# US 2001/0032580 A1 · Barium doping of molten silicon for use in crystal growing process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0032580 A1
- Document ID: US20010032580A1
- Status: Published application
- Kind: A1
- Application number: 09/859,826
- Filed: 2001-05-17
- Published: 2001-10-25
- Earliest claimed: 1999-03-15
- Assignees: MEMC Electronic Materials, Inc.
- Inventors: Richard J. Phillips; Steven J. Keltner; John D. Holder
- Web page: https://patentgrep.com/patent/US20010032580A1

## CPC

- C30B 29/06: Silicon
- C30B 15/10: Crucibles or containers for supporting the melt
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A process for preparing doped molten silicon for use in a single silicon crystal growing process is disclosed. Polysilicon is doped with barium and melted in a silica crucible containing less than about 0.5% gases insoluble in silicon. During melting and throughout the crystal growing process the barium acts as a devitrification promoter and creates a layer of devitrified silica on the inside crucible surface in contact with the melt resulting in a lower level of contaminants in the melt and grown crystal.

## Claims

### Claim 1

A process for preparing a silicon melt in a silica crucible for growing a single silicon ingot, the process comprising:
charging polysilicon to a crucible having a bottom wall and a sidewall formation, the bottom and sidewall formation having inside and outside surfaces, and the crucible containing less than about 0.5% gases insoluble in silicon;
melting the polysilicon to form a mass of molten silicon in the crucible;
doping the molten mass with barium; and
forming a layer of devitrified silica on the inside surface of the crucible in contact with the molten mass, the layer being nucleated by the barium in the molten mass.

### Claim 2 (depends on 1)

The process as set forth in claim 1 wherein the barium dopant is selected from the group consisting of barium oxide, barium silicate, barium acetate, barium silicide, barium hydride, barium chloride, and barium oxalate.

### Claim 3 (depends on 1)

The process as set forth in claim 1 wherein the barium dopant is selected from the group consisting of barium hydroxide, barium carbonate and barium silicon oxide.

### Claim 4 (depends on 1)

The process as set forth in claim 1 wherein the dopant is in the form of an alloy of polysilicon and barium.

### Claim 5 (depends on 1)

The process as set forth in claim 1 wherein a concentration of at least about 1.5×10−8 grams of barium/volume of silicon charge (cm3)/wetted area of silica (cm2) of barium is added.

### Claim 6 (depends on 1)

The process as set forth in claim 1 wherein a concentration of at least about 6×10−7 grams of barium/volume of silicon charge (cm3)/wetted area of silica (cm2) of barium is added.

### Claim 7 (depends on 1)

The process as set forth in claim 1 further comprising coating the outside surface of the sidewall formation of the crucible with a devitrification promoter prior to the charging of the polysilicon.

### Claim 8 (depends on 1)

The process as set forth in claim 1 wherein the inside surface of the sidewall formation and the inside surface of the bottom of the crucible contains a tungsten doped layer prior to the introduction of the polysilicon and dopant.

### Claim 9 (depends on 8)

The process as set forth in claim 8 further comprising tungsten doping the outside surface of the sidewall formation and the outside surface of the bottom of the crucible prior to the introduction of the polysilicon and dopant.

### Claim 10 (depends on 1)

The process as set forth in claim 1 wherein the outside surface of the sidewall formation and the outside surface of the bottom of the crucible contain a tungsten doped layer prior to the introduction of the polysilicon and dopant.

### Claim 11

A process for preparing a silicon melt in a silica crucible for growing a single silicon ingot, the process comprising:
charging polysilicon and barium to a crucible having a bottom wall and a sidewall formation, the bottom and sidewall formation having inside and outside surfaces, and the crucible containing less than about 0.5% gases insoluble in silicon;
melting the polysilicon to form a mass of molten silicon in the crucible; and
forming a layer of devitrified silica on the inside surface of the crucible which is in contact with the molten mass, the layer being nucleated by the barium in the molten mass.

### Claim 12 (depends on 11)

The process as set forth in claim 11 wherein the barium dopant is selected from the group consisting of barium oxide, barium silicate, barium acetate, barium silicide, barium hydride, barium chloride, and barium oxalate.

### Claim 13 (depends on 11)

The process as set forth in claim 11 wherein the barium dopant is selected from the group consisting of barium hydroxide, barium carbonate and barium silicon oxide.

### Claim 14 (depends on 11)

The process as set forth in claim 11 wherein a concentration of at least about 1.5×10−8 grams of barium/volume of silicon charge (cm3)/wetted area of silica (cm2) of barium is added.

### Claim 15 (depends on 11)

The process as set forth in claim 11 wherein a concentration of at least about 6×10−7 grams of barium/volume of silicon charge (cm3)/wetted area of silica (cm2) of barium is added.

### Claim 16

A process for preparing a silicon melt in a silica crucible for growing a single silicon ingot, the process comprising:
charging polysilicon to a crucible having bottom wall and a sidewall formation, the bottom and sidewall formation having inside and outside surfaces, and the crucible having a tungsten doped layer on the inside bottom and sidewall formation;
melting the polysilicon to form a mass of molten silicon in the crucible;
doping the molten mass with barium; and
forming a layer of devitrified silica on the inside surface of the crucible in contact with molten mass, the layer being nucleated by the barium in the molten mass.

### Claim 17 (depends on 16)

The process as set forth in claim 16 wherein the crucible also has a tungsten doped layer on the sidewall formation of the outside surface.

### Claim 18 (depends on 16)

The process as set forth in claim 16 further comprising coating the outside surface of the sidewall formation of the crucible with a devitrification promoter prior to the charging of the polysilicon.

### Claim 19 (depends on 16)

The process as set forth in claim 16 wherein the barium is added as an alloy of polysilicon and barium.