# US 2001/0026976 A1 · Method of fabricating a semiconductor device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0026976 A1
- Document ID: US20010026976A1
- Status: Published application
- Kind: A1
- Application number: 09/818,773
- Filed: 2001-03-28
- Published: 2001-10-04
- Earliest claimed: 2000-03-28
- Inventors: Yuong-Ho Yang
- Web page: https://patentgrep.com/patent/US20010026976A1

## CPC

- H10D 1/711: {having non-planar surfaces, e.g. formed by texturisation}
- H10B 12/315: {with the capacitor higher than a bit line}
- H10D 1/712: {being rough surfaces, e.g. using hemispherical grains}
- H10D 1/716: {having vertical extensions}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A capacitor for a semiconductor device including a lower electrode having a silicon layer with portions initially doped at different doping densities, a plurality of protrusions formed selectively on the lower electrode according to the different doping densities, a dielectric layer over the lower electrode and the protrusions, and an upper electrode over the dielectric layer. After the protrusions are formed, a step of additionally doping the lower electrode to increase the doping density thereof is not required. The silicon layer with portions initially doped at different doping densities allows the protrusions to form more easily, so that the entire surface area of the lower electrode is increased to thus minimize variations in capacitance.

## Claims

### Claim 1

A method of fabricating a semiconductor device comprising:
forming on a substrate a first amorphous silicon layer doped with impurity ions at a first impurity density;
forming on the first amorphous silicon layer a second amorphous silicon layer doped with impurity ions at a second impurity density higher than the first impurity density;
forming on the second amorphous silicon layer a third amorphous silicon layer doped with impurity ions at a third impurity density lower than the first impurity density;
forming a predetermined pattern by patterning the first to third amorphous silicon layers;
forming hemispherical silicon grains on an exposed surface of the predetermined pattern; and
diffusing the impurity ions among the hemispherical silicon grains and the predetermined pattern so that a density of the impurity ions is uniform in the hemispherical silicon grains and the predetermined pattern.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the first to third amorphous silicon layers and the hemispherical silicon grains are doped with negative impurity ions.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the impurity ions are phosphorus ions.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the first impurity density of the phosphorus ions lies between 1.0E20 and 1.0E21 atoms/cm3, the second impurity density of the phosphorus ions is over 1.0E21 atoms/cm3, and the third impurity density of the phosphorus ions lies between 0.0 and 1.0E20 atoms/cm3.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the step of diffusing the impurity ions further comprises:
depositing a silicon nitride layer on surfaces of the hemispherical silicon grains and the predetermined pattern at a first temperature; and
oxidizing the silicon nitride layer at a second temperature.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the step of diffusing the impurity ions is achieved by carrying out annealing on the hemispherical silicon grains and the predetermined pattern.

### Claim 7 (depends on 5)

The method according to claim 5, wherein after the step of oxidizing the silicon nitride layer, the method further comprises:
forming a conductive layer on the silicon nitride layer wherein the predetermined pattern and the hemispherical silicon grains, the silicon nitride layer, and the conductive layer respectively become a lower electrode, a dielectric layer, and an upper electrode of a capacitor.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the conductive layer is formed of doped polysilicon.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the hemispherical silicon grains are formed by flowing SiH4 gases on the exposed surface of the predetermined pattern.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the first to third amorphous silicon layers are formed of in-situ doped amorphous silicon at the first to third impurity densities, respectively.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the first to third amorphous silicon layers are formed by depositing undoped amorphous silicon and then by doping the undoped amorphous silicon at the first to third impurity densities, respectively.

### Claim 12

A method of fabricating a semiconductor device comprising:
forming an insulating layer on a semiconductor substrate having a contact hole exposing a portion of the substrate;
forming on the insulating layer a first conductive layer contacting a predetermined portion of the semiconductor substrate;
forming on the first conductive layer a first amorphous silicon layer doped with impurity ions at a first impurity density;
forming on the first amorphous silicon layer a second amorphous silicon layer doped with the impurity ions at a second impurity density higher than the first impurity density;
forming on the second amorphous silicon layer a third amorphous silicon layer doped with the impurity ions at a third impurity density lower than the first impurity density;
forming a lower electrode by patterning the first to third amorphous silicon layers and the first conductive layer, wherein the lower electrode comprises the the first to third amorphous silicon layers and the first conductive layer;
forming hemispherical silicon grains on an exposed surface of the lower electrode;
forming a dielectric layer on exposed surfaces of the lower electrode and the hemispherical silicon grains; and
forming on the dielectric layer an upper electrode using a second conductive layer.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the first to third amorphous silicon layers and the hemispherical silicon grains are doped with negative impurity ions.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the impurity ions are phosphorus ions.

