# US 2001/0025090 A1 · Crystalline polypropylenes, process for preparing therof, polypropylene compositions, and thermoformed products

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0025090 A1
- Document ID: US20010025090A1
- Status: Published application
- Kind: A1
- Application number: 09/194,363
- Filed: 1998-11-25
- Published: 2001-09-27
- Earliest claimed: 1996-05-27
- Assignees: Mitsui Chemicals, Inc.
- Inventors: SATORU MORIYA; SHINYA MATSUNAGA; SHINICHI KOJOH; KENJI SUGIMURA; MASAHIRO KISHINE; NORIO KANESHIGE; MAMORU KIOKA; TERUHISA KOJIMA
- Web page: https://patentgrep.com/patent/US20010025090A1

## CPC

- C08F 4/6465: {containing silicium}
- C08F 4/651: Pretreating with non-metals or metal-free compounds
- C08F 4/6543: {halides of magnesium}
- C08F 110/06: Propene
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention presents crystalline polypropylenes that contain components insoluble in 64° C. decane that satisfy the following characteristics (1) to (4) and are excellent in hardness and rigidity, high in melt tension, and excellent in molding properties, process for preparing such crystalline polypropylenes, and polypropylene compositions and thermoformed products that contain such crystalline polypropylenes. (1) The intrinsic viscosity (η) (in 135° C. decalin) is 0.5 to 10 dl/g. (2) The molecular weight distribution (Mz/Mw) as determined by gel permeation chromatography (GPC; solvent: o-chlorobenzene, measurement temperature: 140° C.) is 5 or more. (3) The pentad isotacticity (mmmm percentage), which is a stereoregularity index determined by the measurement of the 13C-NMR spectrum, is 98% or more. (4) The D value, determined using formula (1) below from the loss tangents, tanδ0.05 and tanδ10 measured at the frequencies, 0.05 rad/sec and 10 rad/sec respectively by a melt viscoelasticity measuring device under a temperature of 230° C. and constant strain, and said loss tangent measurement frequencies, is 4.0 or more. 1 It is preferable for the number-average molecular weight Mn of the components insoluble in 64° C. decane to be 25000 or more.

## Claims

### Claim 1

A crystalline polypropylene characterized in that the components insoluble in 64° C. decane meet the following characteristics (1) to (4):
(1) The limiting viscosity (η) (in 135° C. decalin) is 0.5 to 10 dl/g,;
(2) the molecular weight distribution (Mz/Mw) as determined by gel permeation chromatography (GPC; solvent: o-chlorobenzene, measurement temperature: 140° C.) is 5 or more,;
(3) the pentad isotacticity (mmmm percentage), which is a stereoregularity index determined by the measurement of the 13C-NMR spectrum, is 98% or more; and
(4) the D value, determined using formula (1) below from the loss tangents, tanδ0.05 and tanδ10 measured at the frequencies, 0.05 rad/sec and 10 rad/sec, respectively, by a melt viscoelasticity measuring device under a temperature of 230° C. and constant strain, is 4.0 or more. 10

### Claim 2 (depends on 1)

A crystalline polypropylene as set forth in claim 1, wherein the number-average molecular weight Mn of the components insoluble in 64° C. decane is 25000 or more.

### Claim 3 (depends on 1)

A crystalline polypropylene as set forth in claim 1, which contains 60 wt. % or more of the above-described components insoluble in 64° C. decane.

### Claim 4 (depends on 1)

A crystalline polypropylene as set forth in claim 1, which contains a prepolymer as a nucleating agent.

### Claim 5 (depends on 1)

A crystalline polypropylene as set forth in claim 1, which is a homopolypropylene.

### Claim 6 (depends on 1)

A crystalline polypropylene as set forth in claim 1, which is a propylene block copolymer.

### Claim 7 (depends on 1)

A process for preparing the crystalline polypropylene of claim 1, said process being characterized in that propylene is polymerized by multiple-stages, optionally, along with another monomer in the presence of a catalyst for preparing highly stereoregular polypropylene.

