# US 2001/0027025 A1 · Projection lithography photomask blanks, preforms and method of making

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027025 A1
- Document ID: US20010027025A1
- Status: Published application
- Kind: A1
- Application number: 09/876,194
- Filed: 2001-06-06
- Published: 2001-10-04
- Earliest claimed: 1999-02-12
- Assignees: Corning Incorporated
- Inventors: George Edward Berkey; Lisa Anne Moore; Charles Chunzhe Yu
- Web page: https://patentgrep.com/patent/US20010027025A1

## CPC

- C03B 23/07: by blowing, e.g. for making electric bulbs {(C03B23/097 takes precedence)}
- C03B 19/1415: {Reactant delivery systems}
- C03B 19/1423: {Reactant deposition burners}
- C03B 19/1453: {Thermal after-treatment of the shaped article, e.g. dehydrating, consolidating, sintering}
- C03B 19/1469: {Means for changing or stabilising the shape or form of the shaped article or deposit}
- C03B 19/1492: {Deposition substrates, e.g. targets}
- C03B 23/043: Heating devices specially adapted for re-forming tubes or rods in general, e.g. burners
- C03B 23/045: Tools or apparatus specially adapted for re-forming tubes or rods in general, e.g. glass lathes, chucks (C03B23/043 takes precedence)
- C03B 23/051: by gravity, e.g. sagging {(C03B23/093 takes precedence)}
- C03C 3/06: with more than 90% silica by weight, e.g. quartz {(C03C3/045 takes precedence)}
- C03C 4/0085: {for UV-transmitting glass}
- G03F 1/60: Substrates
- C03B 2201/07: Impurity concentration specified
- C03B 2201/075: Hydroxyl ion (OH)
- C03B 2201/12: doped with fluorine (C03B2201/14 takes precedence)
- C03B 2201/21: doped with molecular hydrogen
- C03B 2207/02: Elongated flat flame or slit-nozzle type
- C03B 2207/06: Concentric circular ports
- C03B 2207/20: Specific substances in specified ports, e.g. all gas flows specified
- C03B 2207/32: Non-halide
- C03B 2207/52: Linear array of like burners
- C03B 2207/54: combined with means for heating the deposit, e.g. non-deposition burner
- C03B 2207/66: Relative motion
- C03C 2201/12: containing fluorine (C03C2201/14 takes precedence)
- C03C 2201/21: containing molecular hydrogen
- C03C 2203/50: After-treatment
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

The invention includes methods of making lithography photomask blanks. The invention also includes lithography photomask blanks and preforms for producing lithography photomask. The method of making a lithography photomask blank includes providing a soot deposition surface, producing SiO2 soot particles and projecting the SiO2 soot particles toward the soot deposition surface. The method includes successively depositing layers of the SiO2 soot particle on the deposition surface to form a coherent SiO2 porous glass preform body comprised of successive layers of the SiO2 soot particles and dehydrating the coherent SiO2 glass preform body to remove OH from the preform body. The SiO2 is exposed to and reacted with a fluorine containing compound and consolidated into a nonporous silicon oxyfluoride glass body with parallel layers of striae. The method further includes forming the consolidated silicon oxyfluoride glass body into a photomask blank having a planar surface with the orientation of the striae layer parallel to the photomask blank planar surface.

## Claims

### Claim 1

A method of making a lithography photomask blank, comprising the steps of:
providing a soot deposition surface,
producing a plurality of SiO2 soot particles and projecting said SiO2 soot particles towards said soot deposition surface,
successively depositing said SiO2 soot particles on said deposition surface to form a coherent SiO2 porous glass preform body,
dehydrating said coherent SiO2 glass preform body to remove OH from said coherent SiO2 glass preform body,
exposing said SiO2 to a fluorine containing atmosphere and consolidating the coherent SiO2 glass preform body into a silicon oxyfluoride glass body having less than 1×1017 H2 molecules/cm3,
forming said consolidated silicon oxyfluoride glass body into a photomask blank having less than 1×1017 H2 molecules/cm3 and a planar surface.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein providing a soot deposition surface includes providing a substrate, said substrate having a substrate initial deposition surface.

