# US 2001/0027002 A1 · Method for forming multi-layered interconnect structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0027002 A1
- Document ID: US20010027002A1
- Status: Published application
- Kind: A1
- Application number: 09/784,267
- Filed: 2001-02-15
- Published: 2001-10-04
- Earliest claimed: 2000-02-15
- Assignees: NEC Corporation
- Inventors: Akira Matsumoto
- Web page: https://patentgrep.com/patent/US20010027002A1

## CPC

- H10W 20/085: {involving intermediate temporary filling with material}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a multi-layered interconnect structure including an underlying interconnect, an overlying interconnect and a conductive via-plug for connecting the both interconnects, wherein a through-hole is filled with a protective film plug, and during the etching of the protective film and the protective film plug, a top surface of the protective film plug in the through-hole is placed lower than a top surface of the second dielectric film. In accordance with the present invention, the multi-layered interconnect structure having a smaller connection resistance and smaller dimensions can be obtained.

## Claims

### Claim 1

A method for forming a multi-layered interconnect structure comprising the steps of:
depositing an underlying interconnect overlying a substrate;
consecutively depositing a first dielectric film, an etch stop layer and a second dielectric film on the underlying interconnect;
forming a through-hole penetrating the first dielectric film, the etch stop layer and the second dielectric film to expose a portion of the underlying interconnect;
depositing a protective film on the second dielectric film and a protective film plug in the through-hole;
etching the protective film and the protective film plug by using the etching mask in an etching condition that the protective film has a larger etching rate compared to the second dielectric film, until the protective film plug has a top surface lower than a top surface of the second dielectric film;
etching the second dielectric film and the protective film by using the etching mask in an etching condition that the second dielectric film has an etching rate not lower than an etching rate of the protective film plug, to form an interconnect trench in the second dielectric film while leaving a portion of the protective film plug;
removing the etching mask, the protective film and the protective film plug;
depositing an overlying interconnect in the interconnect trench and the through-hole to form the overlying interconnect connected to the underlying interconnect via the through-hole.

### Claim 2 (depends on 1)

The method as defined in claim 1, wherein the protective film plug in the through-hole is etched in the first protective film etching step such that the top surface of the protective film plug in the through-hole is placed between the top surface of the second dielectric film and the etch stop layer.

### Claim 3 (depends on 1)

The method as defined in claim 1, wherein the protective film plug in the through-hole is etched in the first protective film etching step such that the top surface of the protective film plug in the through-hole is placed lower than the top surface of the second dielectric film by a distance between ½ and ⅓ of the depth of the interconnect trench of the overlying interconnect.

### Claim 4 (depends on 1)

The method as defined in claim 1, wherein, when an inorganic dielectric film is used as the second dielectric film, an organic film is used as the protective film and the protective film plug; an anisotropic dry etching is conducted by using mixed gas including fluorocarbon-based gas, oxygen gas and inert gas in the first protective film etching step; and an anisotropic dry etching is conducted by using mixed gas including fluorocarbon-based gas and inert gas and including no oxygen gas in the second protective film etching step.

### Claim 5 (depends on 1)

The method as defined in claim 1, wherein, when an organic dielectric film is used as the second dielectric film, an inorganic film is used as the protective film and the protective film plug; an anisotropic dry etching is conducted by using mixed gas including fluorocarbon-based gas and inert gas and including no oxygen gas in the first protective film etching step; and an anisotropic dry etching is conducted by using mixed gas including fluorocarbon-based gas, oxygen gas and inert gas in the second protective film etching step.

### Claim 6 (depends on 4)

The method as defined in claim 4, wherein the organic film is formed by a material substantially same as that for a reflection preventing film used for the exposure.

### Claim 7 (depends on 1)

The method as defined in claim 1, wherein a SiN film is formed, as a metal-diffusion preventing film, on the underlying interconnect formed by a metal or alloy of which a main component is copper and then the first dielectric film is formed.

### Claim 8 (depends on 1)

The method as defined in claim 1, wherein a SiON film is formed as the etch stop layer for the second dielectric film formed by a SiO2 film.

### Claim 9 (depends on 1)

The method as defined in claim 1, wherein the underlying interconnect is an impurity-diffused layer.

### Claim 10 (depends on 1)

A multi-layered interconnect structure for a semiconductor device fabricated in accordance with the method as defined in claim 1.

### Claim 11 (depends on 9)

A multi-layered interconnect structure for a semiconductor device fabricated in accordance with the method as defined in claim 9.
