# US 2001/0027244 A1 · Polyethylene glycol modified polyester fibers, yarns, and fabrics and method for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027244 A1
- Document ID: US20010027244A1
- Status: Published application
- Kind: A1
- Application number: 09/858,388
- Filed: 2001-05-16
- Published: 2001-10-04
- Earliest claimed: 1999-11-19
- Assignees: Wellman, Inc.
- Inventors: James Burch Branum
- Web page: https://patentgrep.com/patent/US20010027244A1

## CPC

- D02G 3/04: Blended or other yarns or threads containing components made from different materials
- C08G 63/668: derived from polycarboxylic acids and polyhydroxy compounds
- C08G 63/672: Dicarboxylic acids and dihydroxy compounds
- C08G 63/80: Solid-state polycondensation
- D01F 6/86: from polyetheresters
- D03D 1/0041: {Cut or abrasion resistant}
- D03D 15/283: synthetic polymer-based, e.g. polyamide or polyester fibres (cellulose-based artificial fibres D03D15/225)
- D03D 15/49: textured (chenille D03D27/18); curled; crimped
- D03D 15/513: heat-resistant or fireproof
- D10B 2201/02: Cotton
- D10B 2201/24: Viscose
- D10B 2201/28: Cellulose esters or ethers, e.g. cellulose acetate
- D10B 2321/022: polypropylene
- D10B 2331/02: polyamides (D10B2331/08 takes precedence)
- D10B 2331/04: polyesters, e.g. polyethylene terephthalate [PET]
- D10B 2401/046: Shape recovering or form memory
- D10B 2401/14: Dyeability
- D10B 2501/00: Wearing apparel
- Y10T 428/29: Coated or structually defined flake, particle, cell, strand, strand portion, rod, filament, macroscopic fiber or mass thereof
- Y10T 428/2904: Staple length fiber
- Y10T 428/2913: Rod, strand, filament or fiber
- Y10T 428/2915: including textile, cloth or fabric
- Y10T 428/2924: Composite
- Y10T 428/2929: Bicomponent, conjugate, composite or collateral fibers or filaments [i.e., coextruded sheath-core or side-by-side type]
- Y10T 442/60: Nonwoven fabric [i.e., nonwoven strand or fiber material]
- Y10T 442/635: Synthetic polymeric strand or fiber material
- Y10T 442/636: Synthetic polymeric strand or fiber material is of staple length
- D02G: CRIMPING OR CURLING FIBRES, FILAMENTS, THREADS, OR YARNS; YARNS OR THREADS
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS
- D03D: WOVEN FABRICS; METHODS OF WEAVING; LOOMS
- D10B: INDEXING SCHEME ASSOCIATED WITH SUBLASSES OF SECTION D, RELATING TO TEXTILES
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

Disclosed is a method of copolymerizing polyethylene glycol (PEG) and branching agent into polyethylene terephthalate (PET) to achieve a polyethylene glycol-modified polyester composition that can be spun into filaments. Fabrics made from fibers formed from the copolyester composition possess wicking, drying, stretching, abrasion-resistance, flame-retardancy, static-dissipation, dyeability, and tactility properties that are superior to those of fabrics formed from conventional polyethylene terephthalate fibers of the same yarn and fabric construction. Also disclosed are polyethylene glycol modified copolyester compositions, fibers, yarns, and fabrics.

## Claims

### Claim 1

A method of preparing polyethylene glycol modified copolyester fibers that can be formed into exceptionally comfortable fabrics, comprising:
copolymerizing polyethylene glycol and a chain branching agent into polyethylene terephthalate in the melt phase to form a copolyester composition that has an intrinsic viscosity of at least about 0.67 dl/g and that comprises polymer chains formed from structural units consisting essentially of diol monomers, non-substituted diacid monomers, and branching agent monomers;
wherein the polyethylene terephthalate is present in the copolyester composition in an amount sufficient for a fiber made from the copolyester composition to possess dimensional stability properties substantially similar to those of conventional, unmodified polyethylene terephthalate fibers;
wherein the polyethylene glycol has an average molecular weight of less than about 5000 g/mol and is present in an amount sufficient for a fiber made from the copolyester composition to possess wicking, drying, and static-dissipation properties that are superior to those of conventional, unmodified polyethylene terephthalate fibers; and
wherein the chain branching agent is present in the copolyester composition in an amount between about 0.0003 and 0.0014 mole-equivalent branches per mole of standardized polymer, the standardized polymer being unmodified polyethylene terephthalate; and
thereafter spinning POY from the copolyester composition.

