# US 2001/0026979 A1 · Method of performing threshold voltage adjustment for MOS transistors

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0026979 A1
- Document ID: US20010026979A1
- Status: Published application
- Kind: A1
- Application number: 09/537,175
- Filed: 2000-03-29
- Published: 2001-10-04
- Earliest claimed: 2000-03-29
- Assignees: Vanguard International Semiconductor Corporation
- Inventors: Yuh-Sheng Chern
- Web page: https://patentgrep.com/patent/US20010026979A1

## CPC

- H10P 30/204: {into Group IV semiconductors}
- H10D 62/299: {having lateral doping variations (IGFETs having lightly doped source or drain extensions H10D30/601)}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 30/212: {Through-implantation}
- H10P 30/225: {of a molecular ion, e.g. decaborane}
- H10W 10/0148: {comprising introducing impurities in side walls or bottom walls of trenches, e.g. for forming channel stoppers}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The invention discloses a method of forming threshold voltage adjustment for MOS transistors. At first, a first oxide layer and a nitride layer are formed on a silicon substrate in sequence. Next, shallow trenches and active regions are formed by using photolithography and dry etching technology. A wet etching step is performed to remove part of the nitride layer, and then the first ion implantation for threshold voltage adjustment are performed. After accomplishing shallow trench isolations, the second ion implantation for threshold voltage adjustment are finally performed.

## Claims

### Claim 1

A method of performing threshold voltage adjustment for MOS transistors, wherein said threshold voltage adjustment is performed by means of P-type ion implantation, comprising the steps of:
a. forming a first oxide layer and a layer of hard mask on a silicon substrate;
b. forming shallow trenches and active regions by using photolithography and anisotropic etching steps;
c. removing part of said layer of hard mask by using wet etching;
d. performing a first ion implantation for threshold voltage adjustment by using P-type semiconductor;
e. completing shallow trench isolations; and
f. performing a second ion implantation for threshold voltage adjustment by using P-type semiconductor.

### Claim 2 (depends on 1)

The method of claim 1, wherein said first oxide layer has a thickness in the range between 50 to 500 Angstroms.

### Claim 3 (depends on 1)

The method of claim 1, wherein said hard mask is a nitride layer.

### Claim 4 (depends on 1)

The method of claim 1, wherein said hard mask is an oxynitride layer.

### Claim 5 (depends on 1)

The method of claim 1, wherein said hard mask has a thickness in the range between 500 to 3000 Angstroms.

### Claim 6 (depends on 1)

The method of claim 1, further including a thermal oxidation process after the step of forming shallow trenches.

### Claim 7 (depends on 1)

The method of claim 1, wherein said wet etching step is to remove said layer of hard mask in the range between 30 to 300 Angstroms.

### Claim 8 (depends on 1)

The method of claim 1, wherein said first ion implantation for threshold voltage adjustment is performed at an energy between 10 to 80 KeV and at a dose between 1E12 to 1E14 cm−2.

### Claim 9 (depends on 1)

The method of claim 1, wherein said step of completing shallow trench isolations comprising the steps of:
a. depositing a second oxide layer to fill said shallow trenches;
b. performing a chemical mechanical polishing step to remove a part of said second oxide layer on said layer of hard mask;
c. removing said layer of hard mask, a part of said second oxide layer on said silicon substrate, and said first oxide layer continuously.

### Claim 10 (depends on 1)

The apparatus of claim 1, wherein said second ion implantation for threshold voltage adjustment is performed at an energy between 10 to 80 KeV and at a dose between 1E12 to 1E14 cm−2.

### Claim 11

A method of performing threshold voltage adjustment for MOS transistors, wherein said threshold voltage adjustment is performed by means of N-type ion implantation, comprising the steps of:
a. forming a first oxide layer and a layer of hard mask on a silicon substrate;
b. forming shallow trenches and active regions by using photolithography and anisotropic etching steps;
c. removing part of said layer of hard mask by using wet etching;
d. performing a first ion implantation for threshold voltage adjustment by using N-type semiconductor;
e. completing shallow trench isolations; and
f. performing a second ion implantation for threshold voltage adjustment by using N-type semiconductor.

### Claim 12 (depends on 11)

The method of claim 11, wherein said first oxide layer has a thickness in the range between 50 to 500 Angstroms.

### Claim 13 (depends on 11)

The method of claim 11, wherein said hard mask is a nitride layer.

### Claim 14 (depends on 11)

The method of claim 11, wherein said hard mask is an oxynitride layer.

### Claim 15 (depends on 11)

The method of claim 11, wherein said hard mask has a thickness in the range between 500 to 3000 Angstroms.

### Claim 16 (depends on 11)

The method of claim 11, further including a thermal oxidation process after the step of forming shallow trenches.

### Claim 17 (depends on 11)

The method of claim 11, wherein said wet etching step is to remove said layer of hard mask in the range between 30 to 300 Angstroms.

### Claim 18 (depends on 11)

The method of claim 11, wherein said first ion implantation for threshold voltage adjustment is performed at an energy between 10 to 80 KeV and at a dose between 1E12 to 1E14 cm−2.

### Claim 19 (depends on 11)

The method of claim 11, wherein said step of completing shallow trench isolations comprising the steps of:
a. depositing a second oxide layer to fill said shallow trenches;
b. performing a chemical mechanical polishing step to remove a part of said second oxide layer on said layer of hard mask;
c. removing said layer of hard mask, a part of said second oxide layer on said silicon substrate, and said first oxide layer continuously.

### Claim 20 (depends on 11)

The apparatus of claim 11, wherein said second ion implantation for threshold voltage adjustment is performed at an energy between 10 to 80 KeV and at a dose between 1E12 to 1E14 cm−2.