### Claim 3 (depends on 2)

A method as claimed in claim 2, wherein said substrate initial deposition surface is curved.

### Claim 4 (depends on 2)

A method as claimed in claim 2, wherein said substrate initial deposition surface is a flat planar surface.

### Claim 5 (depends on 1)

A method as claimed in claim 1, wherein producing and projecting SiO2 soot particles includes providing a SiO2 soot deposition burner which produces a conversion site flame, feeding a SiO2 feedstock to the burner wherein said flame converts said feedstock into a SiO2 soot particle stream aimed at said deposition surface.

### Claim 6 (depends on 5)

A method as claimed in claim 5, wherein producing and projecting said SiO2 soot particles and successively depositing said SiO2 soot particles further includes providing relative motion between said burner and said soot deposition surface.

### Claim 7 (depends on 1)

A method as claimed in claim 1, the step of successively depositing said soot particles to form a coherent porous glass preform further includes depositing said soot particles by thermophoresis at a soot deposition temperature and with a soot deposition size wherein said deposited soot particles are bonded together to form said coherent porous glass preform body.

### Claim 8 (depends on 1)

A method as claimed in claim 1, wherein dehydrating further includes, exposing said coherent SiO2 glass preform body to a heated halide containing atmosphere.

### Claim 9 (depends on 8)

A method as claimed in claim 8, wherein said heated halide containing atmosphere is comprised of helium and chlorine.

### Claim 10 (depends on 8)

A method as claimed in claim 8, wherein said heated halide containing atmosphere includes fluorine.

### Claim 11 (depends on 1)

A method as claimed in claim 1, wherein exposing said preform body to said fluorine containing atmosphere and consolidating the preform body into a silicon oxyfluoride glass body includes replacing a plurality of silicon to oxygen bonds with a plurality of silicon to fluorine bonds.

### Claim 12 (depends on 1)

A method as claimed in claim 1, wherein said fluorine containing atmosphere includes SiF4.

### Claim 13 (depends on 1)

A method as claimed in claim 1, wherein said fluorine containing atmosphere includes CF4.

### Claim 14 (depends on 1)

A method as claimed in claim 1, wherein said fluorine containing atmosphere includes C2F6.

### Claim 15 (depends on 1)

A method as claimed in claim 1, wherein said fluorine containing atmosphere includes SF6.

### Claim 16 (depends on 1)

A method as claimed in claim 1, wherein exposing said SiO2 to a fluorine containing atmosphere comprises exposing said SiO2 to a fluorine source compound concurrent with producing said SiO2 soot particles and projecting said SiO2 soot particles.

### Claim 17 (depends on 16)

A method as claimed in claim 16, further comprising exposing said coherent SiO2 porous glass preform body to a fluorine containing atmosphere.

### Claim 18 (depends on 1)

A method as claimed in claim 1, wherein said fluorine containing atmosphere includes helium.

### Claim 19 (depends on 1)

A method as claimed in claim 1, wherein OH is first removed by dehydrating and fluorine is incorporated into the dehydrated SiO2 soot and consolidated into said silicon oxyfluoride glass body with said glass containing at least
0.5 wt. % F.

### Claim 20 (depends on 1)

A method as claimed in claim 1, wherein said consolidated silicon oxyfluoride glass consists essentially of Si, O, and F.

### Claim 21 (depends on 1)

A method as claimed in claim 1, wherein said consolidated silicon oxyfluoride glass has a F wt. % concentrated ranging from 0.5 to 3 wt. % and has an OH content less than 10 ppm.

### Claim 22 (depends on 1)

A method as claimed in claim 1, wherein dehydrating includes heating the preform body to a temperature in the range from 900 to 1100° C. in a dehydrating atmosphere, and exposing to said fluorine containing body and consolidating into a silicon oxyfluoride glass includes heating the dehydrated preform body to a temperature in the range from 1125 to 1325° C. in an atmosphere containing F, and then sintering said preform body at a temperature in the range from 1350° C. to 1550° C.

