# US 2001/0027018 A1 · Finishing method for semiconductor wafers using a lubricating boundary layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027018 A1
- Document ID: US20010027018A1
- Status: Published application
- Kind: A1
- Application number: 09/766,958
- Filed: 2001-01-22
- Published: 2001-10-04
- Earliest claimed: 1998-11-06
- Assignees: Beaver Creek Concepts Inc
- Inventors: Charles J. Molnar
- Web page: https://patentgrep.com/patent/US20010027018A1

## CPC

- B24B 37/20: Lapping pads for working plane surfaces
- H10P 52/403: {of conductive or resistive materials}
- B65H 2701/3772: Double-sided
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- B65H: HANDLING THIN OR FILAMENTARY MATERIAL, e.g. SHEETS, WEBS, CABLES

## Abstract

A method of using lubricating boundary layers for finishing semiconductor wafers is described. The lubricating boundary layer thickness is controlled to improve finishing and reduce unwanted surface defects. Differential lubricating boundary layer methods are described to differentially finish semiconductor wafers. Planarization and localized finishing can be improved using differential lubricating boundary layer methods of finishing.

## Claims

### Claim 1

A method of finishing of a semiconductor wafer surface being finished having uniform regions and a plurality of wafer die, each wafer die having a repeating pattern of unwanted raised regions, the method comprising the steps of:
providing a finishing element finishing surface;
supplying an organic boundary lubricant to the interface between the semiconductor wafer surface being finished and the finishing element finishing surface;
positioning the semiconductor wafer surface being finished proximate to the finishing surface;
applying an operative finishing motion in the interface between the semiconductor wafer surface being finished and the finishing element finishing surface; and
wherein
applying the operative finishing motion to the operative finishing interface forms an organic lubricating boundary layer of from 1 to 6 molecules thick which interacts with and adheres to the semiconductor wafer surface for at least a portion of the finishing cycle time.

### Claim 2 (depends on 1)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 1 further comprising an additional step of controlling the thickness of the organic lubricating boundary layer by changing at least one process control parameter in situ based on feed back information from a control subsystem.

### Claim 3 (depends on 1)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 1 wherein applying the operative finishing motion causes the unwanted raised regions to have a temperature of at least 7 degrees centigrade higher than that of the proximate low local regions.

### Claim 4 (depends on 1)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 1 wherein applying the higher pressure comprises applying at least five times higher pressure to the unwanted raised regions when compared to the applied pressure in a lower region proximate to the unwanted raised regions.

### Claim 5 (depends on 1)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 1 wherein the organic boundary layer interaction with and adhesion to the uniform region of the semiconductor wafer surface comprises dipole-dipole interactions.

### Claim 6 (depends on 1)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 1 wherein the unwanted raised regions have a finishing rate measured in angstroms per minute of at least 4 times faster than in a proximate low local region.

### Claim 7 (depends on 1)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 1 wherein applying the operative finishing motion comprises:
applying a higher pressure to the unwanted raised regions compared to the pressure applied to regions below the unwanted raised regions causing less boundary layer lubrication and a higher temperature on the unwanted raised regions and the boundary layer lubrication to be greater and the temperature to be lower on a portion of the semiconductor wafer surface below the unwanted raised regions.

### Claim 8 (depends on 7)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 7 wherein applying the higher pressure comprises applying at least five times higher pressure to the unwanted raised region when compared to the applied pressure in a lower region proximate to the unwanted raised regions.

### Claim 9 (depends on 7)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 7 wherein applying the operative finishing motion causes the unwanted raised regions to have a temperature of at least 7 degrees centigrade higher than that of the proximate low local regions.

### Claim 10 (depends on 7)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 7 wherein the unwanted raised regions have a finishing rate measured in angstroms per minute of at least 4 times faster than in a proximate low local region.

### Claim 11 (depends on 7)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 7 wherein the finishing element finishing surface comprises an organic synthetic polymer having a flexural modulus of at least 20,000 psi when measured according to ASTM 790 B at 73 degrees Fahrenheit.

### Claim 12 (depends on 1)

The method of finishing a semiconductor wafer surface being finished according to claim 1 wherein the organic boundary lubricating layer is capable of changing from a solid film to a different physical form in the operative finishing interface temperature range.

### Claim 13

A method of finishing of a semiconductor wafer surface being finished having uniform regions having a plurality of unwanted raised regions, the method comprising the steps of:
providing a finishing element finishing surface;
supplying an organic boundary lubricant to the interface between the semiconductor wafer surface being finished and the finishing element finishing surface;
positioning the semiconductor wafer surface being finished proximate to the finishing surface;
applying an operative finishing motion in the interface between the semiconductor wafer surface being finished; and wherein
applying the operative finishing motion to the operative finishing interface forms an organic lubricating boundary layer having a thickness of at most 4 molecules on at least a portion of the semiconductor surface being finished and:
the operative finishing motion forms a friction in the interface between a uniform region of the semiconductor wafer surface and the finishing element finishing surface;
the organic boundary layer physically or chemically interacts with and adheres to a uniform region of the semiconductor wafer surface;
the friction formed between the uniform region of the semiconductor wafer surface and the finishing element finishing surface is determined by properties other than viscosity.

