# US 2001/0027083 A1 · Method for forming a copper interconnect using a multi-platen chemical mechanical polishing (CMP) process

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027083 A1
- Document ID: US20010027083A1
- Status: Published application
- Kind: A1
- Application number: 09/835,276
- Filed: 2001-04-16
- Published: 2001-10-04
- Earliest claimed: 1999-07-13
- Assignees: Motorola, Inc.
- Inventors: Janos Farkas; Brian G. Anthony; Abbas Guvenilir; Mohammed Rabiul Islam; Venkat Kolagunta; John Mendonca; Rajesh Tiwari; Suresh Venkatesan
- Web page: https://patentgrep.com/patent/US20010027083A1

## CPC

- H10W 20/062: {by smoothing of conductive parts, e.g. by planarisation}
- H10P 52/403: {of conductive or resistive materials}
- H10P 70/277: {the processing being a planarisation of conductive layers}
- H10P 95/062: {involving a dielectric removal step}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A copper interconnect polishing process begins by polishing (17) a bulk thickness of copper (63) using a first platen. A second platen is then used to remove (19) a thin remaining interfacial copper layer to expose a barrier film (61). Computer control (21) monitors polish times of the first and second platen and adjusts these times to improve wafer throughput. One or more platens and/or the wafer is rinsed (20) between the interfacial copper polish and the barrier polish to reduce slurry cross contamination. A third platen and slurry is then used to polish away exposed portions of the barrier (61) to complete polishing of the copper interconnect structure. A holding tank that contains anti-corrosive fluid is used to queue the wafers until subsequent scrubbing operations (25). A scrubbing operation (25) that is substantially void of light is used to reduce photovoltaic induced corrosion of copper in the drying chamber of the scubber.

## Claims

### Claim 1

A method for forming an interconnect comprising:
forming a dielectric layer over a semiconductor device substrate;
forming an opening in the dielectric layer;
forming a barrier layer over the dielectric layer and within the opening;
forming a bulk metallic layer over the barrier layer;
polishing the bulk metallic layer using a first polish process;
polishing the barrier layer using a second polish process wherein the second polish process includes a slurry containing a pH adjusted silica abrasive, and a corrosion inhibitor.

### Claim 2 (depends on 1)

The method of claim 1 wherein the pH adjusted silica abrasive has a pH level substantially within a range of 8 to 11.

### Claim 3 (depends on 1)

The method of claim 1 wherein the pH adjusted silica abrasive has a pH level substantially within a range of 2 to 6.

### Claim 4 (depends on 1)

The method of claim 1 wherein the pH adjusted silica abrasive has a pH level substantially within a range of 8.0 to 9.0.

### Claim 5 (depends on 1)

The method of claim 1 wherein the pH adjusted silica abrasive has a pH that is adjusted by the presence of ammonium hydroxide within the slurry.

### Claim 6 (depends on 1)

The method of claim 1 wherein the barrier layer comprises predominantly tantalum.

### Claim 7 (depends on 1)

The method of claim 1 wherein the bulk metallic layer comprises predominantly copper.

### Claim 8 (depends on 7)

The method of claim 7 wherein the bulk metallic layer comprising predominantly copper includes a lower seed layer comprised of CVD copper and an upper bulk region comprised of electroplated copper.

### Claim 9 (depends on 1)

The method of claim 1, wherein the step of polishing the bulk metallic layer comprises the steps of:
polishing a top portion of the bulk metallic layer using a first platen that polishes at a first removal rate.
polishing a bottom portion of the bulk metallic layer that underlies the top portion of the bulk metallic layer using a second platen that polishes at a second removal rate that is less than the first removal rate.

### Claim 10 (depends on 9)

The method of claim 9, further comprising rinsing the semiconductor device substrate after polishing the top portion of the bulk metallic layer and before polishing the bottom portion of the bulk metallic layer.

### Claim 11 (depends on 9)

The method of claim 9, wherein rinsing the semiconductor device substrate is performed after polishing the bottom portion of the bulk metallic layer.

### Claim 12 (depends on 9)

The method of claim 9 wherein:
polishing the top portion of the bulk metallic layer includes using a first polishing down force of 2-6 psi; and
polishing the bottom portion of the bulk metallic layer includes using a second polishing down force of 0.5-4 psi, wherein the second polishing down force is less than the first polishing down force.

### Claim 13 (depends on 9)

The method of claim 9, wherein polishing the top portion of the bulk metallic layer is a timed polish process and polishing the bottom portion of the bulk metallic layer is optically endpointed.

### Claim 14 (depends on 9)

The method of claim 9, wherein the first platen uses a slurry that contains an abrasive, an oxidizer, and a corrosion inhibitor.

### Claim 15 (depends on 14)

The method of claim 14, wherein the first platen uses a slurry that contains an alumina abrasive as the abrasive, hydrogen peroxide as the oxidizer, and 1, 2, 4 triazole as the corrosion inhibitor.

### Claim 16 (depends on 9)

The method of claim 9, wherein the first and second removal rates are compared to each other and the first and second removal rates are occasionally adjusted by process changes in response thereto.