### Claim 2 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the copolyester composition has an intrinsic viscosity of at least about 0.73 dl/g.

### Claim 3 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the copolyester composition has an intrinsic viscosity of at least about 0.80 dl/g.

### Claim 4 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the step of copolymerizing polyethylene glycol and a chain branching agent into polyethylene terephthalate yields a copolyester composition that comprises polymer chains formed from structural units consisting essentially of diol monomers, aromatic non-substituted diacid monomers, and branching agent monomers.

### Claim 5 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the polyethylene glycol has an average molecular weight of between about 300 g/mol and 1000 g/mol.

### Claim 6 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the weight fraction of polyethylene glycol in the copolyester composition is between about 4 percent and 20 percent.

### Claim 7 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the weight fraction of polyethylene glycol in the copolyester composition is between 10 percent and 20 percent.

### Claim 8 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the weight fraction of polyethylene glycol in the copolyester composition and the intrinsic viscosity of the copolyester after melt phase polymerization are defined by the shaded region of FIG. 1.

### Claim 9 (depends on 1)

A method of preparing copolyester fibers according to claim 1, wherein the POY has a mean tenacity of less than 3 grams per denier.

### Claim 10 (depends on 1)

A method for producing copolyester fibers according to claim 1, further comprising drawing the POY to form drawn yarn.

### Claim 11 (depends on 10)

A method for producing copolyester fibers according to claim 10, wherein the step of drawing the POY comprises draw-texturing the POY to form textured yarn.

### Claim 12 (depends on 10)

A method for producing copolyester fibers according to claim 10, further comprising:
forming the drawn yarn into a fabric; and
finishing the fabric.

### Claim 13 (depends on 10)

A method for producing copolyester fibers according to claim 10, further comprising forming the drawn yarn and a second kind of fiber into a blended yarn.

### Claim 14 (depends on 13)

A method for producing copolyester fibers according to claim 13, wherein the second kind of fiber is selected from the group consisting of cotton fibers, rayon fibers, polypropylene fibers, acetate fibers, nylon fibers, spandex fibers, conventional polyester fibers, and copolyester staple fibers.

### Claim 15 (depends on 10)

A method for producing copolyester fibers according to claim 10, further comprising forming the drawn yarn and a second kind of fiber into a fabric.

### Claim 16 (depends on 15)

A method for producing copolyester fibers according to claim 15, wherein the second kind of fiber is selected from the group consisting of cotton fibers, rayon fibers, polypropylene fibers, acetate fibers, nylon fibers, spandex fibers, conventional polyester fibers, and copolyester staple fibers.

### Claim 17 (depends on 1)

A method for producing copolyester fibers according to claim 1, further comprising:
forming the POY and a nylon yarn into a blended yarn;
texturing the blended yarn; and
dyeing the blended yarn with a disperse dye, which selectively dyes the copolyester component, and an acid-based dye, which selectively dyes the nylon component.

### Claim 18

A method of preparing polyethylene glycol modified copolyester fibers that can be formed into exceptionally comfortable fabrics, comprising:
copolymerizing polyethylene glycol and a chain branching agent into polyethylene terephthalate in the melt phase to form a copolyester composition that has an intrinsic viscosity of at least about 0.67 dl/g and that comprises polymer chains formed from structural units consisting essentially of diol monomers, non-substituted diacid monomers, and branching agent monomers;
wherein the polyethylene terephthalate is present in the copolyester composition in an amount sufficient for a fiber made from the copolyester composition to possess dimensional stability properties substantially similar to those of conventional, unmodified polyethylene terephthalate fibers;
wherein the polyethylene glycol has an average molecular weight of less than about 5000 g/mol and is present in an amount sufficient for a fiber made from the copolyester composition to possess wicking, drying, and static-dissipation properties that are superior to those of conventional, unmodified polyethylene terephthalate fibers; and
wherein the chain branching agent is present in the copolyester composition in an amount between about 0.0003 and 0.0014 mole-equivalent branches per mole of standardized polymer, the standardized polymer being unmodified polyethylene terephthalate; and
thereafter spinning the copolyester composition into a filament and cutting the filament into staple fibers.

