# US 2001/0027159 A1 · Method for preparation of sintered body of rare earth oxide

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027159 A1
- Document ID: US20010027159A1
- Status: Published application
- Kind: A1
- Application number: 09/783,602
- Filed: 2001-02-15
- Published: 2001-10-04
- Earliest claimed: 2000-03-07
- Assignees: Shin-Etsu Chemical Co., Ltd.
- Inventors: Masami Kaneyoshi
- Web page: https://patentgrep.com/patent/US20010027159A1

## CPC

- C04B 35/50: based on rare-earth compounds {(non-oxide rare earth compounds C04B35/5156)}
- C04B 35/44: based on aluminates
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

Disclosed is a method for the preparation of a high-quality sintered body of a rare earth oxide or a composite oxide of a rare earth oxide and an adjuvant oxide such as aluminum oxide. The method comprises shaping a rare earth oxide powder characterized by specified particle diameter distribution values of D50 and D90 and a specified specific surface area or a powder blend of the rare earth oxide and adjuvant oxide into a powder compact and subjecting the powder compact to a sintering heat treatment at a specified sintering temperature by increasing and decreasing the temperature up to and from the sintering temperature each at a rate not exceeding a specified upper limit.

## Claims

### Claim 1

A method for the preparation of a sintered body of a rare earth oxide which comprises the steps of:
(a) shaping a powder of the rare earth oxide, of which the D50 value of the particle diameter distribution does not exceed 2.0 μm, the D90 value of the particle diameter distribution does not exceed 3.0 μm and the specific surface area is in the range from 5 to 20 m2/g, into a powder compact; and
(b) subjecting the powder compact to a heat treatment for sintering at a sintering temperature of 1000° C. or higher for at least 1 hour, in which the rate of temperature elevation in the range from 500° C. to the sintering temperature does not exceed 500° C. per hour and the rate of temperature decrease from the sintering temperature does not exceed 600° C. per hour.

### Claim 2 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the D50 value of the particle diameter distribution of the rare earth oxide powder does not exceed 1.5 μm.

### Claim 3 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the D50 value of the particle diameter distribution of the rare earth oxide powder is in the range from 0.9 to 1.3 μm.

### Claim 4 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the D value of the particle diameter distribution of the rare earth oxide powder does not exceed 2.7 μm.

### Claim 5 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the D90 value of the particle diameter distribution of the rare earth oxide powder is in the range from 1.9 to 2.3 μm.

### Claim 6 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the specific surface area of the rare earth oxide powder is in the range from 7 to 18 m2/g.

### Claim 7 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the specific surface area of the rare earth oxide powder is in the range from 10 to 15 m2/g.

### Claim 8 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the D′50 value of the pore diameter distribution of the rare earth oxide powder does not exceed 20 nm.

### Claim 9 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the sintering temperature is in the range from 1200 to 1900° C.

### Claim 10 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the sintering temperature is in the range from 1400 to 1800° C.

### Claim 11 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which shaping of the rare earth oxide powder into a powder compact is conducted by hydrostatic compression.

### Claim 12 (depends on 11)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 11 in which the pressure of hydrostatic compression is at least 100 MPa.

### Claim 13 (depends on 11)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 11 in which the pressure of hydrostatic compression is at least 150 MPa.

### Claim 14 (depends on 1)

The method for the preparation of a sintered body of a rare earth oxide as claimed in claim 1 in which the rate of temperature elevation is in the range from 150 to 400° C. per hour.

### Claim 15

A method for the preparation of a sintered body of a rare earth oxide-based composite oxide with a n adjuvant oxide which comprises the steps of:
(a) blending a powder of the rare earth oxide, of which the D50 value of the particle diameter distribution does not exceed 2.0 μm, the D90 value of the particle diameter distribution does not exceed 3.0 μm and the specific surface area is in the range from 5 to 20 m2/g, and an adjuvant oxide of an element selected from the group consisting of magnesium, aluminum, silicon, titanium, vanadium, chromium, manganese, iron, cobalt, nickel, copper, zinc, gallium, germanium, zirconium, niobium, molybdenum, indium, tin, hafnium, tantalum and tungsten to give a powder blend;
(b) shaping the powder blend into a powder compact; and
(c) subjecting the powder compact to a heat treatment for sintering at a sintering temperature of 1000° C. or higher for at least 1 hour, in which the rate of temperature elevation in the range from 500° C. to the sintering temperature does not exceed 500° C. per hour and the rate of temperature decrease from the sintering temperature does not exceed 600° C. per hour.

### Claim 16 (depends on 15)

The method for the preparation of a sintered body of a rare earth oxide-based composite oxide with an adjuvant oxide as claimed in claim 15 in which the amount of the rare earth oxide powder in the powder blend is at leasr 40% by weight based on the total amount of the powder blend.

### Claim 17 (depends on 15)

The method for the preparation of a sintered body of a rare earth oxide-based composite oxide with an adjuvant oxide as claimed in claim 15 in which the adjuvant oxide is selected from the group consisting of the oxides of iron, aluminum, silicon, titanium, gallium and zirconium.