# US 2001/0027158 A1 · Si3N4 sintered body with high thermal conductivity and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027158 A1
- Document ID: US20010027158A1
- Status: Published application
- Kind: A1
- Application number: 09/819,986
- Filed: 2001-03-29
- Published: 2001-10-04
- Earliest claimed: 1998-03-05
- Assignees: Sumitomo Electric Industries, Ltd.
- Inventors: Ai Itoh; Michimasa Miyanaga
- Web page: https://patentgrep.com/patent/US20010027158A1

## CPC

- C04B 35/591: obtained by reaction sintering
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE

## Abstract

An Si3N4 sintered body produced by reactive sintering of silicon, wherein a compound of at least one element selected from the group consisting of Y, Yb and Sm is contained by 0.6 to 13% by weight as Ln2O3 (wherein Ln=Y, Yb or Sm), an oxygen content in Si3N4 crystal grains is not more than 1% by weight, a ratio of Si and Ln in the Si3N4 sintered body is within a range of 0.1 to 0.8 in a molar ratio of SiO2/Ln2O3 of the Si in terms of SiO2 to the oxide Ln2O3, and the sintered body has a relative density of 85 to 99.9%, a thermal conductivity of at least 70 W/m.K or more and a three-point bending strength of at least 600 MPa. The Si3N4 sintered body is produced by mixing 80 to 99% by weight of silicon powder and 1 to 20% by weight of powder of oxide of at least one element of Y, Yb and SM, by nitriding a molded body of the powder mixture in an atmosphere containing nitrogen at 1400° C. or less, and then sintering the nitrided body in an atmosphere containing nitrogen at a temperature of 1700 to 1950° C. In the production, a coupling agent including C, H, O and metal cations (e.g., Si or Ti) can be used as a reducing coating agent to further improve the thermal conductivity.

## Claims

### Claim 1

A Si3N4 sintered body produced by reactive sintering of silicon, said Si3N4 sintered body comprising crystal grains of Si3N4 and a grain boundary phase, wherein:
an oxide (Ln2O3) of at least one element (Ln) selected from the group consisting of Y, Yb and Sm is contained in an amount of 0.6 to 13% by weight;
an oxygen content in the crystal grains of Si3N4 is not more than 1% by weight;
a ratio of oxygen and Ln in the Si3N4 sintered body is within a range of 0.1 to 0.8 in a molar ratio SiO2/Ln2O3 of the oxygen in terms of SiO2 to the oxide Ln2O3; and
the Si3N4 sintered body has a relative density in the range of 85 to 99.9%, a thermal conductivity of at least 70 W/m.K or more, and a three point bending strength of at least 600 MPa.

### Claim 2 (depends on 1)

The Si3N4 sintered body according to claim 1, wherein said crystal grains of Si3N4 are a β-Si3N4 crystal having an average grain size of 2 μm or more in major axis, and a compound of LnaSibOcNd (wherein 2<a<4, 2<b<3, 0<c<7, 2<d<4) is contained in a grain boundary phase.

### Claim 3 (depends on 1)

The Si3N4 sintered body according to claim 1, wherein said Ln2O3 and said Ln are Yb2O3 and Yb, respectively.

### Claim 4 (depends on 3)

The Si3N4 sintered body according to claim 3, wherein a compound Yb4Si2O7N2 is contained in the grain boundary phase.

### Claim 5 (depends on 1)

The Si3N4 sintered body according to claim 1, wherein silicon powder is used as starting material of the Si3N4 sintered body.

### Claim 6 (depends on 1)

A Si3N4 sintered body according to claim 1, wherein sintering temperature of the Si3N4 sintered body is within 1700-1800° C.

### Claim 7

A method for producing an Si3N4 sintered body comprising:
mixing 80 to 99% by weight of a silicon powder having a oxygen content of not more than 1% by weight and 1 to 20% by weight of a powder of oxide Ln2O3 (wherein Ln=Y, Yb or Sm) of at least one element selected from the group consisting of Y, Yb and Sm, thereby providing a powdered raw material;
nitriding a molded body of the resultant raw material in an atmosphere containing nitrogen at a temperature of not higher than 1400° C.; and then
sintering the resultant nitride body in an atmosphere containing nitrogen at a temperature of 1700 to 1950° C.

### Claim 8 (depends on 7)

The method for producing the Si3N4 sintered body according to claim 7, wherein the content of oxygen, Y, Yb and Sm in said powdered raw material is within the range of 0.1 to 2 in terms of a molar ratio of oxides, SiO2/Ln2O3.

### Claim 9 (depends on 8)

The method for producing the Si3N4 sintered body according to claim 8, wherein the molar ratio of SiO2/Ln2O3 in said powdered raw material is within the range of 0.1 to 0.8.

### Claim 10 (depends on 7)

The method for producing the Si3N4 sintered body according to claim 7, wherein a reducing coating agent is further added in an amount of 1 to 10% by weight based on the weight of the silicon powder to and mixed with said powdered raw material, and a molded body of the raw material is treated with heat in a vacuum of not more than 100 Torr or in an atmosphere containing nitrogen at a temperature of 200 to 800° C., and then said nitriding treating and sintering are performed.

### Claim 11 (depends on 10)

The method for producing the Si3N4 sintered body according to claim 10, wherein said reducing coating agent is a compound including C, H, O and metal cations.

### Claim 12 (depends on 11)

The method for producing the Si3N4 sintered body according to claim 11, wherein said reducing coating agent is a coupling agent including Si or Ti as the metal cations.