### Claim 17 (depends on 1)

The method of claim 1, wherein polishing the bulk metallic layer comprises:
polishing a top portion of the bulk metallic layer on a first platen;
polishing a bottom portion of the bulk metallic layer on a second platen; and
polishing the barrier layer on a third platen.

### Claim 18 (depends on 17)

The method of claim 17, further comprising rinsing the semiconductor device substrate after polishing the bottom portion of the bulk metallic layer and before polishing the barrier layer.

### Claim 19 (depends on 18)

The method of claim 18, further comprising rinsing the second and third platen.

### Claim 20 (depends on 1)

The method of claim 1, wherein the slurry comprises at least approximately 2% 1, 2, 4 triazole by volume as the corrosion inhibitor.

### Claim 21 (depends on 1)

The method of claim 1 wherein the slurry comprises ammonium hydroxide.

### Claim 22 (depends on 1)

The method of claim 1 further comprising placing semiconductor device substrate into a holding tank, wherein the holding tank contains a metal corrosion inhibitor.

### Claim 23 (depends on 1)

The method of claim 1 further comprising:
placing the semiconductor device substrate into a scubber after polishing the barrier layer;
cleaning the semiconductor device substrate within the scrubber; and
drying the semiconductor device substrate after cleaning the semiconductor device substrate, wherein drying is performed in an environment that is substantially void of visible light.

### Claim 24

A method for forming an interconnect comprising:
forming a copper containing interconnect over a semiconductor device substrate, wherein forming the copper-containing interconnect includes removing portions of a copper containing layer using a polishing process;
cleaning the semiconductor device substrate using a wet cleaning process; and
drying the semiconductor device substrate after cleaning the semiconductor device substrate, wherein drying is performed in an environment that is substantially void of visible light.

### Claim 25 (depends on 24)

The method of claim 24, wherein drying the semiconductor device substrate further comprises rotating the semiconductor device substrate about a central axis of the semiconductor device substrate.

### Claim 26 (depends on 24)

The method of claim 24 wherein drying the semiconductor device substrate further comprises flowing heated air across a surface of the semiconductor device substrate while rotating the semiconductor device substrate.

### Claim 27 (depends on 24)

The method of claim 24 wherein drying the semiconductor device substrate further comprises applying an energy source to the semiconductor device substrate, and wherein the energy source does not induce a photovoltaic effect on the interconnect.

### Claim 28 (depends on 24)

The method of claim 24, wherein cleaning further comprises ultrasonically cleaning the semiconductor device substrate.

### Claim 29 (depends on 24)

The method of claim 24 wherein cleaning further comprises mechanically scrubbing the semiconductor device substrate

### Claim 30

A method for forming a interconnect comprising:
forming a barrier layer over a semiconductor device substrate;
forming a bulk metal layer over the barrier layer;
placing the semiconductor device substrate onto a first platen;
polishing the bulk metal layer using a first platen;
removing the semiconductor device substrate from the first platen;
rinsing the first platen, a second platen, and the semiconductor device substrate after removing the semiconductor device substrate from the first platen and before placing the semiconductor device substrate onto a second platen;
placing the semiconductor device substrate onto the second platen and polishing the barrier layer using the second platen.

### Claim 31 (depends on 30)

The method of claim 30 wherein one of either the first platen or the second platen supports polishing using an alumina abrasive and the other another of the first platen or the second platen supports polishing using a silica abrasive.

### Claim 32 (depends on 30)

The method of claim 30 wherein one of either the first platen or the second platen supports polishing using a slurry with a first pH and another of the first platen or the second platen supports polishing using a slurry with a second pH wherein the first pH is different from the second pH.

### Claim 33

A method for forming an interconnect comprising:
forming a metal interconnect material over a surface of a wafer;
polishing a first portion of the interconnect using a first platen and a first polish process;
polishing the second portion of the interconnect using a second platen and a second polish process;
comparing a first platen polish time to second platen polish time and adjusting an ending polish time of at least one of the first polish process and the second polish process in response to comparing.

### Claim 34 (depends on 33)

The method of claim 33, wherein the ending polish time of at least one of the first polish process and the second polish process are occasionally adjusted to be substantially equal to each other over time.

### Claim 35 (depends on 33)

The method of claim 33 wherein a downforce pressure of one of either the first or second polish process is changed in response to the step of comparing.

### Claim 36 (depends on 33)

The method of claim 33 wherein a slurry flow rate of one of either the first or second polish process is changed in response to the step of comparing.

### Claim 37 (depends on 33)

The method of claim 33 wherein the platen movement speed of one of either the first or second polish process is changed in response to the step of comparing.

### Claim 38 (depends on 33)

The method of claim 33 wherein the interconnect is a copper interconnect.

### Claim 39 (depends on 33)

The method of claim 33 wherein the polishing rate of one of either the first polish process or the second polish process are occasionally adjusted in response to the step of comparing.

### Claim 40 (depends on 33)

The method of claim 33 wherein the first polish process removes interconnect material at a rate substantially greater than a removal rate in the second polishing process.