### Claim 23 (depends on 1)

A method as claimed in claim 1, wherein forming said consolidated silicon oxyfluoride glass body into a photomask blank having a planar surface further includes polishing said silicon oxyfluoride glass body.

### Claim 24 (depends on 1)

A method as claimed in claim 1, further comprising transmitting 157 nm wavelength light through said formed photomask blank planar surface.

### Claim 25 (depends on 1)

A method as claimed in claim 1, further comprising forming a lithographic image pattern on said photomask blank planar surface.

### Claim 26 (depends on 25)

A method as claimed in claim 25, further comprising impinging light including the 157 nm wavelength towards said photomask blank planar surface to form a projection image pattern and projecting the projection image pattern onto a radiation sensitive material.

### Claim 27

A method of making a lithography photomask blank having a photomask blank large dimension L and a photomask blank thickness T comprising the steps of:
providing a coherent SiO2 porous glass preform column,
dehydrating said coherent SiO2 porous preform column to remove OH from said coherent SiO2 glass preform column,
exposing said SiO2 to a fluorine containing atmosphere and consolidating the coherent SiO2 glass preform column into a consolidated silicon oxyfluoride glass having less than 1×1017 H2 molecules/cm3,
forming said silicon oxyfluoride glass into a photomask blank having less than 1×1017 H2 molecules/cm3 and a planar surface.

### Claim 28 (depends on 27)

A method as claimed in claim 27, wherein consolidating and providing said SiO2 porous glass preform column further includes consolidating the preform column into a consolidated silicon oxyfluoride glass column having a column height CH and a column diameter CD, wherein (CD)2 CH≧L2T.

### Claim 29 (depends on 28)

A method as claimed in claim 28, wherein said silicon oxyfluoride glass has a diameter greater than L and a thickness greater than T.

### Claim 30 (depends on 29)

A method as claimed in claim 29, wherein said diameter is greater than {square root}{square root over (2)} L.

### Claim 31 (depends on 28)

A method as claimed in claim 28, wherein said SiO2 porous glass preform column has a preform height PH and a preform diameter PD, with PH(PD)2≈8(CD)2 CH.

### Claim 32 (depends on 28)

A method as claimed in claim 28, said method including heating said glass column to a flow temperature in the range from 1800 to 2300° C.

### Claim 33 (depends on 32)

A method as claimed in claim 32, wherein heating said glass column includes applying a force to the glass column.

### Claim 34

A method as claimed in 27, wherein said silicon oxyfluoride glass consists essentially of Si, O, and F.

### Claim 35

A method as claimed in 27, wherein said silicon oxyfluoride glass has an OH content ≦10 ppm and a F wt. % of at least 0.5 wt. %.

### Claim 36

A method of making a lithography photomask blank having a photomask blank large dimension L and a photomask blank thickness T comprising the steps of:
providing a cylindrical coherent SiO2 porous glass preform column comprised of a plurality of SiO2 soot particles,
dehydrating said coherent SiO2 porous glass preform column to remove OH from said coherent SiO2 glass preform column,
exposing said coherent SiO2 glass preform column to a fluorine containing atmosphere and consolidating the coherent SiO2 glass preform column into a consolidated silicon oxyfluoride glass column having less than 1×1017 H2 molecules/cm3 and forming said consolidated silicon oxyfluoride glass column into a photomask blank having a planar surface.

### Claim 37 (depends on 36)

A method as claimed in claim 36, wherein said consolidated silicon oxyfluoride glass column has a column height CH and a column radius CR wherein CR≧L/2 and CH≧T.

### Claim 38 (depends on 37)

A method as claimed in claim 37, wherein CR≧({square root}{square root over (2)})L/2.

### Claim 39 (depends on 37)

A method as claimed in claim 37, wherein said SiO2 porous glass preform column has a preform height PH and a preform diameter PD, with PH(PD)2≧8CH(CR)2.

### Claim 40

A method as claimed in 36, wherein said silicon oxyfluoride glass consists essentially of Si, O, and F.