### Claim 19 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the copolyester composition has an intrinsic viscosity of at least about 0.73 dl/g.

### Claim 20 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the copolyester composition has an intrinsic viscosity of at least about 0.80 dl/g.

### Claim 21 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the step of copolymerizing polyethylene glycol and a chain branching agent into polyethylene terephthalate yields a copolyester composition that comprises polymer chains formed from structural units consisting essentially of diol monomers, aromatic non-substituted diacid monomers, and branching agent monomers.

### Claim 22 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the polyethylene glycol has an average molecular weight of between about 300 g/mol and 1000 g/mol.

### Claim 23 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the weight fraction of polyethylene glycol in the copolyester composition is between about 4 percent and 20 percent.

### Claim 24 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the weight fraction of polyethylene glycol in the copolyester composition is between 10 percent and 20 percent.

### Claim 25 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the weight fraction of polyethylene glycol in the copolyester composition and the intrinsic viscosity of the copolyester composition after melt phase polymerization are defined by the shaded region of FIG. 1.

### Claim 26 (depends on 18)

A method of preparing copolyester fibers according to claim 18, wherein the staple fibers have a mean tenacity of less than 3 grams per denier.

### Claim 27 (depends on 18)

A method for producing copolyester fibers according to claim 18, further comprising forming the staple fibers into yarn.

### Claim 28 (depends on 18)

A method for producing copolyester fibers according to claim 18, further comprising forming the staple fibers into fabric.

### Claim 29 (depends on 18)

A method for producing copolyester fibers according to claim 18, further comprising forming the copolyester staple fibers and a second kind of fiber into a blended yarn.

### Claim 30 (depends on 29)

A method for producing copolyester fibers according to claim 29, wherein the second kind of fiber is selected from the group consisting of cotton fibers, rayon fibers, polypropylene fibers, acetate fibers, nylon fibers, spandex fibers, and conventional polyester fibers.

### Claim 31 (depends on 18)

A method for producing copolyester fibers according to claim 18, further comprising forming the copolyester staple fibers and a second kind of fiber into a fabric.

### Claim 32 (depends on 31)

A method for producing copolyester fibers according to claim 31, wherein the second kind of fiber is selected from the group consisting of cotton fibers, rayon fibers, polypropylene fibers, acetate fibers, nylon fibers, spandex fibers, and conventional polyester fibers.

### Claim 33

A method of preparing polyethylene glycol modified copolyester fibers that can be formed into exceptionally comfortable fabrics, comprising:
copolymerizing polyethylene glycol and a chain branching agent into polyethylene terephthalate in the melt phase to form a copolyester composition that has an intrinsic viscosity of at least about 0.67 dl/g;
wherein the polyethylene terephthalate is present in the copolyester composition in an amount sufficient for a fiber made from the copolyester composition to possess dimensional stability properties substantially similar to those of conventional, unmodified polyethylene terephthalate fibers;
wherein the polyethylene glycol has an average molecular weight of less than about 5000 g/mol and is present in an amount sufficient for a fiber made from the copolyester composition to possess wicking, drying, and static-dissipation properties that are superior to those of conventional, unmodified polyethylene terephthalate fibers; and
wherein the chain branching agent is present in the copolyester composition in an amount between about 0.0003 and 0.0014 mole-equivalent branches per mole of standardized polymer, the standardized polymer being unmodified polyethylene terephthalate;
thereafter forming copolyester fibers from the copolyester composition;
blending the copolyester fibers with spandex fibers; and
dyeing the blended copolyester fibers and the spandex fibers at a temperature of less than about 240° F.

