# US 2001/0036708 A1 · Method for forming a capacitor for semiconductor devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0036708 A1
- Document ID: US20010036708A1
- Status: Published application
- Kind: A1
- Application number: 09/751,396
- Filed: 2001-01-02
- Published: 2001-11-01
- Earliest claimed: 1999-12-30
- Assignees: Hyundai Electronics Industries Co., Ltd.
- Inventors: Dong Woo Shin; Seung Joon Jeon
- Web page: https://patentgrep.com/patent/US20010036708A1

## CPC

- H10D 1/696: {comprising multiple layers, e.g. comprising a barrier layer and a metal layer (barrier layers to prevent diffusion of hydrogen or oxygen in perovskite based capacitors H10D1/688)}
- H10D 1/712: {being rough surfaces, e.g. using hemispherical grains}
- H10P 14/418: {the conductive layers comprising transition metals}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a capacitor for a semiconductor device is provided. In the method, a storage electrode is formed of a polysilicon layer, and a hemispherical silicate glass (HSG) layer is optionally formed on the surface of the storage electrode to increase the surface area of the storage electrode. Next, a TaSiN layer as a diffusion barrier is formed, a TaON layer as a dielectric layer is formed, and then a TaSiN layer is formed on the TaON layer. Next, a plate electrode is formed on the TaSiN layer, thereby completing a capacitor. Diffusion of oxygen between the electrodes and the dielectric layer is effectively blocked, so that reduction of capacitance and occurrence of leakage current are prevented. Due to improved dielectric characteristics of the TaON layer, increasing the surface area of the dielectric layer-for example, by forming a HSG layer-may not be required, thereby increasing a processing margin between adjacent capacitors. In addition, the thickness of the TaON layer can be adjusted, thereby raising the breakdown voltage of the TaON layer.

## Claims

### Claim 1

A method for forming a capacitor for a semiconductor device, comprising:
forming a storage electrode on a semiconductor substrate;
forming a hemispherical silicate glass layer on the storage electrode;
forming a first TaSiN layer as a diffusion barrier on the hemispherical silicate glass layer;
forming a TaON layer as a dielectric layer on the first TaSiN layer;
forming a second TaSiN layer as a diffusion barrier on the TaON layer; and
forming a plate electrode on the second TaSiN layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein each of the first TaSiN layer and the second TaSiN layer is formed to have a thickness in a range between about 100 Å and 500 Å using TaCl5 as a solid source material, and SiH4 and NH3 as reaction gases, at a temperature between about 450° C. and 600° C. by low-pressure chemical vapor deposition (LPCVD).

### Claim 3 (depends on 1)

The method of claim 1, after forming each of the first TaSiN layer and the second TaSiN layer, further comprising densifying each of the first and TaSiN layer and the second TaSiN layer in a N2 and H2 atmosphere by a plasma process.

### Claim 4 (depends on 2)

The method of claim 2, wherein the first TaSiN layer and the second TaSiN layer are formed by using Ta(N(CH3)2)5 or Ta(N(C2H5) 2) 5 as a source material.

### Claim 5 (depends on 3)

The method of claim 3, wherein the TaON layer is formed to have a thickness between about 100 Å and 120 Å using Ta(OC2H5)5 as a source material, and NH3 as a reaction gas, by metal organic chemical vapor deposition (MOCVD).

### Claim 6 (depends on 1)

The method of claim 1, wherein
the TaON layer has a total thickness and consists of a first portion and a second portion, the first portion having a thickness of about a half of the total thickness of the TaON layer and the second portion having a thickness of about the other half of the thickness of the total thickness of the TaNO layer, and
forming the TaON layer comprises:
forming the first portion of the TaON layer;
performing a plasma process on the first portion of the TaON layer; and
forming the second portion of the TaON layer.

### Claim 7 (depends on 1)

The method of claim 1, after forming the second TaSiN layer, further comprising performing a rapid annealing process to densify the second TaSiN layer, the TaON layer and the first TaSiN layer.

### Claim 8 (depends on 7)

The method of claim 7, wherein the rapid annealing process is performed at a temperature between about 600° C. and 700° C.