### Claim 41 (depends on 36)

A method as claimed in claim 36, wherein said silicon oxyfluoride glass has an OH content ≦10 ppm and a F wt. % >0.5 wt. %.

### Claim 42

A glass lithography mask blank consolidated preform comprising a silicon oxyfluoride glass column having an OH content ≦10 ppm, a F wt. % concentration ≧0.5 wt. %, said silicon oxyfluoride glass column having less than 1×1017 H2 molecules/cm3.

### Claim 43 (depends on 42)

A mask blank preform as claimed in claim 42, wherein said silicon oxyfluoride glass consists essentially of Si, O, and F.

### Claim 44 (depends on 42)

A mask blank preform as claimed in claim 42, wherein said silicon oxyfluoride glass has a fluorine content in the range from 0.5 to 3 wt. % F.

### Claim 45

A mask blank preform as claimed in 43, wherein said silicon oxyfluoride glass has a molecular H2 content of less than 5×1016 molecules/cm3.

### Claim 46

A mask blank preform as claimed in 43, wherein said silicon oxyfluoride glass has a chlorine content less than 10 ppm.

### Claim 47 (depends on 42)

A mask blank preform as claimed in claim 42, wherein said silicon oxyfluoride glass has a 157 nm light transmission percentage of at least 70% per 5 mm thickness of glass.

### Claim 48 (depends on 42)

A mask blank preform as claimed in claim 42, wherein said silicon oxyfluoride glass column is free of inclusions having a dimension >1 μm.

### Claim 49

A glass lithography mask blank consolidated preform for forming a lithography mask blank having a mask blank large dimension L and a mask blank thickness T, said mask blank preform comprising a silicon oxyfluoride glass column having less than 1×1017 H2 molecules/cm3 and a column height CH and a column diameter CD, wherein (CD)2CH≧L2T.

### Claim 50 (depends on 49)

A glass mask blank preform as claimed in claim 49, wherein said silicon oxyfluoride glass has an OH content ≦10 ppm, and a F wt. % concentration ≧0.5 wt. %.

### Claim 51 (depends on 49)

A glass mask blank preform as claimed in claim 49, wherein said silicon oxyfluoride glass consists essentially of Si, O, and F.

### Claim 52 (depends on 49)

A glass mask blank preform as claimed in claim 49, wherein said silicon oxyfluoride glass has a fluorine content in the range from 0.5 to 3 wt. % F.

### Claim 53 (depends on 49)

A glass mask blank preform as claimed in claim 49, wherein said silicon oxyfluoride glass has a molecular H2 content of less than 5×1016 molecules/cm3.

### Claim 54 (depends on 49)

A glass mask blank preform as claimed in claim 49, wherein said silicon oxyfluoride glass has a chlorine content less than 10 ppm Cl.

### Claim 55 (depends on 48)

A glass lithography mask blank formed from a glass lithography mask blank preform as claimed in claim 48, wherein said mask blank is comprised of a flat planar glass member having a top planar surface, a bottom planar surface, a mask blank large dimension L and a mask blank thickness T.

### Claim 56

A glass lithography mask blank consolidated preform for forming a lithography mask blank having a mask blank large dimension L and a mask blank thickness T, said mask blank preform comprising a silicon oxyfluoride glass column having less than 1×1017 H2 molecules/cm3 and said glass column having a column height CH and a column radius CR wherein CR≧L/2 and CH≧T.

### Claim 57 (depends on 56)

A glass mask blank preform as claimed in claim 56, wherein said silicon oxyfluoride glass has an OH content ≦10 ppm, a F wt. % concentration ≧0.5 wt. %.

### Claim 58 (depends on 56)

A glass mask blank preform as claimed in claim 56, wherein said silicon oxyfluoride glass consists essentially of Si, O, and F.

### Claim 59 (depends on 56)

A glass mask blank preform as claimed in claim 56, wherein said silicon oxyfluoride glass has a fluorine content in the range from 0.5 to 3 wt. % F.

### Claim 60 (depends on 56)

A glass mask blank preform as claimed in claim 56, wherein said silicon oxyfluoride glass has a molecular H2 content of less than 5×1016 molecules/cm3.

