# US 2001/0036725 A1 · Method for fabricating a bottom anti-reflectivity coating layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0036725 A1
- Document ID: US20010036725A1
- Status: Published application
- Kind: A1
- Application number: 09/335,633
- Filed: 1999-06-18
- Published: 2001-11-01
- Earliest claimed: 1999-06-18
- Inventors: STEVEN CHANG
- Web page: https://patentgrep.com/patent/US20010036725A1

## CPC

- H10W 20/0526: {by thermal treatment thereof}
- H10P 50/71: {using masks for conductive or resistive materials}
- H10W 20/038: {covering conductive structures (H10W20/037 takes precedence)}
- H10W 20/048: {by using plasmas or gaseous environments, e.g. by nitriding}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method of fabricating a bottom anti-reflectivity coating (BARC) layer. The method of the invention comprises performing a pre-bake process on a provided titanium nitride layer. Amine ions absorbed into the surface of the titanium nitride layer are thus removed by the high temperature of the pre-bake process. A BARC layer is formed on the titanium nitride layer. A bake step is performed to remove a solvent, which is used for coating the BARC layer. A photoresist layer is coated on the BARC layer. Then, a soft-bake step is performed to remove a solvent, which is used for coating the photoresist layer. A photomask with a pattern is provided over the photoresist layer. An exposure step is performed to transfer the pattern to the photoresist layer. A development step is performed to remove a part of the photoresist layer so that the pattern is shown within the photoresist layer. A hard-bake step is performed to minimize the solvent in the photoresist layer.

## Claims

### Claim 1

A method of fabricating a bottom anti-reflectivity coating layer, comprising the steps of:
providing a titanium nitride layer;
performing a pre-bake process on the titanium nitride layer;
forming a bottom anti-reflectivity coating layer on the titanium nitride layer; and
baking the bottom anti-reflectivity coating layer.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the pre-bake process further comprises steps of:
baking the titanium nitride layer at a high temperature of about 170-300 degrees Celsius; and
cooling the titanium nitride layer to room temperature.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the baking step is performed for about 50-70 seconds.

### Claim 4 (depends on 2)

The method according to claim 2, wherein the cooling step is performed for about 10-30 seconds.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the titanium nitride layer is formed by nitridation.

### Claim 6 (depends on 5)

The method according to claim 5, wherein a gas used for nitridation comprises nitrogen.

### Claim 7 (depends on 5)

The method according to claim 5, wherein a gas used for nitridation comprises ammonia.

### Claim 8

A photolithography process, comprising the steps of:
providing a conductive layer;
baking the conductive layer at a high temperature;
cooling the conductive layer;
coating a bottom anti-reflectivity coating layer on the conductive layer;
baking the bottom anti-reflectivity coating layer;
coating a photoresist layer on the bottom anti-reflectivity coating layer;
performing a soft-bake step on the photoresist layer;
patterning the photoresist layer to remove a part of the photoresist layer; and
performing a hard-bake step on the remaining photoresist layer.

### Claim 9 (depends on 8)

The process according to claim 8, wherein the conductive layer further comprises a titanium nitride layer.

### Claim 10 (depends on 8)

The process according to claim 8, wherein the high temperature for baking the conductive layer is about 170-300 degrees Celsius.

### Claim 11 (depends on 8)