### Claim 9

A method for forming a capacitor for a semiconductor device, comprising:
forming a storage electrode on a semiconductor substrate;
forming a hemispherical silicate glass layer on the storage electrode;
forming a first TaSiN layer as a diffusion barrier;
densifying the first TaSiN layer by a plasma process;
forming a TaON layer as a dielectric layer;
forming a second TaSiN layer as a diffusion barrier on the TaON layer;
densifying the second TaSiN layer by a plasma process; and
densifying the second TaSiN layer, the TaON layer, and the first TaSiN layer by a rapid annealing process; and
forming a plate electrode on the second TaSiN layer.

### Claim 10 (depends on 9)

The method of claim 9, wherein each of the first TaSiN layer and the second TaSiN layer is formed to have a thickness of about 100 Å to 500 Å using TaCl5 as a solid source material, and SiH4 and NH3 as reaction gases, at a temperature between about 450° C. and 600° C. by low-pressure chemical vapor deposition (LPCVD).

### Claim 11 (depends on 9)

The method of claim 9, wherein the first TaSiN layer and the second TaSiN layer are formed of using Ta(N(CH3)2)5 or Ta(N(C2H5)2)5 as a source material.

### Claim 12 (depends on 9)

The method of claim 9, wherein the TaON layer is formed to have a thickness of about 100 Å to 120 Å using Ta(OC2H5)5 as a source material, and NH3 as a reaction gas, by metal organic chemical vapor deposition (MOCVD).

### Claim 13 (depends on 9)

The method of claim 9, wherein
the TaON layer has a total thickness and consists of a first portion and a second portion, the first portion having a thickness of about a half of the total thickness of the TaON layer and the second portion having a thickness of about the other half of the thickness of the total thickness of the TaNO layer, and
forming the TaON layer comprises:
forming the first portion of the TaON layer;
performing a plasma process on the first portion of the TaON layer; and
forming the second portion of the TaON layer.

### Claim 14 (depends on 9)

The method of claim 9, wherein the rapid annealing process is performed at a temperature between about 600° C. and 700° C. in a N2 atmosphere.

### Claim 15

A method for forming a capacitor for a semiconductor device, comprising:
forming a storage electrode on a semiconductor substrate;
forming a hemispherical silicate glass layer on the storage electrode;
forming a first TaSiN layer as a diffusion barrier;
densifying the first TaSiN layer by a plasma process;
forming a first TaON layer, performing a plasma process on the first TaON layer, and forming a second TaON layer on the first TaON layer, the first and second TaON layers serving as a dielectric layer;
forming a second TaSiN layer as a diffusion barrier on the second TaON layer;
densifying the second TaSiN layer by a plasma process; and
densifying the second TaSiN layer, the second and first TaON layers, and the first TaSiN layer by a rapid annealing process; and
forming a plate electrode on the second TaSiN layer.

### Claim 16 (depends on 15)

The method of claim 15, wherein each of the first TaSiN layer and the second TaSiN layer is formed to have a thickness of about 100 Å to 500 Å using TaCl5 as a solid source material, and SiH4 and NH3 as reaction gases, at a temperature between about 450° C. and 600° C. by low-pressure chemical vapor deposition (LPCVD).

### Claim 17 (depends on 15)

The method of claim 15, wherein the first TaSiN layer and the second TaSiN layer are formed of using Ta(N(CH3)2)5 or Ta(N(C2H5)2)5 as a source material.

### Claim 18 (depends on 15)

The method of claim 15, wherein the first and second TaON layers are formed to have a total thickness of about 100 Å to 120 Å using Ta(OC2H5)5 as a source material, and NH3 as a reaction gas, by metal organic chemical vapor deposition (MOCVD).

### Claim 19 (depends on 18)

The method of claim 18, wherein each of the first and second TaON layers has a thickness of about 50 Å to 60 Å.

### Claim 20 (depends on 9)

The method of claim 9, wherein the rapid annealing process is performed at a temperature between about 600° C. and 700° C. in a N2 atmosphere.