# US 2001/0026948 A1 · Method for appraising the condition of a semiconductor polishing cloth

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0026948 A1
- Document ID: US20010026948A1
- Status: Published application
- Kind: A1
- Application number: 09/266,051
- Filed: 1999-03-10
- Published: 2001-10-04
- Earliest claimed: 1998-03-10
- Assignees: Komatsu Electronic Metals Co., Ltd.
- Inventors: YUICHI NAKAYOSHI; NAOKI YAMADA
- Web page: https://patentgrep.com/patent/US20010026948A1

## CPC

- B24B 37/24: characterised by the composition or properties of the pad materials
- B24B 49/12: involving optical means
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS

## Abstract

The present invention provides a method for appraising the condition of a polishing cloth, and a method for manufacturing semiconductor wafers employing the disclosed appraisal method, allowing acceptably low light point defect numbers of semiconductor wafers to be maintained. The disclosed method comprises polishing the semiconductor wafer using a polishing cloth, washing the wafer, and drying the wafer. The size of particles comprising light point defects is chosen, and the number of light point defects on the semiconductor wafer is counted. Typically, the diameter of particles comprising light point defects is set as 0.12 μm or greater. The polishing cloth is exchanged when the number of light point defects counted exceeds a prescribed number.

## Claims

### Claim 1

A method for appraising the condition of a polishing cloth used to polish semiconductor wafers, comprising:
selecting a diameter of particle defining a light point defect;
selecting a number of light point defects;
polishing a semiconductor wafer with said polishing cloth;
counting the number of light point defects on said semiconductor wafer; and
replacing said polishing cloth if said counted number of light point defects is greater than said selected number of light point defects.

### Claim 2 (depends on 1)

The method of claim 1, wherein said selected diameter of particle defining a light point defect is greater than about 0.12 μm.

### Claim 3 (depends on 1)

The method of claim 1, wherein said selected diameter of particle defining a light point defect is greater than a certain diameter, and said certain diameter is about 0.12 μm.

### Claim 4 (depends on 1)

The method of claim 1, wherein said selected diameter of particle defining a light point defect is greater than a certain diameter, and said certain diameter is about 0.16 μm.

### Claim 5

A method for appraising the condition of a polishing cloth used to polish semiconductor wafers, comprising:
selecting a diameter of particle defining a light point defect;
selecting a number of light point defects;
polishing a semiconductor wafer with said polishing cloth;
washing said semiconductor wafer;
drying said semiconductor wafer;
counting the number of light point defects of said selected diameter on said semiconductor wafer; and
replacing said polishing cloth if said counted number of light point defects is greater than said selected number of light point defects.

### Claim 6 (depends on 5)

The method of claim 5, wherein particles defining light point defects have a diameter greater than about 0.12 μm.

### Claim 7 (depends on 5)

The method of claim 5, wherein particles defining light point defects have a diameter greater than a certain diameter, and said certain diameter is about 0.12 μm.

### Claim 8 (depends on 5)

The method of claim 5, wherein particles defining light point defects have a diameter greater than a certain diameter, and said certain diameter is about 0.16 μm.

### Claim 9

A method for manufacturing semiconductor wafers that are polished using a polishing cloth, comprising:
selecting a diameter of particle defining a light point defect;
selecting a number of light point defects;
polishing a semiconductor wafer with a polishing cloth;
washing said semiconductor wafer;
drying said semiconductor wafer;
counting the number of light point defects of said selected diameter on said semiconductor wafer; and
replacing said polishing cloth if said counted number of light point defects is greater than said selected number of light point defects before polishing a next semiconductor wafer.

### Claim 10 (depends on 9)

The method of claim 9, wherein said selected diameter of particle defining a light point defect is greater than about 0.12 μm.

### Claim 11 (depends on 9)

The method of claim 9, wherein said selected diameter of particle defining a light point defect is greater than a certain diameter, and said certain diameter is about 0.16 μm.

### Claim 12 (depends on 9)