### Claim 14 (depends on 13)

The method of finishing of the semiconductor wafer surface being finished having uniform regions having the plurality of unwanted raised regions according to claim 13 wherein the finishing element comprises a mixture of a plurality of organic synthetic polymers.

### Claim 15 (depends on 13)

The method of finishing of the semiconductor wafer surface being finished having uniform regions having the plurality of unwanted raised regions according to claim 13 wherein applying the operative finishing motion comprises:
applying a higher pressure to the unwanted raised regions compared to the pressure applied to regions below the unwanted raised regions causing less boundary layer lubrication and a higher temperature on the unwanted raised regions and the boundary layer lubrication to be greater and the temperature to be lower on a portion of the semiconductor wafer surface below the unwanted raised regions.

### Claim 16 (depends on 15)

The method of finishing of the semiconductor wafer surface being finished having uniform regions having the plurality of unwanted raised regions according to claim 15 wherein applying the higher pressure comprises applying at least five times higher pressure to the unwanted raised region when compared to the applied pressure in a lower region proximate to the unwanted raised regions.

### Claim 17 (depends on 15)

The method of finishing of the semiconductor wafer surface being finished having uniform regions having the plurality of unwanted raised regions according to claim 15 wherein the unwanted raised regions have a finishing rate measured in angstroms per minute of at least 4 times faster than in a proximate low local region.

### Claim 18 (depends on 15)

The method of finishing of a semiconductor wafer surface being finished having uniform regions and the plurality of wafer die, each wafer die having the repeating pattern of unwanted raised regions according to claim 15 wherein applying the operative finishing motion causes the unwanted raised regions to have a temperature of at least 7 degrees centigrade higher than that of the proximate low local regions.

### Claim 19 (depends on 15)

The method of finishing of the semiconductor wafer surface being finished having uniform regions having the plurality of unwanted raised regions according to claim 15 wherein the finishing element finishing surface comprises an organic synthetic polymer having a flexural modulus of at least 20,000 psi when measured according to ASTM 790 B at 73 degrees Fahrenheit.

### Claim 20 (depends on 15)

The method of finishing of the semiconductor wafer surface being finished having uniform regions having the plurality of unwanted raised regions according to claim 15 further comprising an additional step of controlling the thickness of the organic lubricating boundary layer by changing at least one process control parameter in situ based on feed back information from a control subsystem.

### Claim 21

A method of finishing of a semiconductor wafer surface being finished comprising the steps of:
providing a finishing element finishing surface;
providing an organic lubricant to an operative finishing interface;
applying an operative finishing motion in the operative finishing interface forming an organic lubricating boundary layer of from 1 to 6 molecules thick; and
controlling at least once the thickness of the organic lubricating boundary layer which changes the coefficient of friction in the operative finishing interface by changing at least one process control parameter in situ based on feed back information from a control subsystem during the finishing cycle time.

### Claim 22 (depends on 21)

A method of finishing of a heterogeneous semiconductor wafer surface being finished according to claim 21 further comprising an additional step of controlling the thickness of the organic lubricating boundary layer by changing at least one lubrication control parameter in a manner that changes the tangential force of friction in at least two different regions in the operative finishing interface in response to an in situ control signal.

### Claim 23 (depends on 21)

A method of finishing of a semiconductor wafer surface being finished according to claim 21 wherein the semiconductor wafer surface being finished has a plurality of unwanted raised regions and further comprising the additional step of applying a higher pressure to the plurality of unwanted raised regions with a finishing element having a flexural modulus of at least 20,000 psi when measured by ASTM 790 B at 73 degrees Fahrenheit as compared to the lower pressure applied to the lower regions proximate to the unwanted raised regions.

### Claim 24 (depends on 21)

The method of finishing of a semiconductor wafer surface being finished according to claim 21 wherein the organic boundary lubricating layer is capable of changing from a solid film to a different physical form in the operative finishing interface temperature range.

### Claim 25 (depends on 21)

A method of finishing of a semiconductor wafer surface being finished according to claim 21 wherein the control subsystem comprises a plurality of friction sensors.

### Claim 26 (depends on 21)

A method of finishing of a semiconductor wafer surface being finished according to claim 21 wherein the control subsystem comprises a plurality of friction sensors and a workpiece sensor.