# US 2001/0027017 A1 · Minimizing metal corrosion during post metal solvent clean

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027017 A1
- Document ID: US20010027017A1
- Status: Published application
- Kind: A1
- Application number: 09/877,661
- Filed: 2001-06-08
- Published: 2001-10-04
- Earliest claimed: 1999-06-15
- Inventors: Anne E. Sanderfer; Jacques Bertrand
- Web page: https://patentgrep.com/patent/US20010027017A1

## CPC

- H10P 70/273: {the processing being a delineation of conductive layers, e.g. by RIE}
- C11D 7/5013: {containing nitrogen}
- C11D 2111/22: Electronic devices, e.g. PCBs or semiconductors
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C11D: DETERGENT COMPOSITIONS; USE OF SINGLE SUBSTANCES AS DETERGENTS; SOAP OR SOAP-MAKING; RESIN SOAPS; RECOVERY OF GLYCEROL

## Abstract

The inventive method provides a wet cleaning of semiconductor devices on semiconductor wafers after photoresist is stripped. Semiconductor wafers are placed into a centrifuge carriage of a processing chamber. The centrifuge carriage rotates the semiconductor wafers. N-methylpyrrolidine heated to a temperature between 65° C. and 85° C. is sprayed onto the semiconductor wafers. Next N-methylpyrrolidine at room temperature is sprayed onto the semiconductor wafers. Finally, water at room temperature is sprayed onto the semiconductor wafers. The inventive method provides high throughput cleaning without undue corrosion or damage to metal layers.

## Claims

### Claim 1

A method of cleaning a semiconductor wafer, comprising the steps of:
placing the semiconductor wafer into a processing chamber;
spraying a first solvent, maintained at a temperature between 50° C. and 100° C., on to the semiconductor wafer;
discontinuing the spraying of the first solvent on to the semiconductor wafer;
spraying a second solvent, at a temperature between 20° C. and 40° C., on to the semiconductor wafer; and
discontinuing the spraying of the second solvent on to the semiconductor wafer.

### Claim 2 (depends on 1)

The method, as recited in claim 1, further comprising the step of:
spraying water, at a temperature between 20° C. and 40° C., on to the semiconductor wafer, wherein the step of spraying water is after the discontinuing of the spraying of the second solvent on the semiconductor wafer.

### Claim 3 (depends on 2)

The method, as recited in claim 2, wherein the first solvent and the second solvent are made of the same chemicals.

### Claim 4 (depends on 3)

The method, as recited in claim 3, further comprising the step of centrifuging the wafer during the steps of spraying the first solvent, spraying the second solvent, and spraying the water.

### Claim 5 (depends on 4)

The method, as recited in claim 4, wherein in the step of spraying the first solvent, the first solvent is at a temperature between 65° C. and 85° C.

### Claim 6 (depends on 5)

The method, as recited in claim 5, wherein in the step of spraying the second solvent, the second solvent is at a temperature between 25° C. and 30° C.

### Claim 7 (depends on 6)

The method, as recited in claim 6, wherein the first solvent and the second solvent are N-methylpyrrolidine.

### Claim 8 (depends on 7)

The method, as recited in claim 7, further comprising the steps of:
applying a layer on the semiconductor wafer, prior to placing the semiconductor wafer into the processing chamber;
placing a resist mask on the layer, prior to placing the semiconductor wafer into the processing chamber;
etching the layer, prior to placing the semiconductor wafer into the processing chamber; and
stripping the resist mask, prior to placing the semiconductor wafer into the processing chamber.

### Claim 9 (depends on 8)

The method, as recited in claim 8, wherein part of the layer is metallic.

### Claim 10 (depends on 8)

The method, as recited in claim 8, further comprising the step of stripping a sidewall polymer residue, prior to placing the semiconductor wafer into the processing chamber.

### Claim 11 (depends on 1)

The method, as recited in claim 1, wherein the first solvent and the second solvent are made of the same chemicals.

### Claim 12 (depends on 11)

The method, as recited in claim 11, wherein in the step of spraying the first solvent, the first solvent is at a temperature between 65° C. and 85° C.

### Claim 13 (depends on 12)

The method, as recited in claim 12, wherein in the step of spraying the second solvent, the second solvent is at a temperature between 25° C. and 30° C.

### Claim 14 (depends on 13)

The method, as recited in claim 13, wherein the first solvent and the second solvent are N-methylpyrrolidine.

### Claim 15

An apparatus for cleaning a semiconductor wafer, comprising:
a processing chamber;
a wafer centrifuge mounted in the processing chamber, with a means for retaining a semiconductor wafer;
a spray nozzle mounted within the processing chamber;
means for providing a first solvent, at a temperature between 50° C. and 100° C., to the spray nozzle;
means for providing a second solvent, at a temperature between 20° C. and 40° C., to the spray nozzle; and
means for providing water, at a temperature between 20° C. and 40° C., to the spray nozzle.