# US 2001/0036703 A1 · Method of manufacturing capacitor of semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0036703 A1
- Document ID: US20010036703A1
- Status: Published application
- Kind: A1
- Application number: 09/745,426
- Filed: 2000-12-26
- Published: 2001-11-01
- Earliest claimed: 1999-12-23
- Assignees: Hynix Semiconductor Inc.
- Inventors: Kee Jeung Lee; Hong Seon Yang
- Web page: https://patentgrep.com/patent/US20010036703A1

## CPC

- H10D 1/68: Capacitors having no potential barriers
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/6544: {to change the morphology of the insulating materials, e.g. transformation of an amorphous layer into a crystalline layer}
- H10B 12/033: {the capacitor extending over the transistor}
- H10D 1/692: {Electrodes}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/69393: {the material containing tantalum, e.g. Ta2O5}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

The present invention discloses a method of manufacturing a TaON capacitor having a high capacity comprising the steps of forming an intermediate insulating layer on a semiconductor substrate; forming a lower electrode on the intermediate insulating layer; depositing a TaON thin film in an amorphous state on the lower electrode; annealing the amorphous TaON thin film in a vacuum state to form a crystalline TaON thin film that will serve as a dielectric layer; and forming an upper electrode on the dielectric layer made of the TaON thin film.

## Claims

### Claim 1

A method of manufacturing a capacitor for a semiconductor device, comprising the steps of:
providing a semiconductor substrate on which selected lower patterns have been formed;
forming an intermediate insulating layer on the semiconductor substrate;
forming a lower electrode on the intermediate insulating layer;
depositing an amorphous TaON thin film on the lower electrode;
annealing the amorphous TaON thin film under reduced pressure to form a dielectric layer comprising crystalline TaON; and
forming an upper electrode on the dielectric layer.

### Claim 2

The method according to claim l, wherein the lower electrode comprises doped polysilicon.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the lower electrode consists essentially of one material selected from a group consisting of TiN, TaN, W, WSi, Ru, RuO2, Ir, IrO2, and Pt.

### Claim 4 (depends on 2)

The method according to claim 2, further comprising the step of cleaning the lower electrode after the step of forming the lower electrode and before the step of depositing the TaON film.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the cleaning step is performed by a dry method using HF vapor or a wet method using HF solution.

### Claim 6 (depends on 2)

The method according to claim 2, further comprising the step of nitrifying the surface of the lower electrode after the step of forming the lower electrode.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the nitrifying step is performed using an in-situ plasma under NH3 gas atmosphere for 1 to 5 minutes.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the step of depositing the amorphous TaON thin film further comprises reacting a predetermined amount of a Ta compound vapor and a reaction gas, the reaction gas comprising NH3 or O2, in a LPCVD chamber at a temperature of between 300 and 600° and at a pressure of less than 100 Torr.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the Ta compound vapor is obtained by supplying a selected amount of a Ta(OC2H5)5 solution into an evaporator, the evaporator being maintained at a temperature of between 150 and 200° C., evaporating the Ta(OC2H5)5 solution to form the Ta compound vapor, and injecting the Ta compound vapor into the LPCVD chamber.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the amorphous TaON thin film is annealed under a reduced pressure of less than 100 Torr in a N2 or NH3 atmosphere and at a temperature between 600 and 950° C.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising an additional annealing step, the additional annealing step being completed after the step of annealing the amorphous TaON thin film under reduced pressure and before the step of forming the upper electrode.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the additional annealing step is performed under an O2 or N2O atmosphere or under an UV—O3 or O3 atmosphere at a temperature of between 600 and 950° C.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the upper electrode comprises doped polysilicon.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the upper electrode consists essentially of one material is made of one selected from a group consisting of TiN, TaN, W, WSi, Ru, RuO2, Ir, IrO2 and Pt.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the upper electrode comprises a multi-layer structure, the multi-layer structure comprising a buffer layer formed on a metal layer.

### Claim 16 (depends on 15)

The method according to claim 15, wherein the metal layer consists essentially of one material selected from a group consisting of TiN, TaN, W, WSi, Ru, RuO2, Ir, IrO and Pt, and further wherein the buffer layer comprises doped polysilicon.