### Claim 41

A method for forming a interconnect comprising:
forming a interconnect material over a semiconductor substrate, the interconnect material comprising a top bulk metal layer and a lower barrier layer;
polishing an upper portion of the bulk metal layer at a first removal rate using a first platen;
polishing a lower portion of the bulk metal layer at a second removal rate using a second platen wherein the first removal rate is greater than the second removal rate; and
polishing the barrier layer using a third platen.

### Claim 42 (depends on 41)

The method of claim 41 wherein the interconnect material comprises primarily copper overlying a tantalum-containing barrier layer.

### Claim 43 (depends on 41)

The method of claim 41 wherein the second platen supports an alumina slurry and the third platen supports an alumina slurry.

### Claim 44

A method for forming a interconnect comprising:
forming a dielectric layer over a semiconductor device substrate;
forming an opening in the dielectric layer;
forming a barrier layer over the dielectric layer and within the opening;
forming a bulk metallic layer over the barrier layer;
polishing a first portion of the bulk metallic layer using a first polish process;
polishing a second portion of the bulk metallic layer using a second polish process;
polishing the barrier layer and a first exposed portions of the dielectric layer using a third polish process wherein the third polish process is further characterized as a dielectric buff process;
polishing a remaining portion of the bulk metallic layer and a second exposed portion of the dielectric layer using a fourth polish process.

### Claim 45 (depends on 44)

The method of claim 44 wherein the barrier layer comprises predominantly tantalum.

### Claim 46 (depends on 44)

The method of claim 44 wherein the bulk metallic layer comprises predominantly copper.

### Claim 47 (depends on 44)

The method of claim 44 wherein the bulk metallic layer comprising predominantly copper includes a lower seed layer comprised of CVD copper and an upper bulk region comprised of electroplated copper.

### Claim 48 (depends on 44)

The method of claim 44, wherein the step of polishing the bulk metallic layer comprises the steps of:
polishing a first portion of the bulk metallic layer using a first platen that polishes at a first removal rate.
polishing a second portion of the bulk metallic layer that underlies the top portion of the bulk metallic layer using a second platen that polishes at a second removal rate that is less than the first removal rate;

### Claim 49 (depends on 48)

The method of claim 48, further comprising rinsing the semiconductor device substrate after polishing the first portion of the bulk metallic layer and before polishing the second portion of the bulk metallic layer.

### Claim 50 (depends on 44)

The method of claim 44, wherein rinsing the semiconductor device substrate is performed after polishing the second portion of the bulk metallic layer.

### Claim 51 (depends on 44)

The method of claim 44 wherein:
polishing the first portion of the bulk metallic layer includes using a first polishing down force of 2-6 psi; and
polishing the second portion of the bulk metallic layer includes using a second polishing down force of 0.5-4 psi, wherein the second polishing down force is less than the first polishing down force.

### Claim 52 (depends on 44)

The method of claim 44, wherein polishing the top portion of the bulk metallic layer is a timed polish process and polishing the bottom portion of the bulk metallic layer is optically endpointed.

### Claim 53 (depends on 48)

The method of claim 48, wherein the first platen uses a slurry that contains an abrasive, an oxidizer, and a corrosion inhibitor.

### Claim 54 (depends on 48)

The method of claim 48, wherein the first platen uses a slurry that contains an alumina abrasive as the abrasive, hydrogen peroxide as the oxidizer, and 1, 2, 4 triazole as the corrosion inhibitor.

### Claim 55 (depends on 48)

The method of claim 48, wherein the first and second removal rates are compared to each other and the first and second removal rates are occasionally adjusted by process changes in response thereto.

### Claim 56 (depends on 44)

The method of claim 44, wherein polishing barrier layer is performed using a third platen.

### Claim 57 (depends on 56)

The method of claim 56, further comprising rinsing the semiconductor device substrate after polishing the second portion of the bulk metallic layer and before polishing the barrier layer.

### Claim 58 (depends on 57)

The method of claim 57, further comprising rinsing the second and third platen.

### Claim 59 (depends on 44)

The method of claim 44 further comprising placing semiconductor device substrate into a holding tank, wherein the holding tank contains a metal corrosion inhibitor.

### Claim 60 (depends on 44)

The method of claim 44 wherein polishing a remaining portion of the bulk metallic layer includes using a fourth platen.

### Claim 61 (depends on 60)

The method of claim 60 wherein polishing the remaining portion removes the bulk metallic layer at removal rate that is less than a bulk metallic layer removal rate of the second polish process.

### Claim 62

A method for forming a metallic interconnect comprising:
forming the metallic interconnect over a semiconductor substrate using a polishing process;
storing the semiconductor substrate having a metallic interconnect in a holding tank that contains fluid, the fluid containing a copper corrosion inhibitor; and
removing the semiconductor substrate from the holding tank for subsequent processing.

### Claim 63 (depends on 62)

The method of claim 62, wherein the inhibitor is further characterized as 1, 2, 4 triazole.

### Claim 64 (depends on 62)

The method of claim 62, wherein the holding tank is periodically refreshed at intervals in a range of approximately 2-24 hours.