# US 2001/0044080 A1 · Method for forming a finely patterned photoresist layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0044080 A1
- Document ID: US20010044080A1
- Status: Published application
- Kind: A1
- Application number: 09/839,200
- Filed: 2001-04-23
- Published: 2001-11-22
- Earliest claimed: 2000-04-26
- Assignees: Tokyo Ohka Kogyo Co., Ltd.
- Inventors: Etsuko Iguchi; Kazumasa Wakiya
- Web page: https://patentgrep.com/patent/US20010044080A1

## CPC

- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- Y10S 430/151: Matting or other surface reflectivity altering material
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

The invention discloses an improvement in the photolithographic patterning method of a photoresist layer formed on a substrate surface with intervention of an anti-reflection coating film, in which the refractive index and the light-absorption coefficient of the anti-reflection coating film are controlled in such a way that, in a graph prepared by plotting the thickness of the anti-reflection coating film taken as the abscissa values and the reflectivity of the light for patterning exposure at the interface between the anti-reflection coating film and the photoresist layer thereon taken as the ordinate values, the range of the variation in the film thickness corresponding to an increment of 0.01 in the reflectivity in the vicinity of the minimum point on the thickness vs. reflectivity curve does not exceed ±0.01 μm.

## Claims

### Claim 1

In a method for the formation of a patterned photoresist layer on the surface of a substrate with intervention of an anti-reflection film by a photolithographic patterning process comprising the steps of forming an anti-reflection coating film containing a resinous ingredient, a highly light-absorbing compound and a thermally crosslinkable compound on the substrate surface, forming a photoresist layer on the anti-reflection coating film, patternwise exposing the photoresist layer to a light and subjecting the patternwise exposed photoresist layer to a development treatment, the improvement which comprises controlling the refractive index and the light-absorption coefficient of the anti-reflection coating film in such a way that, in a graph prepared by plotting the thickness of the anti-reflection coating film taken as the abscissa values and the reflectivity of the light for patterning exposure at the interface between the anti-reflection coating film and the photoresist layer thereon taken as the ordinate values, the range of the variation in the film thickness corresponding to an increment of 0.01 in the reflectivity in the vicinity of the minimum point on the thickness vs. reflectivity curve does not exceed ±0.01 μm.

### Claim 2 (depends on 1)

The improvement as claimed in claim 1 in which the reflectivity at the minimum point on the thickness vs. reflectivity curve does not exceed 0.01.

### Claim 3 (depends on 1)

The improvement as claimed in claim 1 in which the refractive index and light-absorption coefficient of the anti-reflection coating film are controlled by selecting the kinds and contents of the resinous ingredient contained therein.

### Claim 4 (depends on 1)

The improvement as claimed in claim 1 in which the refractive index and light-absorption coefficient of the anti-reflection coating film are controlled by selecting the kinds and contents of the highly light-absorbing compound contained therein.

### Claim 5 (depends on 1)

The improvement as claimed in claim 1 in which the refractive index and light-absorption coefficient of the anti-reflection coating film are controlled by selecting the kinds and contents of the thermally crosslinkable compound contained therein.