# US 2001/0036755 A1 · Method of fabricating semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0036755 A1
- Document ID: US20010036755A1
- Status: Published application
- Kind: A1
- Application number: 09/842,797
- Filed: 2001-04-27
- Published: 2001-11-01
- Earliest claimed: 2000-04-28
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Koichiro Tanaka
- Web page: https://patentgrep.com/patent/US20010036755A1

## CPC

- H10P 14/3808: {using laser beams}
- H10D 30/0314: {of lateral top-gate TFTs comprising only a single gate}
- H10D 30/0321: {comprising silicon, e.g. amorphous silicon or polysilicon}
- H10D 30/6715: {characterised by the doping profiles, e.g. having lightly-doped source or drain extensions}
- H10D 30/6733: {Multi-gate TFTs}
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/381: {Beam shaping, e.g. using a mask}
- H10P 14/382: {Scanning of a beam}
- H10P 34/42: with electromagnetic radiation, e.g. laser annealing (laser cutting H10P54/20)
- H10D 30/6721: {having lightly-doped extensions consisting of multiple lightly doped zones or having non-homogeneous dopant distributions, e.g. graded LDD}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method of promoting crystalline performance of a region of irradiating laser beam by a plurality of times is provided. A first crystalline region is formed by subjecting a portion of an amorphous semiconductor film to laser annealing by using laser beam having a wavelength in a range of 370 nm through 650 nm. It is preferable in carrying out laser annealing to irradiate laser beam after shaping the laser beam into linear beam having a shape at an irradiated face or a vicinity thereof in a linear shape by using an optical system. A second crystalline region is formed by subjecting a region including a portion of the first crystalline region to laser annealing. Crystalline performance of the first crystalline region formed as above, crystalline performance of the second crystalline region and crystalline performance of a region overlapped with the first crystalline region and the second crystalline region are the same and a crystalline semiconductor film having excellent crystalline performance can be provided. When the crystalline semiconductor film constitutes an activation layer of TFT and electric properties of the TFT are measured, there are provided excellent properties having small dispersion.

## Claims

### Claim 1

A method of fabricating a semiconductor device comprising the steps of:
forming a first crystalline region by irradiating a laser beam to an amorphous semiconductor film while relatively moving the laser beam with respect to said amorphous semiconductor film; and
forming a second crystalline region by irradiating the laser beam to a region including a portion of the first crystalline region of the amorphous semiconductor film formed with the first crystalline region by relatively moving the laser beam with respect to said region including a portion of the first crystalline region;
wherein a wavelength of the laser beam falls in a range 1.5. of 370 nm through 650 nm.

### Claim 2

A method of fabricating a semiconductor device comprising the steps of:
forming a first crystalline region by irradiating a laser beam having a shape at an irradiated face or a vicinity thereof in a linear or a rectangular shape to an amorphous semiconductor film while relatively moving the laser beam with respect to said amorphous semiconductor film; and
forming a second crystalline region by irradiating the laser beam to a region including a portion of the first crystalline region of the amorphous semiconductor film formed with the first crystalline region while relatively moving the laser beam with respect to said region including a portion of the first crystalline region;
wherein a wavelength of the laser beam falls in a range of 370 nm through 650 nm.

### Claim 3

A method of fabricating a semiconductor device comprising the steps of:
forming a first crystalline region by irradiating a laser beam having a shape at an irradiated face or a vicinity thereof in a linear or rectangular shape to an amorphous semiconductor film while relatively moving the laser beam in a short direction of the laser beam with respect to said amorphous semiconductor film; and
forming a second crystalline region by irradiating the laser beam to a region including a portion of the first crystalline region of the amorphous semiconductor film formed with the first crystalline region while relatively moving the laser beam in the short direction of the laser beam with respect to said region including a portion of the first crystalline region;
wherein a wavelength of the laser beam falls in a range of 370 nm through 650 nm.