### Claim 61 (depends on 56)

A glass mask blank preform as claimed in claim 56, wherein said silicon oxyfluoride glass has a chlorine content less than 10 ppm Cl.

### Claim 62 (depends on 56)

A glass lithography mask blank formed from a glass lithography mask blank preform as claimed in claim 56, wherein said mask blank is comprised of a flat planar glass member having a top planar surface, a bottom planar surface, a mask blank large dimension L and a mask blank thickness T.

### Claim 63

A lithography photomask blank comprising a flat planar silicon oxyfluoride glass member having a top planar surface and a bottom planar surface, said planar silicon oxyfluoride glass member having an OH content ≦10 ppm, a F wt. % concentration ≧0.5 wt. %, said silicon oxyfluoride glass having less than 1×1017 H2 molecules/cm3 and said top planar surface has a surface roughness ≦0.15 nm rms.

### Claim 64 (depends on 63)

A lithography photomask blank as claimed in claim 63, wherein said planar silicon oxyfluoride glass member has a 157 nm light transmission percentage of at least 70% per 5 mm thickness of glass.

### Claim 65 (depends on 63)

A lithography photomask blank as claimed in claim 63, wherein said silicon oxyfluoride glass consists essentially of Si, O, and F.

### Claim 66 (depends on 63)

A lithography photomask blank as claimed in claim 63, wherein said silicon oxyfluoride glass has a F wt. % content in the range from 0.5 wt. % to 3 wt. %.

### Claim 67 (depends on 63)

A lithography photomask blank as claimed in claim 63, wherein said flat planar silicon oxyfluoride glass member has a transmission uniformity at 157 nm in the range from −2% to +2%.

### Claim 68 (depends on 63)

A lithography photomask blank as claimed in claim 63, wherein said silicon oxyfluoride glass member is free of inclusions having a dimension >1 μm.

### Claim 69 (depends on 63)

A lithography photomask blank as claimed in claim 63, wherein said silicon oxyfluoride glass member has a birefringence ≦5 nm/cm.

### Claim 70 (depends on 63)

A lithography photomask blank claimed in claim 63, wherein said flat planar silicon oxyfluoride glass member has a thickness of at least 0.6 cm, a length of at least 15 cm, is free of inclusions having a dimension >1 μm, a transmission uniformity at 157 nm in the range from −2 to +2%, transmission at 157 nm >70%, and a birefringence ≦5 nm/cm.

### Claim 71 (depends on 1)

A method as claimed in claim 1, wherein said silicon oxyfluoride glass body has less than 5×1016 H2 molecules/cm3.

### Claim 72 (depends on 1)

A method as claimed in claim 1, wherein said silicon oxyfluoride glass body has no detectable hydrogen.

### Claim 73 (depends on 27)

A method as claimed in claim 27, wherein said silicon oxyfluoride glass column has less than 5×1016 H2 molecules/cm3.

### Claim 74 (depends on 27)

A method as claimed in claim 27, wherein said silicon oxyfluoride glass column has no detectable hydrogen.

### Claim 75 (depends on 36)

A method as claimed in claim 36, wherein said silicon oxyfluoride glass column has less than 5×1016 H2 molecules/cm3.

### Claim 76 (depends on 36)

A method as claimed in claim 36, wherein said silicon oxyfluoride glass column has no detectable hydrogen.

### Claim 77 (depends on 42)

A preform as claimed in claim 42, wherein said silicon oxyfluoride glass column has no detectable hydrogen.

### Claim 78 (depends on 49)

A preform as claimed in claim 49, wherein said silicon oxyfluoride glass column has no detectable hydrogen.

### Claim 79 (depends on 56)

A preform as claimed in claim 56, wherein said silicon oxyfluoride glass column has no detectable hydrogen.

### Claim 80 (depends on 65)

A photomask blank as claimed in claim 65, wherein said silicon oxyfluoride glass has less than 5×1016 H2 molecules/cm3.

### Claim 81 (depends on 65)

A photomask blank as claimed in claim 65, wherein said silicon oxyfluoride glass has no detectable hydrogen.