### Claim 15 (depends on 14)

The method according to claim 14, wherein the first impurity density of the phosphorus ions lies between 1.0E20 and 1.0E21 atoms/cm3 the second impurity density of the phosphorus ions is over 1.0E21 atoms/cm3, and the third impurity density of the phosphorus ions lies between 0.0 and 1.0E20 atoms/cm3.

### Claim 16 (depends on 12)

The method according to claim 12, wherein the step of forming a dielectric layer further comprises:
depositing a silicon nitride layer on surfaces of the hemispherical silicon grains and the lower electrode at a first temperature; and
oxidizing the silicon nitride layer at a second temperature at which the impurity ions diffuse naturally.

### Claim 17 (depends on 12)

The method according to claim 12, further comprising the step of carrying out annealing on the hemispherical silicon grains and the lower electrode to diffuse the impurity ions therebetween.

### Claim 18 (depends on 12)

The method according to claim 12, wherein the second conductive layer is formed of doped polysilicon.

### Claim 19 (depends on 12)

The method according to claim 12, wherein the hemispherical silicon grains are formed by flowing SiH4 gases on the exposed surface of the lower electrode.

### Claim 20 (depends on 12)

The method according to claim 12, wherein the first to third amorphous silicon layers are formed of in-situ doped amorphous silicon at the first to third impurity densities, respectively.

### Claim 21 (depends on 12)

The method according to claim 12, wherein the first to third amorphous silicon layers are formed by depositing undoped amorphous silicon and then by doping the undoped amorphous silicon at the first to third impurity densities, respectively.

### Claim 22

A method of fabricating a semiconductor device comprising:
forming an insulating layer on a semiconductor substrate having a contact hole exposing a portion of the substrate;
forming on the insulating layer a first conductive layer contacting a predetermined portion of the semiconductor substrate;
patterning the first conductive layer so that the first conductive layer remains in the contact hole and extends on a top surface portion of the insulating layer;
forming a pillar at a side of the remaining first conductive layers wherein the pillar is constructed using a first amorphous silicon layer doped with impurity ions at a first impurity density, a second amorphous silicon layer doped with impurity ions at a second impurity density higher than the first impurity density, and a third amorphous silicon layer doped with impurity ions at a third impurity density lower than the first impurity density, and wherein the first to third amorphous silicon layers are stacked successively;
forming hemispherical silicon grains on exposed surfaces of the remaining first conductive layer and the pillar;
forming a dielectric layer on exposed surfaces of the pillar and the hemispherical silicon grains; and
forming on the dielectric layer an upper electrode using a second conductive layer.

### Claim 23 (depends on 22)

The method according to claim 22, the step of forming the pillar further comprises:
forming a sacrificing layer on the first conductive layer using a substance having an etch rate that differs from that of the insulating layer;
patterning the sacrificing layer and the first conductive layer to remain in the contact hole and extends on a top surface portion of the insulating layer;
forming a first amorphous silicon layer doped with impurity ions at a first impurity density on the insulating layer including the remaining sacrificing layer and a first conductive layer pattern of the remaining first conductive layer;
forming on the first amorphous silicon layer a second amorphous silicon layer doped with impurity ions at a second impurity density higher than the first impurity density;
forming on the second amorphous silicon layer a third amorphous silicon layer doped with impurity ions at a third impurity density lower than the first impurity density;
patterning the first to third amorphous silicon layers to remain at sides of the remaining sacrificing layer and the first conductive layer pattern; and
removing the remaining sacrificing layer.

