# US 2001/0027234 A1 · Radiation-curable binders of low additive content

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027234 A1
- Document ID: US20010027234A1
- Status: Published application
- Kind: A1
- Application number: 09/824,762
- Filed: 2001-04-04
- Published: 2001-10-04
- Earliest claimed: 2000-04-04
- Assignees: BASF SE
- Inventors: Horst Binder; Petra Neumann
- Web page: https://patentgrep.com/patent/US20010027234A1

## CPC

- C08F 8/00: Chemical modification by after-treatment (graft polymers, block polymers, crosslinking with unsaturated monomers or with polymers C08F251/00 - C08F299/00; of conjugated diene rubbers C08C)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The invention relates to transparent, undiscolored and uncrosslinked, radiation-curable binders of low additive content, obtainable by polymer-analogous reaction of epoxy-functional (meth)acrylate copolymers (A) with an unsaturated monocarboxylic acid (B), the reaction a) of the copolymer (A) taking place with at least 2 equivalents of the carboxylic acid (B), b) in the absence of reaction accelerators and inhibitors, c) in a continuously operated reactor, d) without solvent, e) at from 130 to 170° C., f) with a degree of conversion of at least 90% within an average residence time which is as short as possible but sufficient, and which is below 13 to 22 minutes. The reaction products contain virtually no byproducts and are advantageous binders for clearcoat materials and powder coating materials.

## Claims

### Claim 1

An uncrosslinked, radiation-curable binder of low additive content, obtained by polymer-analogous reaction of
A) an epoxy-functional (meth)acrylate copolymer A with
B) at least one olefinically unsaturated aliphatic C3-C6 monocarboxylic acid, the polymer-analogous reaction of the copolymer A taking place
a) with at least 2 equivalents of the carboxylic acid B, based on the epoxide groups of the copolymer A,
b) in the absence of any significant amount of a reaction accelerator for the epoxide-carboxylic acid reaction and in the absence of any significant amount of a polymerization inhibitor,
c) in a continuously operated reactor,
d) with essentially no solvent,
e) at a reaction temperature of from 130 to 170° C., and
f) with a degree of conversion of the epoxide groups of the copolymer A of at least 90%,
g) the average residence time established being sufficient for achieving the chosen degree of conversion f), and not exceeding a maximum average residence time which shortens with the increasing reaction temperature e) and amounts to 32 minutes at 130° C., 25 minutes at 140° C., 20 minutes at 150° C., 17 minutes at 160° C., and 13 minutes at 170° C.

### Claim 2 (depends on 1)

A radiation-curable binder of low additive content as claimed in claim 1, wherein the degree of conversion is at least 95%.

### Claim 3 (depends on 1)

A radiation-curable binder as claimed in claim 1, wherein the continuously operated reactor is an extruder.

### Claim 4 (depends on 3)

A radiation-curable binder of low additive content as claimed in claim 3, wherein the reaction temperature in the extruder is from 140 to 160° C., the degree of conversion f) is at least 95% and the average residence time is from about 10 to 15 minutes.

### Claim 5 (depends on 1)

A radiation-curable binder of low additive content as claimed in claim 1, wherein the copolymer A is an alkyl (meth)acrylate copolymer containing, in copolymerized form, from 5 to 60% by weight of a comonomer containing reactive epoxide groups based on the overall weight of the copolymer.

### Claim 6 (depends on 1)

A radiation-curable binder of low additive content as claimed in claim 1, which is transparent and undiscolored.

### Claim 7 (depends on 1)

A process for preparing a radiation-curable binder of low additive content as claimed in claim 1 by polymer-analogous reaction of
A) a copolymer containing reactive epoxide groups with
B) at least one olefinically unsaturated aliphatic C3-C6 monocarboxylic acid, the polymer-analogous reaction of the copolymer A taking place
a) with at least 2 equivalents of the carboxylic acid B, based on the epoxide groups of the copolymer A,
b) in the absence of any significant amount of a reaction accelerator for the epoxide-carboxylic acid reaction and in the absence of any significant amount of a polymerization inhibitor,
c) in a continuously operated reactor,
d) with essentially no solvent,
e) at a reaction temperature of from 130 to 170° C., and
f) with a degree of conversion of the epoxide groups of the copolymer A of at least 90%,
g) the average residence time established being sufficient for achieving the chosen degree of conversion f), and not exceeding a maximum average residence time which shortens with the increasing reaction temperature e) and amounts to 32 minutes at 130° C., 25 minutes at 140° C., 20 minutes at 150° C., 17 minutes at 160° C., and 13 minutes at 170° C.

### Claim 8 (depends on 1)

A clearcoat material, powder coating material, packaging varnish or powder slurry comprising a binder as claimed in claim 1.