# US 2001/0027024 A1 · Method of forming a polycide electrode in a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027024 A1
- Document ID: US20010027024A1
- Status: Published application
- Kind: A1
- Application number: 09/817,061
- Filed: 2001-03-27
- Published: 2001-10-04
- Earliest claimed: 2000-03-29
- Assignees: NEC Corporation
- Inventors: Hiroshi Murase
- Web page: https://patentgrep.com/patent/US20010027024A1

## CPC

- H10W 20/031: {of conductive parts of the interconnections}
- H10D 64/231: {Emitter or collector electrodes for bipolar transistors}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

The present invention provides a method of forming an emitter electrode of a bipolar transistor, the emitter electrode comprising a double-layered structure of a polysilicon layer and a refractory metal silicide layer. The method comprises the steps of: removing a natural oxide film from a surface of a polysilicon layer by a sputter-etching process using inert gas ions in the range of acceleration energy from 5 eV to 50 eV; depositing a refractory metal layer on the surface of the polysilicon layer; and carrying out a heat treatment to cause a silicidation reaction to form a refractory metal silicide layer over the polysilicon layer.

## Claims

### Claim 1

A method of forming an emitter electrode of a bipolar transistor, said emitter electrode comprising a double-layered structure of a polysilicon layer and a refractory metal silicide layer, said method comprising the steps of:
removing a natural oxide film from a surface of a polysilicon layer by a sputter-etching process using inert gas ions in the range of acceleration energy from 5 eV to 50 eV;
depositing a refractory metal layer on said surface of said polysilicon layer; and
carrying out a heat treatment to cause a silicidation reaction to form a refractory metal silicide layer over said polysilicon layer.

### Claim 2 (depends on 1)

The method as claimed in claim 1, wherein said inert gas ions comprise argon ions.

### Claim 3 (depends on 1)

The method as claimed in claim 1, wherein said sputter-etching process is a radio frequency plasma etching process.

### Claim 4 (depends on 1)

The method as claimed in claim 1, wherein said refractory metal layer is deposited with keeping said surface of said polysilicon layer from an oxygen atmosphere after said natural oxide film is completely removed.

### Claim 5 (depends on 4)

The method as claimed in claim 4, wherein said refractory metal layer is deposited in the same vacuum chamber in which said sputter-etching process has been carried out.

### Claim 6 (depends on 1)

The method as claimed in claim 1, further comprising the step of: patterning laminations of the refractory metal silicide layer and the polysilicon layer.

### Claim 7 (depends on 1)

The method as claimed in claim 1, wherein said sputter-etching process is carried out by applying a bias voltage in the range of 5 V to 50 V.

### Claim 8

A method of forming an emitter electrode of a bipolar transistor, said emitter electrode comprising a double-layered structure of a polysilicon layer and a refractory metal suicide layer, said method comprising the steps of:
removing a natural oxide film from a surface of a polysilicon layer by a sputter-etching process using inert gas ions by applying a bias voltage level in the range from 5 V to 50 V;
depositing a refractory metal layer on said surface of said polysilicon layer; and
carrying out a heat treatment to cause a silicidation reaction to form a refractory metal silicide layer over said polysilicon layer.

### Claim 9 (depends on 8)

The method as claimed in claim 8, wherein said inert gas ions comprise argon ions.

### Claim 10 (depends on 8)

The method as claimed in claim 8, wherein said sputter-etching process is a radio frequency plasma etching process.

### Claim 11 (depends on 8)

The method as claimed in claim 8, wherein said refractory metal layer is deposited with keeping said surface of said polysilicon layer from an oxygen atmosphere after said natural oxide film is completely removed.

### Claim 12 (depends on 11)

The method as claimed in claim 11, wherein said refractory metal layer is deposited in the same vacuum chamber in which said sputter-etching process has been carried out.

### Claim 13 (depends on 8)

The method as claimed in claim 8, further comprising the step of: patterning laminations of the refractory metal silicide layer and the polysilicon layer.

### Claim 14 (depends on 8)

The method as claimed in claim 8, wherein said inert gas ions are accelerated in the range of 5 eV to 50 eV.

### Claim 15

A method of forming a double-layered structure of a polysilicon layer and a refractory metal silicide layer, said method comprising the steps of:
removing a natural oxide film from a surface of a polysilicon layer by a sputter-etching process using inert gas ions in the range of acceleration energy from 5 eV to 50 eV;
depositing a refractory metal layer on said surface of said polysilicon layer; and
carrying out a heat treatment to cause a silicidation reaction to form a refractory metal silicide layer over said polysilicon layer.

### Claim 16 (depends on 15)

The method as claimed in claim 15, wherein said inert gas ions comprise argon ions.

### Claim 17 (depends on 15)

The method as claimed in claim 15, wherein said sputter-etching process is a radio frequency plasma etching process.

### Claim 18 (depends on 15)

The method as claimed in claim 15, wherein said refractory metal layer is deposited with keeping said surface of said polysilicon layer from an oxygen atmosphere after said natural oxide film is completely removed.

### Claim 19 (depends on 18)

The method as claimed in claim 18, wherein said refractory metal layer is deposited in the same vacuum chamber in which said sputter-etching process has been carried out.

### Claim 20 (depends on 15)

The method as claimed in claim 15, wherein said sputter-etching process is carried out by applying a bias voltage in the range of 5 V to 50 V.

### Claim 21

A method of forming a double-layered structure of a polysilicon layer and a refractory metal silicide layer, said method comprising the steps of:
removing a natural oxide film from a surface of a polysilicon layer by a sputter-etching process using inert gas ions by applying a bias voltage level in the range from 5 V to 50 V;
depositing a refractory metal layer on said surface of said polysilicon layer; and
carrying out a heat treatment to cause a silicidation reaction to form a refractory metal silicide layer over said polysilicon layer.

### Claim 22 (depends on 21)

The method as claimed in claim 21, wherein said inert gas ions comprise argon ions.

### Claim 23 (depends on 21)

The method as claimed in claim 21, wherein said sputter-etching process is a radio frequency plasma etching process.

### Claim 24 (depends on 21)

The method as claimed in claim 21, wherein said refractory metal layer is deposited with keeping said surface of said polysilicon layer from an oxygen atmosphere after said natural oxide film is completely removed.

### Claim 25 (depends on 24)

The method as claimed in claim 24, wherein said refractory metal layer is deposited in the same vacuum chamber in which said sputter-etching process has been carried out.

### Claim 26 (depends on 21)

The method as claimed in claim 21, wherein said inert gas ions are accelerated in the range of 5 eV to 50 eV.
