer, heating the first diffusion layer to a predetermined temperature, and wherein the first diffusion layer is applied to the electrolyte membrane with a force of at least about 400 pounds per square inch to about 10,000 pounds per square inch.

### Claim 13 (depends on 1)

A method as claimed in claim 1, and wherein the first diffusion layer comprises carbon and a fluropolymer, and wherein before the step of applying the first diffusion layer, heating the first diffusion layer to a temperature of about 100 degrees C. to about 500 degrees C. in the presence of air; and wherein the first diffusion layer is applied to the ion conducting electrolyte membrane with a force of at least about 400 pounds to about 10,000 pounds per square inch.

### Claim 14 (depends on 1)

A method as claimed in claim 1, and further comprising:
before the step of applying the first diffusion layer, providing anode and cathode electrodes individually disposed on the opposite sides of the ion conducting electrolyte membrane, and wherein the first diffusion layer comprises carbon and a fluropolymer;
heating the first diffusion layer to a temperature of about 100 degrees C. to about 500 degrees C., and wherein after the step of heating the first diffusion layer, positioning the first diffusion layer in covering relation relative to the respective anode and cathode electrodes; and
applying the first diffusion layer to the ion conducting electrolyte membrane by the application of a force of about 400 pounds to about 10,000 pounds per square inch to the ion conducting electrolyte membrane and the first diffusion layer.

### Claim 15 (depends on 14)

A method as claimed in claim 14, and further comprising:
after the step of applying the first diffusion layer, providing a permeable substrate; and
applying a porous layer to the permeable substrate and which comprises at least about 20% to about 90% by weight of particulate carbon and a hydrophobic binding resin which forms a resulting second diffusion layer; and
positioning the second diffusion layer in covering relation relative to the first diffusion layer.

### Claim 16 (depends on 15)

A method as claimed in claim 15, wherein the step of applying the porous layer to the permeable substrate further comprises:
applying the porous layer in a slurry onto the permeable substrate in successive coats to form a hydrophobic gradient.

### Claim 17 (depends on 16)

A method as claimed in claim 16, wherein each successive coat of the porous layer forming the second diffusion layer is air dried prior to the application of a subsequent coat.

### Claim 18

A method for forming a membrane electrode diffusion assembly for use in an ion exchange membrane fuel, comprising:
providing an ion conducting electrolyte membrane having opposite anode and cathode sides;
affixing an anode and cathode electrode on the respective anode and cathode sides;
positioning a first diffusion layer on one of the anode and/or cathode sides of the ion conducting electrolyte membrane and in covering relation over the respective anode and/or cathode electrode; and
applying a force of at least about 400 pounds to about 10,000 pounds per square inch to the first diffusion layer to affix the first diffusion layer on the ion conducting electrolyte membrane to form a membrane electrode diffusion assembly.

### Claim 19 (depends on 18)

A method as claimed in claim 18, and wherein the membrane electrode diffusion assembly is incorporated into an ion exchange membrane fuel cell which has a cathode air flow, and wherein the ion exchange membrane fuel cell has a power output, and wherein the method further comprises:
exposing the cathode side of the membrane electrode diffusion assembly to the cathode air flow, and wherein the power output of the ion exchange membrane fuel cell is not substantially degraded upon exposure of the cathode side of the membrane electrode diffusion assembly to cathode air flow temperatures of less than about 95 degrees C.

### Claim 20 (depends on 19)

A method as claimed in claim 19, and wherein the first diffusion layer comprises carbon and a fluropolymer, and wherein before the step of affixing the first diffusion layer the method further comprises:
heating the first diffusion layer to a temperature of about 100 degrees C. to about 500 degrees C. in the presence of air.

### Claim 21 (depends on 20)

A method as claimed in claim 20 and further comprising:
after the step of providing the ion conducting electrolyte membrane and affixing the first diffusion layer thereto, providing a permeable substrate; and
applying a porous layer to the permeable substrate to form a second diffusion layer.

### Claim 22 (depends on 20)

A method as claimed in claim 20, and further comprising:
after the step of applying the first diffusion layer, providing a permeable substrate; and
applying a porous layer to the permeable substrate and which comprises at least about 20% to about 90% by weight of particulate carbon and a hydrophobic binding resin, and which forms a second diffusion layer.

### Claim 23 (depends on 22)

A method as claimed in claim 22, wherein the step of applying the porous layer to the permeable substrate further comprises:
applying the porous layer in the form of a slurry to the permeable substrate in successive coats to form a resulting hydrophobic gradient in the second diffusion layer.

### Claim 24

A method for forming a membrane electrode diffusion assembly for use in an ion exchange membrane fuel cell, comprising:
first, providing an ion conducting electrolyte membrane having opposite anode and cathode sides;
second, providing anode and cathode electrodes which are individually affixed on, and located at least in partial covering relation relative to the respective anode and cathode sides of the electrolyte membrane;
third, providing a first diffusion layer comprising carbon and a fluropolymer, and then heating the first diffusion layer to a temperature of about 100 degrees C. to about 500 degrees C. for a predetermined period of time in the presence of air;
fourth, affixing the previously heated first diffusion layer in at least partial covering relation relative to each of the anode and cathode electrodes by the application of pressure in the amount of about 400 pounds to about 10,000 pounds per square inch of surface area of the first diffusion layer;
providing a permeable substrate having a predetermined thickness dimension and opposite sides;
preparing a slurry comprising at least about 20% to about 90% by weight of a particulate carbon and a hydrophobic binding resin dispersed in a water solution, and applying the slurry to coat one of the sides of the permeable substrate;
air drying the coated side of the porous substrate, and after the step of air drying the coated side, applying additional coats of the slurry, each separated by the aforementioned air drying step, to form a second diffusion layer having a resulting hydrophobic gradient; and
positioning the second diffusion layer in juxtaposed, covering relation relative to the first diffusion layer.