# US 2001/0033637 A1 · X-ray target

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0033637 A1
- Document ID: US20010033637A1
- Status: Published application
- Kind: A1
- Application number: 09/892,434
- Filed: 2001-06-28
- Published: 2001-10-25
- Earliest claimed: 1999-11-22
- Assignees: Generel Electric Company
- Inventors: Wayne Charles Hasz; Mark Gilbert Benz; Charles Gitahi Mukira; Thomas Robert Raber; Gregory Alan Steinlage; Gregory Reznikov
- Web page: https://patentgrep.com/patent/US20010033637A1

## CPC

- H01J 35/108: {Substrates for and bonding of emissive target, e.g. composite structures}
- H01J 2235/086: Target geometry
- Y10T 428/12063: Nonparticulate metal component
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

An improved X-ray tube target comprises a refractory metal target substrate and a refractory metal focal track applied to the target substrate by a tape casting process. The X-ray tube target comprises a refractory metal target substrate and a refractory metal focal track formed on the target substrate to form a focal track/target substrate interface plane that varies less than about ±0.13 mm.

## Claims

### Claim 1

An X-ray tube anode comprising:
a refractory metal target substrate; and
a refractory metal focal track formed on said target substrate with a focal track/target substrate interface that varies less than about ±0.13 mm from a perfect plane interface between said target substrate and said track.

### Claim 2 (depends on 1)

The X-ray tube anode of claim 1, wherein said focal track/target substrate interface varies less than about ±0.10 mm from said perfect plane interface between said target substrate and said track.

### Claim 3 (depends on 1)

The X-ray tube anode of claim 1, wherein said focal track/target substrate interface varies less than about ±0.05 mm from said perfect plane interface between said target substrate and said track.

### Claim 4 (depends on 1)

The X-ray tube anode of claim 1, wherein said focal track has a surface that varies less than about ±0.13 mm.

### Claim 5 (depends on 1)

The X-ray tube anode of claim 1, wherein said focal track has a surface that varies less than about ±0.10 mm.

### Claim 6 (depends on 1)

The X-ray tube anode of claim 1, wherein said focal track surface varies less than about ±0.05 mm.

### Claim 7 (depends on 1)

The X-ray tube anode of claim 1, wherein said refractory metal target substrate comprises a titanium-zirconium-molybdenum alloy or a titanium-zirconium-molybdenum with carbon alloy.

### Claim 8 (depends on 1)

The X-ray tube anode of claim 1, wherein said focal track is formed by tape casting, slip casting, roll compaction, slurry spraying, thermal spraying or waterfall processing.

### Claim 9 (depends on 1)

An X-ray tube having a rotating anode assembly comprising the X-ray tube anode of claim 1.

### Claim 10

A process of making an X-ray tube anode, comprising:
depositing a refractory metal onto a surface to form a tape, and
forming an X-ray anode from said tape applied to a refractory metal substrate.

### Claim 11 (depends on 10)

The process of claim 10, comprising forming said deposited refractory focal track by:
(i) forming a slurry of a solvent and binder with an X-ray target-forming metal, (ii) casting a uniform film of said slurry onto a surface, and (iii) evaporating solvent from said slurry to form said tape; and
removing said tape from said surface to apply to said refractory metal target substrate-forming material.

### Claim 12 (depends on 10)

The process of claim 10, further comprising forming a pack from said focal track metal applied to said refractory metal target substrate-forming material and sintering said pack to produce said X-ray anode.

### Claim 13

A process of forming an X-ray anode, comprising:
casting a slurry of a powder in a solvent containing a binder onto a casting surface;
evaporating said solvent from the slurry to produce a tape of a shaped layer removably adhering to said casting surface;
densifying the tape to increase its green strength;
peeling the casting surface from said tape;
forming a pack from said tape and an X-ray target substrate-forming material; and
sintering said pack to produce said X-ray anode.

### Claim 14 (depends on 13)

The process of claim 13, comprising evaporating said solvent under a controlled humidity of between about 85% to about 95% at room temperature.

### Claim 15 (depends on 13)

The process of claim 13, wherein said slurry comprises between about 50 and about 98 weight percent metal powder and between about 5 and about 20 weight percent binder.

### Claim 16 (depends on 13)

The process of claim 13, wherein said slurry comprises between about 84 and about 96 weight percent metal powder and between about 7 and about 16 weight percent binder.

### Claim 17 (depends on 13)

The process of claim 13, wherein said slurry comprises between about 87 and about 94 weight percent metal powder and between about 8 and about 13 weight percent binder.

### Claim 18 (depends on 13)

The process of claim 13, comprising forming said pack by placing a multiplicity of shaped layers within a die with said X-ray target substrate-forming material and pressing said multiplicity of layers and X-ray target substrate-forming material.

### Claim 19 (depends on 13)

The process of claim 13, comprising forming said pack by placing a single shaped layer having a thickness greater than about 1.40 mm within a die with said X-ray target substrate-forming material; pressing said multiplicity of layers and said X-ray target substrate-forming material; sintering said pack; and machining said layer to 1.40 mm or less.

### Claim 20 (depends on 13)

The process of claim 13, comprising forming said pack by applying a compression force of between about 32 tons/cm2 and about 226 tons/cm2.

### Claim 21 (depends on 13)

The process of claim 13, comprising forming said pack by applying a compression force of between about 65 tons/cm2 and about 194 tons/cm2.

### Claim 22 (depends on 13)

The process of claim 13, comprising forming said pack by applying a compression force of between about 97 tons/cm2 and about 162 tons/cm2.

### Claim 23 (depends on 13)

The process of claim 13, comprising sintering at a temperature of between about 2000° C. to about 2200° C. for a period of between about 5 hours and about 10 hours in vacuum.

### Claim 24 (depends on 13)

The process of claim 13, comprising forming an X-ray anode from said deposited focal track metal that is less than about 1.40 mm thick without machining.

### Claim 25 (depends on 10)

The product of the process of claim 10, wherein said focal track is less than about 1.40 mm thick without machining.

### Claim 26 (depends on 13)

The product of the process of claim 13, wherein said focal track is less than about 1.40 mm thick without machining.