### Claim 4

A method of fabricating a semiconductor device comprising:
a first step of forming a first crystalline semiconductor film by partially crystallizing an amorphous semiconductor film by a heating treatment; and
a second step of forming a second crystalline semiconductor film by irradiating a laser beam to the crystalline semiconductor film;
wherein the second step comprises the steps of:
forming a first crystalline region by irradiating the laser beam to the first crystalline semiconductor film while relatively moving the laser beam with respect to the first crystalline semiconductor film; and
forming a second crystalline region by irradiating the laser beam to a region including a portion of the first crystalline region of the first crystalline semiconductor film formed with the first crystal line region while relatively moving the laser beam with respect to said region including a portion of the first crystalline region of the first crystalline semiconductor film; and
wherein a wavelength of the laser beam falls in a range of 370 nm through 650 nm.

### Claim 5

A method of fabricating a semiconductor device comprising:
a first step of forming a first crystalline semiconductor film by partially crystallizing an amorphous semiconductor film by a heating treatment; and
a second step of forming a second crystalline semiconductor film by irradiating a laser beam having a shape at an irradiated face or a vicinity thereof in a linear or a rectangular shape to the first crystalline semiconductor film;
wherein the second step comprises the steps of:
forming a first crystalline region by irradiating the laser beam to the first crystalline semiconductor film by relatively moving the laser beam with respect to the first crystalline semiconductor film; and
forming a second crystalline region to a region including a portion of the crystalline region of the first crystalline semiconductor film formed with the first crystalline region by relatively moving the laser beam with respect to said region including a portion of the crystalline region of the first crystalline semiconductor film; and
wherein a wavelength of the laser beam falls in a range of 370 nm through 650 nm.

### Claim 6

A method of fabricating a semiconductor device comprising:
a first step of forming a first crystalline semiconductor film by partially crystallizing an amorphous semiconductor film by a heating treatment; and
a second step of forming a second crystalline semiconductor film by irradiating a laser beam having a shape at an irradiated face or a vicinity thereof in a linear or a rectangular shape to the first crystalline semiconductor film while relatively moving the laser beam in a short direction of the laser beam with respect to the first crystalline semiconductor film;
wherein the second step comprises the steps of:
forming a first crystalline region by irradiating the laser beam to the first crystalline semiconductor film while relatively moving the laser beam in the short direction of the laser beam with respect to the first crystalline semiconductor film; and
forming a second crystalline region by irradiating the laser beam to a region including a portion of the first crystalline region of the first crystalline semiconductor film formed with the first crystalline region while relatively moving the laser beam in the short direction of the laser beam with respect to the region including a portion of the first crystalline region of the first crystalline semiconductor film; and
wherein a wavelength of the laser beam falls in a range of 370 nm through 650 nm.

### Claim 7 (depends on 1)

The method of fabricating a semiconductor device according to claim 1, wherein a crystalline performance of the first crystalline region, a crystalline performance of the second crystalline region and a crystalline performance of a region overlapped with the first crystalline region and the second crystalline region are the same.

### Claim 8 (depends on 2)

The method of fabricating a semiconductor device according to claim 2, wherein a crystalline performance of the first crystalline region, a crystalline performance of the second crystalline region and a crystalline performance of a region overlapped with the first crystalline region and the second crystalline region are the same.

### Claim 9 (depends on 3)

The method of fabricating a semiconductor device according to claim 3, wherein a crystalline performance of the first crystalline region, a crystalline performance of the second crystalline region and a crystalline performance of a region overlapped with the first crystalline region and the second crystalline region are the same.

### Claim 10 (depends on 4)

The method of fabricating a semiconductor device according to claim 4, wherein a crystalline performance of the first crystalline region, a crystalline performance of the second crystalline region and a crystalline performance of a region overlapped with the first crystalline region and the second crystalline region are the same.

### Claim 11 (depends on 5)

The method of fabricating a semiconductor device according to claim 5, wherein a crystalline performance of the first crystalline region, a crystalline performance of the second crystalline region and a crystalline performance of a region overlapped with the first crystalline region and the second crystalline region are the same.