### Claim 8 (depends on 7)

A process for preparing crystalline polypropylene as set forth in claim 7, wherein the multiple-stage polymerization is carried out in three stages,
wherein in the first stage crystalline polypropylene having an intrinsic viscosity (η) of 8 to 20 dl/g is produced at an amount corresponding to 0.5 to 15 wt. % of the finally obtained crystalline polypropylene,
in the second stage crystalline polypropylene ahving an intrinsic viscosity (η) of 3 to 10 dl/g is produced at an amount corresponding to 0.5 to 30 wt. % of the finally obtained crystalline polypropylene, and
in the third stage crystalline polypropylene,having an intrinsic viscosity (η) of 0.8 to 4.0 dl/g is produced at an amount corresponding to 99 to 55 wt. % of the finally obtained crystalline polypropylene.

### Claim 9 (depends on 7)

A prcoess for preparing crystalline polypropylene as set forth in claim 7, wherein the multiple-stage polymerization is carried out in two stages,
wherein in the first stage crystalline polypropylene having an intrinsic viscosity (η) of 8 to 20 dl/g is produced at an amount corresponding to 0.5 to 15 wt. % of the finally obtained crystalline polypropylene and
in the second stage crystalline polypropylene having an intrinsic viscosity (η) of 0.8 to 4.0 dl/g is produced at an amount corresponding to 99.5 to 85 wt. % of the finally obtained crystalline polypropylene.

### Claim 10 (depends on 1)

A process for preparing the crystalline polypropylene of claim 1, said process being characterized in that 0.5 to 15 wt. % of a crystalline polypropylene having an intrinsic viscosity (η) of 8 to 20 dl/g is blended with 99.5 to 85 wt. % of a crystalline polypropylene having an intrinsic viscosity (η) of 0.8 to 4.0 dl/g.

### Claim 11

A polypropylene composition comprising components soluble in 140° C. decane and, optionally, components insoluble in 140° C. decane, said polypropylene composition being characterized in that the components soluble in 140° C. decane that are also components insoluble in 64° C. decane comprising a crystalline polypropylene that satisfies the following characteristics (1) to (4):
(1) The intrinsic viscosity (η) (in 135° C. decalin) is 0.5 to 10 dl/g:
(2) the molecular weight distribution (Mz/Mw) as determined by gel permeation chromatography (GPC; solvent: o-chlorobenzene, measurement temperature: 140° C.) is 5 or more:
(3) the pentad isotacticity (mmmm percentage), which is a stereoregularity index determined by the measurement of the 13C-NMR spectrum, is 98% or more; and
(4) the D value, determined using formula (1) below from the loss tangents, tanδ0.05 and tanδ10 measured at the frequencies, 0.05 rad/sec and 10 rad/sec, respectively, by a melt viscoelasticity measuring device under a temperature of 230° C. and constant strain, and said loss tangent measurement frequencies, is 4.0 or more. 11

### Claim 12 (depends on 11)

A polypropylene composition as set forth in claim 11, wherein the number-average molecular weight of the components insoluble in 64° C. decane is 25000 or more.

### Claim 13 (depends on 11)

A polypropylene composition as set forth in claim 11, which contains 70 wt. % or more of the components soluble in 140° C. decane.

### Claim 14 (depends on 13)

A polypropylene composition as set forth in claim 13, wherein the components insoluble in 64° C. decane is included in an amount of 60 wt. % or more in the components soluble in 140° C. decane.

### Claim 15 (depends on 13)

A polypropylene composition as set forth in claim 13, wherein the components soluble in 64° C. decane of the component soluble in 140° C. decane comprise an ethylene/α-olefin copolymer.

### Claim 16 (depends on 13)

A polypropylene composition as set forth in claim 13, wherein the components soluble in 64° C. decane of the component soluble in 140° C. decane comprise a styrene copolymer.

### Claim 17 (depends on 11)

A polypropylene composition as set forth in claim 11, wherein the components insoluble in 140° C. decane comprise an inorganic filler selected from among talc, glass fiber, potassium titanate, and barium sulfate.

### Claim 18 (depends on 11)

A polypropylene composition as set forth in claim 11, whi ch contains a nucleating agent.

### Claim 19 (depends on 1)

A thermoformed product, which is formed of the crystalline polypropylene of claim 1.

### Claim 20 (depends on 11)

A thermoformed product, which is formed of the polypropylene composition of claim 11.