# US 2001/0026769 A1 · Nickel-based single crystal alloy and a method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0026769 A1
- Document ID: US20010026769A1
- Status: Published application
- Kind: A1
- Application number: 09/874,970
- Filed: 2001-06-07
- Published: 2001-10-04
- Earliest claimed: 1997-10-31
- Inventors: Toshiharu Kobayashi; Yutaka Koizumi; Shizuo Nakazawa; Hiroshi Harada; Toshihiro Yamagata
- Web page: https://patentgrep.com/patent/US20010026769A1

## CPC

- C22F 1/10: of nickel or cobalt or alloys based thereon
- C22C 19/057: {with the maximum Cr content being less 10%}
- C30B 11/00: Single-crystal growth by normal freezing or freezing under temperature gradient, e.g. Bridgman-Stockbarger method (C30B13/00, C30B15/00, C30B17/00, C30B19/00 take precedence; under a protective fluid C30B27/00)
- C30B 29/52: Alloys
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

The present inventions offer a nickel-based single crystal alloy which has a high strength, is easy in conducting the solution heat treatment, hardly gives a harmful phase and is resistant to corrosion at high temperature. A nickel-based single crystal alloy is offered where the composition consists of 7-15 of Co, 0.1-4 of Cr, 1-4 of Mo, 4-7 of W, 5.5-6.5 of Al, 5-7 of Ta, 4-5.5 of Re, 0-0.5 each of Hf and V, and 0-2 each of Ti and Nb in terms of % by weight and residual part substantially consists of Ni wherein said alloy may contain unavoidable impurities

## Claims

### Claim 1

A nickel-based single crystal alloy, characterized in that, the composition consists of 7-15 of Co, 0.1-4 of Cr, 1-4 of Mo, 4-7 of W, 5.5-6.5 of Al, 5-7 of Ta, 4-5.5 of Re, 0-0.5 each of Rf and V, and 0-2 each of Ti and Nb in terms of % by weight and residual part substantially consists of Ni where said alloy may contain unavoidable impurities.

### Claim 2 (depends on 1)

A nickel-based single crystal alloy according claim 1 wherein said alloy contains 10-14 of Co, 2-3 of Cr, 1.5-2.5 of Mo, 5-6.5 of W, 5.7-6.3 of Al, 5.5-6.5 of Ta, 4.5-5 of Re and 0.01-0.3 of Hf in terms of % by weight.

### Claim 3 (depends on 1, 2)

A method of manufacturing a nickel-based single crystal alloy mentioned in claim 1 or 2, characterized in that, a solution heat treatment is conducted at the temperature range of 1,310-1,350° C. and a aging heat treatment is conducted at the temperature range of 850-1,200° C.

### Claim 4 (depends on 3)

A method of manufacturing a nickel-based single crystal alloy according to claim 3 wherein the solution heat treatment is conducted within ten hours and the aging heat treatment is conducted within thirty hours.

### Claim 5 (depends on 3, 4)

A method of manufacturing the nickel-based single crystal alloy according to claim 3 or 4 wherein each of the solution heat treatment and the aging heat treatment is conducted in a single step or by means of temperature changes in two to four steps.

### Claim 6 (depends on 3, 4, 5)

A method of manufacturing the nickel-based single crystal alloy according to any of claims 3 to 5 wherein a preliminary heat treatment at from 1,290° C. to lower than 1,310° C. for two hours or shorter is conducted prior to the solution heat treatment.