# US 2001/0025074 A1 · Long fiber-reinfoced polypropylene resin composition and molded article

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0025074 A1
- Document ID: US20010025074A1
- Status: Published application
- Kind: A1
- Application number: 09/794,127
- Filed: 2001-02-28
- Published: 2001-09-27
- Earliest claimed: 2000-03-01
- Assignees: Chisso Corporation; Chisso Petrochemical Corporation
- Inventors: Koichi Saito; Toshimori Nakai; Nobukazu Atsumi; Hitoshi Kuramochi
- Web page: https://patentgrep.com/patent/US20010025074A1

## CPC

- C08L 23/10: Homopolymers or copolymers of propene
- C08J 5/10: characterised by the additives used in the polymer mixture
- C08K 3/22: of metals
- C08K 7/14: Glass
- C08L 23/12: Polypropene
- C08L 23/142: {at least partially crystalline copolymers of propene with other olefins}
- C08L 51/06: grafted on to homopolymers or copolymers of aliphatic hydrocarbons containing only one carbon-to-carbon double bond
- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C08J 2323/12: Polypropene
- C08L 2205/16: Fibres; Fibrils
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

Provided is a long fiber-reinforced polypropylene resin composition which provides a molded article excellent in a mechanical strength and an impact resistance and having a small anisotropy in a strength, so that it can suitably be used even for uses in medium-sized to large-sized molded articles. The long fiber-reinforced polypropylene resin composition comprises 40 to 85% by weight of (A) a long fiber-reinforced propylene homopolymer pellet shown below and 15 to 60% by weight of (B) a propylene base block copolymer resin having the MFR of 50 g/10 min or less: (A): a long fiber-reinforced propylene homopolymer pellet comprising, (A1): 20 to 64.9% by weight of a modified propylene homopolymer obtained by modifying a propylene homopolymer with unsaturated carboxylic acid or an anhydride thereof or a mixture of the above modified propylene homopolymer and an unmodified propylene homopolymer, wherein an MFR is 60 g/10 min or more, (A2): 0.1 to 5% by weight of at least one selected from the group consisting of simple substances, hydroxides and oxides of alkaline earth metals, and (A3): 35 to 75% by weight of glass long fiber having a length of 2 to 50 mm.

## Claims

### Claim 1

A long fiber-reinforced polypropylene resin composition comprising 40 to 85% by weight of (A) a long fiber-reinforced propylene homopolymer pellet shown below and 15 to 60% by weight of (B) a propylene base block copolymer resin having a melt flow rate (230° C, 21.18 N; hereinafter abbreviated as MFR) of 50 g/10 min or less:
(A): a long fiber-reinforced propylene homopolymer pellet comprising,
(A1): 20 to 64.9% by weight of a modified propylene homopolymer obtained by modifying a propylene homopolymer with unsaturated carboxylic acid or an anhydride thereof or a mixture of the above modified propylene homopolymer and an unmodified propylene homopolymer, wherein the MFR is 60 g/10 min or more,
(A2): 0.1 to 5% by weight of at least one selected from the group consisting of simple substances, hydroxides and oxides of alkaline earth metals, and
(A3): 35 to 75% by weight of glass long fibers having a length of 2 to 50 mm.

### Claim 2 (depends on 1)

The long fiber-reinforced polypropylene resin composition as described in claim 1, wherein (A1) the modified propylene homopolymer obtained by modifying the propylene homopolymer with the unsaturated carboxylic acid or the anhydride thereof or the mixture of the above modified propylene homopolymer and the unmodified propylene homopolymer has an MFR of 100 g/10 min or more, and (B) the propylene base block copolymer resin has an MFR of 35 g/10 min or less.

### Claim 3 (depends on 1, 2)

The long fiber-reinforced polypropylene resin composition as described in claim 1 or 2, wherein (B) the propylene base block copolymer resin is a high rigid propylene-ethylene block copolymer resin comprising a propylene homopolymer part having an isotactic pentad rate of 0.96 or more and an Mw/Mn (Q value) of 6 or less, and a propylene-ethylene copolymer part.

### Claim 4 (depends on 3)

The long fiber-reinforced polypropylene resin composition as described in claim 3, wherein (B) the propylene base block copolymer resin contains 0.0001 to 1% by weight of a nucleating agent based on the propylene base block copolymer resin.

### Claim 5 (depends on 1, 2)

A molded article obtained by molding the long fiber-reinforced polypropylene resin composition as described in claim 1 or 2.

### Claim 6 (depends on 5)

The molded article as described in claim 5, wherein the glass long fibers contained in the molded article originating in the long fiber-reinforced propylene homopolymer pellet have a residual average fiber length of 1 mm or more.