# US 2001/0025085 A1 · Aromatic vinyl resin material and molded products thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0025085 A1
- Document ID: US20010025085A1
- Status: Published application
- Kind: A1
- Application number: 09/773,904
- Filed: 2001-02-02
- Published: 2001-09-27
- Earliest claimed: 1997-10-24
- Assignees: Idemitsu Petrochemical Co., Ltd.
- Inventors: Hideo Teshima; Tomoaki Takebe; Masanori Sera
- Web page: https://patentgrep.com/patent/US20010025085A1

## CPC

- C08F 290/04: Polymers provided for in subclasses C08C or C08F
- C08F 290/044: {Polymers of aromatic monomers as defined in group C08F12/00}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

The present invention provides resin materials for producing molded products endowed with excellent heat resistance, solvent resistance, toughness, tensile elongation, and transparency. Specifically, there are provided aromatic vinyl resin materials which have the following properties: Storage elasticity values G′(1.0) and G′(0.1) as measured at 300° C., a strain γ of 20%, and a frequency of 1.0 Hz or 0.1 Hz satisfy the expression, log[G′(1.0)/G′(0.1)]≦0.6, the heat of fusion ΔH as measured over the range 200-295° C. is 8 to 50 (J/g), and the 1H-NMR peak integrated values for the fraction corresponding to the temperature range of not lower than 50° C., as collected from temperature rising election fraction on the Soxhlet extraction residue by use of cyclohexane or o-dichlorobenzene, satisfy the relation [1.8-2.1 (ppm)]/[1.0-1.7(ppm))<0.49.

## Claims

### Claim 1

An aromatic vinyl resin material which satisfies the relationship represented by the following expression:
SG value=log[G′(1.0)/G′(0.1)]<0.6
wherein G′(1.0) is a storage modulus as measured at a temperature of 300° C., a strain γ of 20%, and a frequency of 1.0 Hz, and G′(0.1) is a storage modulus as measured at a temperature of 300° C., a strain γ of 20%, and a frequency of 0.1Hz.

### Claim 2

An aromatic vinyl resin material having the following properties;
1) the heat of fusion ΔH as measured over the range 200-295° C. with a differential scanning calorimeter is 8 to 50 (J/g),
2) in 1H-NMR performed on the residue obtained from Soxhlet extraction using cyclohexane,
B/A<0.49
wherein A is an integrated value of a peak appearing at 1.0-1.7 (ppm) and B is an integrated value of a peak appearing at 1.8-2.1 (ppm), and
3) a tensile elongation of not less than 5%.

### Claim 3

An aromatic vinyl resin material having the following properties:
1) the heat of fusion ΔH as measured over the range 200-295° C. with a differential scanning calorimeter is 8 to 50 (J/g),
2) in 1H-NMR performed on the fraction eluted at 50° C. or higher through temperature rising election fraction by use of o-dichlorobenzene (hereinafter referred to simply as fractionation by o-dichlorobenzene), B/A<0.49 wherein A is an integrated value of a peak appearing at 1.0-1.7 (ppm) and B is an integrated value of a peak appearing at 1.8-2.1 (ppm), and
3) a tensile elongation of not less than 5%.

### Claim 4 (depends on 1)

An aromatic vinyl resin material according to claim 1, which is a graft copolymerization product of an aromatic vinyl monomer (a) and an ethylene copolymer macromer (b).

### Claim 5 (depends on 2)

An aromatic vinyl resin material according to claim 2, which is a graft copolymerization product of an aromatic vinyl monomer (a) and an ethylene copolymer macromer (b).

### Claim 6 (depends on 3)

An aromatic vinyl resin material according to claim 3, which is a graft copolymerization product of an aromatic vinyl monomer (a) and an ethylene copolymer macromer (b).

### Claim 7 (depends on 4)

An aromatic vinyl resin material according to claim 4, wherein the ethylene copolymer macromer (b) is a copolymerization product of ethylene, a diene monomer, and an optional aromatic vinyl monomer and optional α-olefin.

### Claim 8 (depends on 1)

An aromatic vinyl resin material as described above in claim 1, which has a composition composed of (A) an aromatic vinyl polymer, (B) an ethylene copolymer having a diene-monomer-derived vinyl group in the molecular chain, and (C) a graft copolymerization product of an aromatic vinyl monomer (a) and an ethylene copolymer macromer (b).

### Claim 9 (depends on 4)

An aromatic vinyl resin material according to claim 4, in which a moiety derived from an aromatic vinyl monomer predominantly has a syndiotactic structure.

### Claim 10 (depends on 5)

An aromatic vinyl resin material according to claim 5, in which a moiety derived from an aromatic vinyl monomer predominantly has a syndiotactic structure.

### Claim 11 (depends on 6)

An aromatic vinyl resin material according to claim 6, in which a moiety derived from an aromatic vinyl monomer predominantly has a syndiotactic structure.

### Claim 12 (depends on 7)

An aromatic vinyl resin material according to claim 7, in which a moiety derived from an aromatic vinyl monomer predominantly has a syndiotactic structure.

### Claim 13 (depends on 8)

An aromatic vinyl resin material according to claim 8, in which a moiety derived from an aromatic vinyl monomer predominantly has a syndiotactic structure.

### Claim 14 (depends on 1)

An aromatic vinyl resin material having a composition composed of an aromatic vinyl resin material according to claim 1 and a styrene polymer predominantly having a syndiotactic structure and/or a rubber-like elastic substance.

### Claim 15 (depends on 1)

A molded product obtained through molding of an aromatic vinyl resin material as described in claims 1.