- Number: US 2001/0027012 A1
- Document ID: US20010027012A1
- Status: Published application
- Kind: A1
- Application number: 09/811,798
- Filed: 2001-03-19
- Published: 2001-10-04
- Earliest claimed: 2000-03-17
- Assignees: Infineon Technologies AG
- Inventors: Sven Schmidbauer; Norbert Urbansky
- Web page: https://patentgrep.com/patent/US20010027012A1

## CPC

- H10W 20/047: {by introducing additional elements therein}
- H10W 20/033: {in openings in dielectrics}
- Y10S 438/909: Controlled atmosphere
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A contact layer is used, for example, as a liner for the fabrication of electrical contacts in contact holes. The contact layer is fabricated in two steps, in a first step a first contact layer is deposited, in which only a small proportion of the particles to be sputtered is ionized. In a second sputtering step, a second contact layer is sputtered, in the course of whose fabrication a larger proportion of the particles to be sputtered is ionized. The procedure ensures that the first contact layer is disposed as a protective layer on the substrate by gentle sputtering before the second contact layer is sputtered.

## Claims

### Claim 1

A method for fabricating a contact layer, which comprises the steps of:
providing a substrate in a sputtering chamber;
disposing a dielectric layer on the substrate;
forming a trench in the dielectric layer;
producing a plasma in the sputtering chamber;
sputtering a first contact layer in the trench in a first step, in the sputtering chamber a number of ionized particles in relation to a total number of particles during the first step being less than 5%; and
sputtering a second contact layer onto the first contact layer in a second step, in the sputtering chamber the number of ionized particles in relation to the total number of particles during the second step being greater than 5%.

### Claim 2 (depends on 1)

The method according to claim 1, which comprises during the second step, an alternating magnetic field is present in the sputtering chamber.

### Claim 3 (depends on 1)

The method according to claim 1, which comprises setting a pressure in the sputtering chamber to be lower during the first step than during the second step.

### Claim 4 (depends on 3)

The method according to claim 3, which comprises setting the pressure in the sputtering chamber to be 2 to 50 times lower in the first step than in the second step.

### Claim 5 (depends on 1)

The method according to claim 1, which comprises:
disposing the substrate on a first side of a support;
disposing an electrode on a second side of the support; and
applying an alternating voltage to the electrode during the second step.

### Claim 6 (depends on 1)

The method according to claim 1, which comprises during the first step, setting the number of ionized particles in relation to the total number of particles to be less than 2% in the sputtering chamber.

### Claim 7 (depends on 1)

The method according to claim 1, which comprises during the second step setting the number of ionized particles in relation to the total number of particles to be greater than 40% in the sputtering chamber.

### Claim 8 (depends on 1)

The method according to claim 1, which comprises forming the first contact layer and the second contact layer with a substantially conformal layer thickness.

### Claim 9 (depends on 1)

The method according to claim 1, which comprises forming the first contact layer and the second contact layer with a same chemical element.

### Claim 10 (depends on 1)

The method according to claim 1, which comprises setting a kinetic energy of the particles to be sputtered to be lower in the first step than in the second step.

### Claim 11 (depends on 1)

The method according to claim 1, which comprises setting a kinetic energy of the particles to be sputtered to be less than 10 eV in the first step.

### Claim 12 (depends on 1)

The method according to claim 1, which comprises setting a kinetic energy of the particles to be sputtered to be greater than 100 eV in the second step.