# US 2001/0041416 A1 · Method of fabricating semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0041416 A1
- Document ID: US20010041416A1
- Status: Published application
- Kind: A1
- Application number: 09/897,615
- Filed: 2001-07-03
- Published: 2001-11-15
- Earliest claimed: 1995-12-05
- Assignees: Hitachi, Ltd.
- Inventors: Kazuyoshi Torii; Hiroshi Kawakami; Hiroshi Miki; Keiko Kushida; Yoshihisa Fujisaki; Masahiro Moniwa
- Web page: https://patentgrep.com/patent/US20010041416A1

## CPC

- H10D 1/682: {having dielectrics comprising perovskite structures}
- H10B 12/033: {the capacitor extending over the transistor}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor device having a bottom electrode, a ferroelectric film, and a top electrode formed on a semiconductor substrate, wherein the angle of each of the main cross sectional sides of the ferroelectric film relative to the main surface of the semiconductor substrate is less than 75 degrees. Forming the ferroelectric film into the trapezoid in cross section having such an angle provides a microscopic capacitor without electrical short-circuit between the top and bottom electrodes if the top electrode, the ferroelectric film, and the bottom electrode are etched with single photolithography process step. The novel technique implements a microscopic memory cell structure suitable for highly integrated memory devices.

## Claims

### Claim 1

A method of fabricating a semiconductor device comprising the steps of:
forming a capacitor composed of a platinum bottom electrode, a dielectric film and a top electrode on a substrate; and
etching said capacitor;
wherein the etching is performed such that an angle of each of main cross sectional sides of said dielectric film relative to a main surface of said substrate is not less than 45 degrees and not greater than 75 degrees.

### Claim 2 (depends on 1)

A method of fabricating a semiconductor device as claimed in claim 1, wherein the etching is performed such that an angle of each of main cross sectional sides of said bottom electrode to the main surface of the substrate is not less than 45 degrees and not greater than 75 degrees.

### Claim 3 (depends on 2)

A method of fabricating a semiconductor device as claimed in claim 2, wherein the etching is performed such that an angle of each of main cross sectional sides of said top electrode to the main surface of the substrate is not less than 45 degrees and not greater than 75 degrees.

### Claim 4 (depends on 1)

A method of fabricating a semiconductor device as claimed in claim 1, wherein the etching is performed such that an angle of each of main cross sectional sides of said top electrode to the main surface of the substrate is not less than 45 degrees and not greater than 75 degrees.

### Claim 5 (depends on 1)

A method of fabricating a semiconductor device as claimed in claim 1, wherein said angle of each of said main cross sectional sides of said dielectric film relative to said main surface of said substrate is not less than 60 degrees and not greater than 75 degrees.

### Claim 6 (depends on 5)

A method of fabricating a semiconductor device as claimed in claim 5, wherein the angle of each of the main cross sectional sides of said bottom electrode to the main surface of the substrate is not less than 60 degrees and not greater than 75 degrees.

### Claim 7 (depends on 6)

A method of fabricating a semiconductor device as claimed in claim 6, wherein the angle of each of the main cross sectional sides of said top electrode to the main surface of the substrate is not less than 60 degrees and not greater than 75 degrees.

### Claim 8 (depends on 5)

A method of fabricating a semiconductor device as claimed in claim 5, wherein the angle of each of the main cross sectional sides of said top electrode to the main surface of the substrate is not less than 60 degrees and not greater than 75 degrees.