### Claim 34 (depends on 33)

A method of preparing copolyester fibers according to claim 33, wherein the step of copolymerizing polyethylene glycol and a chain branching agent into polyethylene terephthalate yields a copolyester composition that comprises polymer chains formed from structural units consisting essentially of diol monomers, non-substituted diacid monomers, and branching agent monomers.

### Claim 35 (depends on 34)

A method of preparing copolyester fibers according to claim 34, wherein the step of copolymerizing polyethylene glycol and a chain branching agent into polyethylene terephthalate yields a copolyester composition that comprises polymer chains formed from structural units consisting essentially of diol monomers, aromatic non-substituted diacid monomers, and branching agent monomers.

### Claim 36 (depends on 34)

A method of preparing copolyester fibers according to claim 34, wherein the weight fraction of polyethylene glycol in the copolyester composition is between about 4 percent and 20 percent.

### Claim 37 (depends on 34)

A method for producing copolyester fibers according to claim 34, wherein the step of dyeing the blended copolyester fibers and spandex fibers at a temperature of less than about 240° F. comprises dyeing the blended copolyester fibers and spandex fibers at a temperature of less than about 220° F.

### Claim 38 (depends on 37)

A method for producing copolyester fibers according to claim 37, wherein the step of dyeing the blended copolyester fibers and spandex fibers at a temperature of less than about 220° F. comprises dyeing the blended copolyester fibers and spandex fibers at or below a temperature defined by the boiling point of water at atmospheric pressure.

### Claim 39 (depends on 34)

A method for producing copolyester fibers according to claim 34, further comprising forming the copolyester fibers and the spandex fibers into yarn.

### Claim 40 (depends on 39)

A method for producing copolyester fibers according to claim 39, wherein the step of forming the copolyester fibers and the spandex fibers into yarn comprises core spinning copolyester staple fibers around a core of spandex filaments.

### Claim 41 (depends on 39)

A method for producing copolyester fibers according to claim 39, wherein the step of forming the copolyester fibers and the spandex fibers into yarn comprises wrapping copolyester filaments around spandex filaments.

### Claim 42 (depends on 34)

A method for producing copolyester fibers according to claim 34, further comprising forming the copolyester fibers and the spandex fibers into fabric.

### Claim 43 (depends on 42)

A method for producing copolyester fibers according to claim 42, wherein the step of forming the copolyester fibers and the spandex fibers into fabric comprises laying the spandex fibers into a knit fabric.

### Claim 44

A blended yarn, comprising:
a first set of fibers; and
polyethylene glycol modified copolyester fibers;
said copolyester fibers comprising:
polyethylene terephthalate in an amount sufficient for said copolyester fibers to possess dimensional stability properties substantially similar to those of conventional, unmodified polyethylene terephthalate fibers;
polyethylene glycol in an amount sufficient for said copolyester fibers to possess wicking, drying, and static-dissipation properties that are superior to those of conventional, unmodified polyethylene terephthalate fibers, wherein the polyethylene glycol has an average molecular weight of less than about 5000 g/mol; and
chain branching agent in an amount less than about 0.0014 mole-equivalent branches per mole of standardized polymer, the standardized polymer being unmodified polyethylene terephthalate; and
wherein the weight fraction of the polyethylene glycol in said copolyester fibers and the intrinsic viscosity of said copolyester fibers are defined by the shaded region of FIG. 1; and
wherein said copolyester fibers comprise polymer chains formed from structural units consisting essentially of diol monomers, non-substituted diacid monomers, and branching agent monomers.

### Claim 45 (depends on 44)

A blended yarn according to claim 44, wherein said first set of fibers is selected from the group consisting of cotton fibers, rayon fibers, polypropylene fibers, acetate fibers, nylon fibers, spandex fibers, and conventional polyester fibers.

### Claim 46 (depends on 44)

A blended yarn according to claim 44, wherein the polyethylene glycol has an average molecular weight of between about 300 g/mol and 1000 g/mol.

### Claim 47 (depends on 44)

A blended yarn according to claim 44, wherein said copolyester fibers have an intrinsic viscosity of at least about 0.73 dl/g.

