# US 2001/0043903 A1 · Surface impurity-enriched diamond and method of making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0043903 A1
- Document ID: US20010043903A1
- Status: Published application
- Kind: A1
- Application number: 09/783,441
- Filed: 2001-02-14
- Published: 2001-11-22
- Earliest claimed: 1996-11-12
- Assignees: Diamond Innovations, Inc.
- Inventors: Marl Philip D'Evelyn; Dong-Sil Park; Thomas Richard Anthony; Clifford Lawrence Spiro; Yue Meng; Christopher Allen Long
- Web page: https://patentgrep.com/patent/US20010043903A1

## CPC

- C30B 25/02: Epitaxial-layer growth
- B01J 3/062: {characterised by the composition of the materials to be processed}
- C01B 32/25: Diamond
- C01B 32/26: Preparation (by using ultra-high pressure B01J3/06; by crystal growth C30B29/04)
- C30B 29/04: Diamond
- C30B 31/00: Diffusion or doping processes for single crystals or homogeneous polycrystalline material with defined structure; Apparatus therefor
- B01J 2203/061: Graphite
- B01J 2203/062: Diamond
- B01J 2203/0655: Diamond
- B01J 2203/068: Crystal growth
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An element-doped diamond crystal is disclosed herein. The crystal includes at least one dopant element which has a greater concentration toward or near an outermost surface of the crystal than in the center of the crystal. The concentration of the dopant element is at a local minimum at least about 5 micrometers below the surface. The concentration-profile of the dopant element for these diamond crystals causes an expansion of the diamond lattice, thereby generating tangential compressive stresses at the surface of the diamond crystal. These stresses beneficially increase the compressive fracture strength of the diamond.

## Claims

### Claim 1

A three-dimensional faceted diamond crystal, comprising at least one dopant element which has a greater concentration toward or near an outermost surface of the crystal than in the center of the crystal, wherein the concentration of the dopant element is at a local minimum at least about 5 micrometers below the surface.

### Claim 2 (depends on 1)

The diamond crystal of claim 1, wherein the dopant element is selected from the group consisting of boron, nitrogen, hydrogen, lithium, nickel, cobalt, sodium, potassium, aluminum, phosphorous, oxygen, and mixtures of any of the foregoing.

### Claim 3 (depends on 2)

The diamond crystal of claim 2, wherein the dopant element is selected from the group consisting of boron, nitrogen, hydrogen, and mixtures of any of the foregoing.

### Claim 4 (depends on 1)

The diamond crystal of claim 1, wherein the dopant element is boron, aluminum, or mixtures of any of the foregoing.

### Claim 5 (depends on 4)

The diamond crystal of claim 4, wherein nitrogen is dissolved in the crystal, and wherein the concentration of nitrogen exceeds the total concentration of dopant elements.

### Claim 6 (depends on 5)

The diamond crystal of claim 5, wherein the concentration of nitrogen exceeds the total concentration of dopant elements by at least about 5 parts per million.

### Claim 7 (depends on 1)

A diamond crystal according to claim 1, wherein the dopant element is selected from the group consisting of nitrogen, hydrogen, nickel, cobalt, oxygen, and mixtures of any of the foregoing.

### Claim 8 (depends on 1)

A diamond crystal according to claim 1, wherein the dopant-element concentration within an outermost section of about 3 to about 50 micrometers of the crystal is in an amount of about 40 to about 10,000 parts per million.

### Claim 9 (depends on 1)

A diamond crystal according to claim 1, wherein the concentration of the dopant element is at a local maximum at a distance less than about 5 micrometers from the surface of the crystal.

### Claim 10 (depends on 1)

A diamond crystal according to claim 1, wherein the concentration of the dopant element causes an expansion of the diamond lattice toward or near the outermost surface of the crystal, thereby generating tangential compressive stresses at the surface of the diamond crystal.

### Claim 11 (depends on 10)

The diamond crystal of claim 10, wherein the tangential compressive stresses are in the range of about 10 to about 5000 megapascals (MPa).

### Claim 12 (depends on 10)

The diamond crystal of claim 10, wherein the generation of tangential compressive stresses increases the compressive fracture strength of the diamond, as compared to a diamond crystal in which the diamond lattice is not substantially expanded.

### Claim 13 (depends on 12)

The diamond crystal of claim 12, wherein the increase in compressive fracture strength is at least about 2%.

### Claim 14 (depends on 1)

An article of manufacture which comprises the diamond crystal of claim 1.

### Claim 15

A three-dimensional faceted diamond crystal containing at least one dopant element, wherein the concentration of the dopant element is greater toward or near the outermost surface of the crystal than in the center of the crystal, said crystal being further characterized by a tangential compressive stress at a surface of said crystal of up to about 5000 megapascals.

### Claim 16 (depends on 15)

The diamond crystal of claim 15, having a diameter up to about 2 centimeters.

### Claim 17 (depends on 15)

The diamond crystal of claim 15, wherein said crystal is a single crystal.

### Claim 18 (depends on 15)

The diamond crystal of claim 15, having one or more twin planes.

### Claim 19 (depends on 15)

The diamond crystal of claim 15, wherein the dopant element is selected from the group consisting of boron, nitrogen, hydrogen, lithium, nickel, cobalt, sodium, potassium, aluminum, phosphorous, oxygen, and mixtures thereof.

### Claim 20 (depends on 15)

The diamond crystal of claim 15, comprising a coated film of doped diamond about 3 to about 50 micrometers thick on an outer surface of the crystal, wherein the concentration of the dopant element in the coated film is about 40 to about 10,000 parts per million greater than the concentration of the dopant element in the outer surface of said underlying diamond crystal.

### Claim 21 (depends on 20)

The diamond crystal of claim 20, wherein the dopant element is diffused into the diamond crystal, and the concentration of the dopant element is about 40 to about 10,000 parts per million at a depth of about 3 micrometers to about 50 micrometers within said diamond crystal.

### Claim 22 (depends on 15)

The diamond crystal of claim 15, wherein a range of tangential compressive stresses of about 10 to about 5000 megapascals is superimposed on preexisting tangential tensile stresses in said diamond crystal.

### Claim 23

A method of making a diamond crystal having a tangential compressive stress on a surface up to about 5000 megapascals, comprising the step of:
growing a three-dimensional diamond crystal by a High Temperature High Pressure process, wherein said crystal includes impurities that enrich an outer surface of the crystal in a concentration that is about 40 parts per million to about 10,000 parts per million, at a depth from the outer surface of about 3 micrometers to about 50 micrometers.

### Claim 24 (depends on 23)

The method of claim 23, wherein the growth temperature for the diamond crystals is reduced by at least about 10° C. after about 80% of the normal growth cycle is completed.