# US 2001/0027030 A1 · Method for cleaning a process chamber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027030 A1
- Document ID: US20010027030A1
- Status: Published application
- Kind: A1
- Application number: 09/874,882
- Filed: 2001-06-05
- Published: 2001-10-04
- Earliest claimed: 1998-09-30
- Assignees: Applied Materials, Inc.
- Inventors: Anand Vasudev; Toshio Itoh; Ramamujapuram A. Srinivas; Frederick Wu; Li Wu; Brian Boyle; Mei Chang
- Web page: https://patentgrep.com/patent/US20010027030A1

## CPC

- H10P 72/0406: {for cleaning followed by drying, rinsing, stripping, blasting or the like}
- Y10S 438/905: Cleaning of reaction chamber
- Y10S 438/906: Cleaning of wafer as interim step
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for the in situ cleaning of a semiconductor deposition chamber utilized for the deposition of a semiconductor material such as titanium or titanium nitride comprising, between wafers, introducing chlorine gas into the chamber at elevated temperature, purging the chamber with an inert gas and evacuating it before introduction of the next wafer. A two-stage between wafer cleaning process is carried out by introducing chlorine into the chamber at elevated temperature, thereafter initiating a plasma without removing the chlorine, purging the chamber with an inert gas and evacuating it before introduction of the next wafer. In a preferred embodiment, a thin protective film of titanium is deposited on the inner surfaces of the chamber prior to utilizing the chamber for the deposition of such material. The protective layer is replenished following each two-stage cleaning.

## Claims

### Claim 1

A method for in situ cleaning of a deposition chamber for processing semiconductor wafers comprising the steps of, between processing of said wafers:
a) introducing chlorine gas into the chamber at elevated temperature;
b) purging the chlorine from the chamber with an inert gas; and
c) pumping down the chamber to remove the contents thereof.

### Claim 2 (depends on 1)

The method in accordance with claim 1, wherein said wafers are being processed by deposition thereon of a coating of material by chemical vapor deposition from a precursor therefor.

### Claim 3 (depends on 2)

The method in accordance with claim 2, wherein the material is selected from the group of titanium nitride and titanium and the precursor is titanium tetrachloride.

### Claim 4 (depends on 1)

The method in accordance with claim 1, wherein the elevated temperature is from about approximately 500-700° C.

### Claim 5 (depends on 1)

The method in accordance with claim 1, wherein step a) is performed for approximately 5-60 seconds.

### Claim 6 (depends on 1)

The method in accordance with claim 1, wherein the chlorine gas in step a) is admixed with up to 99.9% by volume of an inert gas.

### Claim 7 (depends on 6)

The method in accordance with claim 6, wherein the inert gas is selected from the group consisting of argon, nitrogen and helium.

### Claim 8 (depends on 6)

The method in accordance with claim 6, wherein the inert gas utilized in step b) is the same as utilized in step a).

### Claim 9 (depends on 1)

The method in accordance with claim 1 further comprising the step of inserting a placebo wafer into the chamber prior to step a).

### Claim 10 (depends on 1)

The method in accordance with claim 1 further comprising the step of purging the chamber prior to step a).

### Claim 11

A method for the in situ cleaning of a deposition chamber comprising the steps of:
a) introducing chlorine gas into the chamber at elevated temperature;
b) maintaining the conditions of step a), initiating a plasma containing the chlorine gas in the chamber;
c) purging the chamber with an inert gas; and
d) pumping down the chamber to remove the contents thereof.

### Claim 12 (depends on 11)

The method in accordance with claim 11, wherein the elevated temperature is from about approximately 500-700° C.

### Claim 13 (depends on 11)

The method in accordance with claim 11, wherein step a) is performed for approximately 5-50 seconds, and step b) is performed for approximately 2-20 seconds.

### Claim 14 (depends on 11)

The method in accordance with claim 11, wherein the chlorine gas in step a) is admixed with up to 99.9% by volume of an inert gas.

### Claim 15 (depends on 14)

The method in accordance with claim 14, wherein the inert gas is selected from the group consisting of argon, nitrogen and helium.

### Claim 16 (depends on 14)

The method in accordance with claim 14, wherein the inert gas utilized in step c) is the same as utilized in step a).

### Claim 17 (depends on 11)

The method in accordance with claim 11, wherein step b) is performed at an RF power of approximately 50-900 Watts.

### Claim 18 (depends on 17)

The method in accordance with claim 17, wherein the power in step c) is reduced to approximately one-half the level utilized in step b).

### Claim 19 (depends on 11)

The method in accordance with claim 11 further comprising the step of inserting a placebo wafer into the chamber prior to step a).

### Claim 20 (depends on 11)

The method in accordance with claim 11 further comprising the step of purging the chamber prior to step a).

### Claim 21 (depends on 11)

The method in accordance with claim 11 wherein the method is performed between processing of individual semiconductor wafers.

### Claim 22 (depends on 11)

The method in accordance with claim 11 further comprising the step of depositing a protective coating of material in the chamber following step d).

### Claim 23 (depends on 22)

A method in accordance with claim 22, wherein the protective coating is selected from the group consisting of titanium and titanium nitride that is deposited on the interior surfaces of the chamber by chemical vapor deposition.

### Claim 24 (depends on 22)

The method in accordance with claim 22, wherein the protective coating is between about 50 Å and 1μthick.

### Claim 25

A method for the in situ cleaning of a deposition chamber comprising the steps of:
a) initiating a plasma containing chlorine in the chamber;
b) halting the plasma and, introducing chlorine gas into the chamber at elevated temperature;
c) purging the chamber with an inert gas; and
d) pumping down the chamber to remove the contents thereof.

### Claim 26

In a system for controlling the process sequence of wafers through a semiconductor processing tool containing at least one chamber for performing the deposition of a material selected from the group consisting of titanium and titanium nitride, a computer readable medium in a general purpose computer system that operates as a special purpose controller when executing a cleaning program for said at least one chamber to perform a process comprising the steps of:
a) introducing chlorine gas into said at least one chamber at elevated temperature;
b) purging said at least one chamber with an inert gas; and
c) pumping down said at least one chamber to remove the contents thereof.

### Claim 27

In a system for controlling the process sequence of wafers through a semiconductor processing tool containing at least one chamber for performing the deposition of a material selected from the group consisting of titanium and titanium nitride, a computer readable medium in a general purpose computer system that operates as a special purpose controller when executing a cleaning program for said at least one chamber to perform a process comprising the steps of:
a) introducing chlorine gas into said at least one chamber at elevated temperature;
b) maintaining the conditions of step a), initiating a plasma containing chlorine in said at least one chamber;
c) purging said at least one chamber with an inert gas; and
d) pumping down said at least one chamber to remove the contents thereof.

### Claim 28 (depends on 27)

A computer readable medium in accordance with claim 27, wherein said at least one chamber has on interior surface thereof, a protective coating of a material selected from the group consisting of titanium and titanium nitride, further comprising the steps of, following step d):
depositing the protective coating on the interior surfaces of said at least one chamber.