# US 2001/0026775 A1 · Optochemical sensor and corresponding production method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0026775 A1
- Document ID: US20010026775A1
- Status: Published application
- Kind: A1
- Application number: 09/802,971
- Filed: 2001-03-12
- Published: 2001-10-04
- Earliest claimed: 1998-09-15
- Assignees: Joanneum Research Forschungagesellschaft mbH
- Inventors: Karin Biebernik; Franz Reininger; Wolfgang Trettnak
- Web page: https://patentgrep.com/patent/US20010026775A1

## CPC

- G01N 21/6428: {Measuring fluorescence of fluorescent products of reactions or of fluorochrome labelled reactive substances, e.g. measuring quenching effects, using measuring "optrodes" (in vivo A61B5/00; immunoassay G01N33/53)}
- G01N 31/224: {for investigating presence of dangerous gases}
- G01N 31/225: {for oxygen, e.g. including dissolved oxygen}
- G01N 2021/7786: {Fluorescence}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

The invention relates to an optochemical sensor consisting of a polymer matrix and a luminescent colorant material contained therein, whose emission power may be modified by the substances to be detected after being excited with electro-magnetic radiation. The polymer matrix is formed by at least one polymer, wherein no plasticizers have been added, which polymer contains phenyl groups in the main chain and may also be sterilized. the invention also relates to a method for producing the disclosed optochemical sensor, wherein a solution of a polymer is prepared, wherein 0,01 to 100 mMol luminescent colorant material per polymer is added to said solution and the mixture is solidified to obtain a homogenous membrane.

## Claims

### Claim 1

An optochemical sensor comprised of a polymer matrix and a luminescent dye incorporated therein, whose emission capacity is variable upon excitation with an electromagnetic radiation, in particular light, by detectable substances such as gaseous or dissolved O2, SO2, H2O2, Cl2, nitrogen oxides, halogenated hydrocarbons, wherein the polymer matrix is formed of at least one polymer without addition of plasticizers, which polymer contains phenyl groups in its main chain, wherein the polymer is selected from polysulfones, polyether sulfones, polyether imides and/or polyoxyphenylenes and that the polymer has a glass transition temperature of above 140° C.

### Claim 2 (depends on 1)

An optochemical sensor according to claim 1, wherein the amount of luminescent dye incorporated in the polymer is 0.01 to 100 mMol dye per kg polymer, in particular 0.1 to 20 mMol dye per kg polymer.

### Claim 3 (depends on 1)

An optochemical sensor according to claim 1, wherein the luminescent dye incorporated in the polymer matrix is a dye that is stable up to at least 150° C. and selected from the group consisting of the inorganic salts of transition metal complexes having α-diimine ligands, such as tris(4,7-diphenyl-1,10-phenanthroline) ruthenium(II) salts, tris(1,10-phenanthroline) ruthenium(II) salts and tris-2,2′-bipyridyl ruthenium(I) salts; or of terpyridine, such as osmium terpyridine; the transition metal complexes of porohyrines or porphyrine derivatives, such as complexes of the tetraphenylporphyrine of Pt or Pd, of the octaethylporphyrine ketone of Pt or Pd, of the tetrapentafluorophenylporphyrine of Pt or Pd, or of the octaethylporphyrine of Pt or Pd; of polycyclic aromatic hydrocarbons, such as decacyclene, pyrene or its derivatives; or campherchinone.

### Claim 4 (depends on 1)

An optochemical sensor according to claim 1, wherein the optochemical sensor is applied on a substrate.

### Claim 5 (depends on 4)

An optochemical sensor according to claim 4, wherein optically inactive light-permeable polymers that are insoluble and resistant in organic solvents, acids, bases and water, such as polyesters like PET, polymethylmethacrylate or glass, are used as said substrate.

### Claim 6 (depends on 1)

An optochemical sensor according to claim 1, wherein the optochemical sensor is covered by an optically insulating or protecting layer permeable to the substance to be analyzed.

### Claim 7 (depends on 6)

An optochemical sensor according to claim 6, wherein the optically insulating layer is comprised of, in particular, coarsely porous polytetrafluoroethylene, copolymers consisting of 2,2-bis-trifluoromethyl-4,5-difluoro-1,3-dioxclene and tetrafluoroethylene, or silicone.

### Claim 8

A method for producing an optochemical sensor whose emission capacity is variable upon excitation with an electromagnetic radiation, in particular light, by detectable substances such as gaseous or dissolved O2, SO2, H2O2, wherein an at least 1 to 25 wt.-% solution of a polymer containing phenyl groups in its main chain is prepared in an organic solvent and the mixture is cured to form a homogenous membrane, wherein 0.01 to 100 mMol luminescent dye per kg polymer are added to the solution and the optochemical sensor is subsequently dried in a furnace at 100 to 150° C. for 30 minutes to 24 hours for its completion.

### Claim 9 (depends on 8)

A method according to claim 8, wherein organic solvents such as toluene, chloroform and/or methylene chloride or a mixture thereof are used.

### Claim 10 (depends on 8, 9)

A method according to claim 8 or 9, wherein the sensor is sterilized at a temperature of between 100° C. and 150° C. and a pressure of between 1.2 bar and 4 bars for 20 to 90 minutes.

### Claim 11 (depends on 10)

A method according to claim 10, wherein sterilization is carried out using hot vapor, H2O2, ethanol or β- or γ-rays.

### Claim 12 (depends on 8)

A method according to claim 8, wherein the sensor is purified by immersion into an about 1 N acid or lye, in particular, phosphoric acid, NaCH, KOH, for 10 to 40 minutes at temperatures of between 20 and 90° C.