### Claim 24 (depends on 22)

The method according to claim 22, wherein a lower electrode being a storage electrode of a capacitor is constructed with the remaining first conductive layer, the pillar, and the hemispherical silicon grains.

### Claim 25 (depends on 22)

The method according to claim 22, wherein the first to third amorphous silicon layers and the hemispherical silicon grains are doped with negative impurity ions enabling to provide electric conductivity thereto.

### Claim 26 (depends on 22)

The method according to claim 22, wherein the impurity ions are phosphorus ions.

### Claim 27 (depends on 26)

The method according to claim 26, wherein the first impurity density of the phosphorus ions lies between 1.0E20 and 1.0E21 atoms/cm3, the second impurity density of the phosphorus ions is over 1.0E21 atoms/cm3, and the third impurity density of the phosphorus ions lies between 0.0 and 1.0E20 atoms/cm3.

### Claim 28 (depends on 22)

The method according to claim 22, the step of forming a dielectric layer further comprises:
depositing a silicon nitride layer on surfaces of the hemispherical silicon grains and the pillar at a first temperature; and
oxidizing the silicon nitride layer at a second temperature at which the impurity ions diffuse naturally.

### Claim 29 (depends on 22)

The method according to claim 22, the method further comprising the step of carrying out annealing on the hemispherical silicon grains and the pillar to diffuse the impurity ions therebetween.

### Claim 30 (depends on 22)

The method according to claim 22, wherein the second conductive layer is formed of doped polysilicon.

### Claim 31 (depends on 22)

The method according to claim 22, wherein the hemispherical silicon grains are formed by flowing SiH4 gases on the exposed surfaces of the first conductive layer and the pillar.

### Claim 32 (depends on 22)

The method according to claim 22, wherein the first to third amorphous silicon layers are formed of in-situ doped amorphous silicon at the first to third impurity densities, respectively.

### Claim 33 (depends on 22)

The method according to claim 22, wherein the first to third amorphous silicon layers are formed by depositing undoped amorphous silicon and then by doping the undoped amorphous silicon at the first to third impurity densities, respectively.

### Claim 34

A method of forming a capacitor for a semiconductor device comprising:
forming a lower electrode having a silicon layer with portions initially doped at different doping densities;
forming a plurality of protrusions selectively on the lower electrode according to the different doping densities;
forming a dielectric layer over the lower electrode and the protrusions; and
forming an upper electrode over the dielectric layer.

### Claim 35 (depends on 34)

The method of claim 34, wherein the silicon layer is formed to have at least two different portions, each initially having a different doping density.

### Claim 36 (depends on 34)

The method of claim 34, wherein forming the lower electrode having the silicon layer further comprises:
forming a first layer at a first doping density;
forming a second layer on the first layer at a second doping density; and
forming a third layer on the second layer at a third doping density.

### Claim 37 (depends on 36)

The method of claim 36, wherein the second doping density is greater than the first doping density.

### Claim 38 (depends on 36)

The method of claim 36, wherein the second doping density is greater than the third doping density.

### Claim 39 (depends on 36)

The method of claim 36, wherein the third doping density is less than the first doping density.

### Claim 40 (depends on 36)

The method of claim 36, wherein the third doping density is the same as the first doping density.

### Claim 41 (depends on 34)

The method of claim 34, wherein the protrusions are formed by growing silicon particles on the lower electrode.

### Claim 42 (depends on 41)

The method of claim 41, wherein the protrusions are formed on the lower electrode at portions having relatively low doping densities.

### Claim 43 (depends on 34)

The method of claim 34, wherein the forming of the dielectric layer diffuses impurity ions in the silicon layer.

### Claim 44

The method of clam 34, wherein a step of additionally doping the lower electrode after the protrusions are formed is not required.

### Claim 45

A capacitor for a semiconductor device formed by a process comprising:
forming a lower electrode having a silicon layer with portions initially doped at different doping densities;
forming a plurality of protrusions selectively on the lower electrode according to the different doping densities;
forming a dielectric layer over the lower electrode and the protrusions; and
forming an upper electrode over the dielectric layer.

### Claim 46 (depends on 45)

The capacitor of claim 45, wherein the silicon layer has at least two portions, each initially having a different doping density.