### Claim 12 (depends on 6)

The method of fabricating a semiconductor device according to claim 6, wherein a crystalline performance of the first crystalline region, a crystalline performance of the second crystalline region and a crystalline performance of a region overlapped with the first crystalline region and the second crystalline region are the same.

### Claim 13 (depends on 1)

The method of fabricating a semiconductor apparatus according to claim 1, wherein the semiconductor device is a liquid crystal display apparatus or an EL display apparatus.

### Claim 14 (depends on 2)

The method of fabricating a semiconductor apparatus according to claim 2, wherein the semiconductor device is a liquid crystal display apparatus or an EL display apparatus.

### Claim 15 (depends on 3)

The method of fabricating a semiconductor apparatus according to claim 3, wherein the semiconductor device is a liquid crystal display apparatus or an EL display apparatus.

### Claim 16 (depends on 4)

The method of fabricating a semiconductor apparatus according to claim 4, wherein the semiconductor device is a liquid crystal display apparatus or an EL display apparatus.

### Claim 17 (depends on 5)

The method of fabricating a semiconductor apparatus according to claim 5, wherein the semiconductor device is a liquid crystal display apparatus or an EL display apparatus.

### Claim 18 (depends on 6)

The method of fabricating a semiconductor apparatus according to claim 6, wherein the semiconductor device is a liquid crystal display apparatus or an EL display apparatus.

### Claim 19 (depends on 1)

The method of fabricating a semiconductor device according to claim 1, wherein the semiconductor device is a device selected from the group consisting of: a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book and a portable information terminal.

### Claim 20 (depends on 2)

The method of fabricating a semiconductor device according to claim 2, wherein the semiconductor device is a device selected from the group consisting of: a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book and a portable information terminal.

### Claim 21 (depends on 3)

The method of fabricating a semi conductor device according to claim 3, wherein the semiconductor device is a device selected from the group consisting of: a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book and a portable information terminal.

### Claim 22 (depends on 4)

The method of fabricating a semiconductor device according to claim 4, wherein the semiconductor device is a device selected from the group consisting of: a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book and a portable information terminal.

### Claim 23 (depends on 5)

The method of fabricating a semiconductor device according to claim 5, wherein the semiconductor device is a device selected from the group consisting of: a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book and a portable information terminal.

### Claim 24 (depends on 6)

The method of fabricating a semiconductor device according to claim 6, wherein the semiconductor device is a device selected from the group consisting of: a portable telephone, a video camera, a digital camera, a projector, a goggle type display, a personal computer, a DVD player, an electronic book and a portable information terminal.

### Claim 25 (depends on 1)

The method of fabricating a semiconductor device according to claim 1, wherein said laser beam is a laser beam selected from the group consisting of: a second harmonic of a YAG laser, a second harmonic of a YVO4 laser and a second harmonic of a YLF laser.

### Claim 26 (depends on 2)

The method of fabricating a semiconductor device according to claim 2, wherein said laser beam is a laser beam selected from-the group consisting of: a second harmonic of a YAG laser, a second harmonic of a YVO4 laser and a second harmonic of a YLF laser.

### Claim 27 (depends on 3)

The method of fabricating a semiconductor device according to claim 3, wherein said laser beam is a laser beam selected from the group consisting of: a second harmonic of a YAG laser, a second harmonic of a YVO4 laser and a second harmonic of a YLF laser.

### Claim 28 (depends on 4)

The method of fabricating a semiconductor device according to claim 4, wherein said laser beam is a laser beam selected from the group consisting of: a second harmonic of a YAG laser, a second harmonic of a YVO4 laser and a second harmonic of a YLF laser.

### Claim 29 (depends on 5)

The method of fabricating a semiconductor device according to claim 5, wherein said laser beam is a laser beam selected from the group consisting of: a second harmonic of a YAG laser, a second harmonic of a YVO4 laser and a second harmonic of a YLF laser.

### Claim 30 (depends on 6)

The method of fabricating a semiconductor device according to claim 6, wherein said laser beam is a laser beam selected from the group consisting of: a second harmonic of a YAG laser, a second harmonic of a YVO4 laser and a second harmonic of a YLF laser.