### Claim 48 (depends on 44)

A blended yarn according to claim 44, wherein said copolyester fibers comprise polymer chains formed from structural units consisting essentially of diol monomers, non-substituted aromatic diacid monomers, and branching agent monomers.

### Claim 49 (depends on 44)

A blended yarn according to claim 44, wherein said copolyester fibers have a mean tenacity of less than 3 grams per denier.

### Claim 50 (depends on 44)

A blended yarn according to claim 44, wherein said copolyester fibers are staple fibers.

### Claim 51 (depends on 44)

A blended yarn according to claim 44, wherein said copolyester fibers are in the form of a partially oriented yarn.

### Claim 52 (depends on 44)

A blended yarn according to claim 44, wherein said copolyester fibers are in the form of a drawn yarn.

### Claim 53 (depends on 44)

A blended yarn according to claim 44, wherein the first set of fibers are in the form of a nylon yarn.

### Claim 54 (depends on 44)

A blended yarn according to claim 44, wherein the first set of fibers are cotton cellulosic fibers.

### Claim 55 (depends on 44)

A blended yarn according to claim 44, wherein the first set of fibers are spandex fibers.

### Claim 56 (depends on 55)

A blended yarn according to claim 55, wherein
said spandex fibers form a core of spandex filaments; and
said copolyester fibers are staple fibers that surround said spandex filament core.

### Claim 57 (depends on 55)

A blended yarn according to claim 55, wherein
said spandex fibers are spandex filaments; and
said copolyester fibers are copolyester filaments that are wrapped around said spandex filaments.

### Claim 58

A blended fabric, comprising:
a first set of fibers; and
polyethylene glycol modified copolyester fibers;
said copolyester fibers comprising:
polyethylene terephthalate in an amount sufficient for said copolyester fibers to possess dimensional stability properties substantially similar to those of conventional, unmodified polyethylene terephthalate fibers;
polyethylene glycol in an amount sufficient for said copolyester fibers to possess wicking, drying, and static-dissipation properties that are superior to those of conventional, unmodified polyethylene terephthalate fibers, wherein the polyethylene glycol has an average molecular weight of less than about 5000 g/mol; and
chain branching agent in an amount less than about 0.0014 mole-equivalent branches per mole of standardized polymer, the standardized polymer being unmodified polyethylene terephthalate; and
wherein the weight fraction of polyethylene glycol in said copolyester fibers and the intrinsic viscosity of said copolyester fibers are defined by the shaded region of FIG. 1; and
wherein said copolyester fibers comprise polymer chains formed from structural units consisting essentially of diol monomers, non-substituted diacid monomers, and branching agent monomers.

### Claim 59 (depends on 58)

A blended fabric according to claim 58, wherein said first set of fibers selected from the group consisting of cotton fibers, rayon fibers, polypropylene fibers, acetate fibers, nylon fibers, spandex fibers, and conventional polyester fibers.

### Claim 60 (depends on 58)

A blended fabric according to claim 58, wherein the polyethylene glycol has an average molecular weight of between about 300 g/mol and 1000 g/mol.

### Claim 61 (depends on 58)

A blended fabric according to claim 58, wherein said copolyester fibers have an intrinsic viscosity of at least about 0.73 dl/g.

### Claim 62 (depends on 58)

A blended fabric according to claim 58, wherein said copolyester fibers comprise polymer chains formed from structural units consisting essentially of diol monomers, non-substituted aromatic diacid monomers, and branching agent monomers.

### Claim 63 (depends on 58)

A blended fabric according to claim 58, wherein said copolyester fibers have a mean tenacity of less than 3 grams per denier.

### Claim 64 (depends on 58)

A blended fabric according to claim 58, wherein said first set of fibers are cotton cellulosic fibers.

### Claim 65 (depends on 58)

A blended fabric according to claim 58, wherein said copolyester fibers are staple fibers.

### Claim 66 (depends on 65)

A blended fabric according to claim 65, wherein
said fabric is a knit fabric formed from said staple fibers;
said first set of fibers are spandex fibers, and
said spandex fibers are laid into said knit fabric.

### Claim 67 (depends on 58)

A blended fabric according to claim 58, wherein said copolyester fibers are in the form of a drawn yarn.
