# US 2001/0039790 A1 · Coalesced multifilament spandex and method for its preparation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0039790 A1
- Document ID: US20010039790A1
- Status: Published application
- Kind: A1
- Application number: 09/791,919
- Filed: 2001-02-23
- Published: 2001-11-15
- Earliest claimed: 1996-07-24
- Assignees: DuPont-Toray Co. Ltd.
- Inventors: Masao Umezawa; Hideki Nakanishi; Toshikazu Matsuda
- Web page: https://patentgrep.com/patent/US20010039790A1

## CPC

- D01F 6/70: from polyurethanes
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS

## Abstract

The present invention provides a process whereby high quality, well-coalesced spandex can be made by dry-spinning a high-melting thermoplastic polyurethane, bundling the as-spun filaments into a side-by-side relationship, and passing the bundled filaments over or through a guide. The spandex made by this method has high-heat settability, high denier uniformity, good knittability and weavability, and provides fabrics having good surface uniformity.

## Claims

### Claim 1

A method for preparing a coalesced multifilament spandex, the improvement comprising:
dry spinning a thermoplastic polyurethane to form as-spun filaments;
bundling a plurality of the as-spun filaments in a first guide;
passing the bundled filaments through a second guide to form a coalesced multifilament, neither the first guide nor the second guide creating false-twist in the filaments; and
winding up the coalesced multifilament.

### Claim 2 (depends on 1)

The method of claim 1 wherein the thermoplastic polyurethane has a melting point in the range of about 160° C. to 250° C. and a glass-transition temperature no higher than about 0° C.

### Claim 3 (depends on 2)

The method of claim 2 wherein the thermoplastic polyurethane has a melting point in the range of about 230° C. to 250° C.

### Claim 4 (depends on 1)

The method of claim 1 wherein the first guide is a comb guide and the second guide is a pigtail guide, a closed-ring guide, or a slit guide.

### Claim 5 (depends on 1)

The method of claim 1 wherein the polyurethane is a polyurethaneurea.

### Claim 6 (depends on 1)

A coalesced multifilament spandex prepared by the method of claim 1.

### Claim 7 (depends on 2)

A coalesced multifilament spandex prepared by the method of claim 2.

### Claim 8 (depends on 5)

A coalesced multifilament spandex prepared by the method of claim 5.