# US 2001/0026841 A1 · Method for pressure treating wood

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0026841 A1
- Document ID: US20010026841A1
- Status: Published application
- Kind: A1
- Application number: 09/862,008
- Filed: 2001-05-21
- Published: 2001-10-04
- Earliest claimed: 1998-06-17
- Assignees: Coating Development Group, Inc.
- Inventors: Michael A. Barnisin, JR.
- Web page: https://patentgrep.com/patent/US20010026841A1

## CPC

- B27K 3/0214: {Drying (drying in general F26B)}
- B05D 7/06: to wood
- B27K 3/08: Impregnating by pressure {, e.g. vacuum impregnation}
- B27K 3/34: Organic impregnating agents {(polymers B27K3/15)}
- B27K 3/36: Aliphatic compounds
- B27K 3/48: Mineral oil
- B05D 3/12: by mechanical means
- B27K 5/001: {Heating}
- B27K: PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR (applying liquids or other fluent materials to surfaces in general B05; coating wood or similar material B44D); CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

The present invention is a process for pressure treating wood and includes wood which has been pressure treated by the process. The process comprises infusion into the wood of a solution in water of an anhydride or the analogous acid of an anhydride, followed by removal of moisture from the wood and the infusion of the wood with a molten waxy solid comprising hydrocarbon paraffins or saturated fatty acids. The molten waxy solid then solidifies, filling all voids in the wood.

## Claims

### Claim 1

A process for treating wood comprising the steps of:
(a) drying the wood to a moisture content below ten percent (10%);
(b) evacuating the air from the wood;
(c) infusing a solution of anhydride and water into the wood;
(d) drying the wood to a moisture content below eight percent (8%);
(e) evacuating the air from the wood again while the wood istill at a high temperature from the step of drying below eight percent (8%) moisture;
(f) infusing a molten waxy solid including an acid neutralizer into the wood;
and
(g) cooling the wood to room temperature.

### Claim 2 (depends on 1)

The process of claim 1 wherein the waxy solid is selected from the group consisting of parafinnic hydrocarbons, saturated fatty acids or a mixture of parafinnic hydrocarbons and saturated fatty acids.

### Claim 3 (depends on 1)

The process of claim 1 wherein the wood is infused with a waxy solid at an temperature higher than the melting temperature of the waxy solid to facilitate the penetration of the waxy solid into the wood.

### Claim 4 (depends on 1)

The process of claim 1 wherein the infusion of the waxy solid includes the infusion of a solution of waxy solid with an active ingredient.

### Claim 5 (depends on 4)

The process of claim 4 wherein the active ingredient is selected from the group consisting of fungicides, mildewicides, bactericides, flame retardants, colorants or water repellants.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The process of claims 1, 2, 3, 4 or 5 where said acid neutralizer is an amine.

### Claim 7 (depends on 1, 2, 3, 4, 5)

The process of claims 1,2, 3, 4 or 5 where said acid neutralizer is 2-Amine-2-Methyl-1-Propanol.