# US 2001/0025072 A1 · Purging agent and purging method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0025072 A1
- Document ID: US20010025072A1
- Status: Published application
- Kind: A1
- Application number: 08/877,878
- Filed: 1997-06-18
- Published: 2001-09-27
- Earliest claimed: 1996-06-18
- Assignees: Kuraray Co., Ltd.
- Inventors: TAICHI NEGI; SYUKITI KAWAMURA; HIROMICHI NAKANO; SATOSHI HIROFUJI
- Web page: https://patentgrep.com/patent/US20010025072A1

## CPC

- B29C 48/27: Cleaning; Purging; Avoiding contamination
- B29C 48/08: flexible, e.g. films
- B29C 48/10: flexible, e.g. blown foils
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A purging agent which contains an ethylene-vinyl alcohol copolymer and which satisfies the conditions specified by the equations (1) and (2) below: 20≧BT(120)≧0.1 (1) 500≧BT(250)/BT(120)≧1.5 (2), where BT(120) is weight loss (%) on heating in nitrogen at 120° C. for 24 hours, and BT(250) is weight loss (%) on heating in nitrogen at 250° C. for 6 hours, rapidly discharges residual thermoplastic resin containing EVOH from molding equipment, and also rapidly discharges itself when a fresh resin is fed again to the equipment. This leads to a remarkable reduction in loss due to residual purging agent. In addition, the purging agent causes only a small amount of resin to stick to the equipment, even after repeated purging. After purging, it is possible to restore normal operation within a short period of time.

## Claims

### Claim 1

A purging agent comprising an ethylene-vinyl alcohol copolymer,
wherein said purging agent has a value of BT(120) of 0.1-20, and a ratio of BT(250)/BT(120) of 1.5-500.

### Claim 2 (depends on 1)

The purging agent of claim 1, wherein said purging agent has a content of 0.1-20 wt % of water, an alcohol or a polyhydric alcohol.

### Claim 3 (depends on 1)

The purging agent of claim 1, further comprising an inorganic powder in an amount of 0.01-20 wt %.

### Claim 4 (depends on 2)

The purging agent of claim 2, wherein said purging agent has a content of 0.1-20 wt % of water.

### Claim 5 (depends on 1)

The purging agent of claim 1, further comprising a salt selected from alkaline metal salts, alkaline earth metal salts, and mixtures thereof, in an amount of 0.0005-0.5 wt % in terms of the amount of metal.

### Claim 6 (depends on 5)

The purging agent of claim 5, wherein said salt is selected from the group consisting of carboxylates, phosphates, carbonates, chlorides and mixtures thereof.

### Claim 7 (depends on 3)

The purging agent of claim 3, wherein said inorganic powder is selected from the group consisting of oxides, hydroxides and chlorides of silicon, aluminum, iron, copper, cobalt and manganese; and mixtures thereof.

### Claim 8 (depends on 1)

The purging agent of claim 1, wherein said purging agent has a value of BT(120) of 1.0-5.

### Claim 9 (depends on 1)

The purging agent of claim 1, wherein said purging agent has a ratio of BT(250)/BT(120) of 3-300.

### Claim 10 (depends on 1)

The purging agent of claim 1, wherein said purging agent has a value of BT(120) of 1.0-5, and a ratio of BT(250)/BT(120) of 3-300,
said purging agent has a water content of 1.0-5 wt %,
said purging agent further comprises an inorganic powder selected from the group consisting of oxides, hydroxides, and chlorides of silicon, aluminum, iron, copper, cobalt and manganese; and mixtures thereof; in an amount of 0.02-10 wt %

### Claim 11 (depends on 1)

A method of purging residual thermoplastic resin from a melt passage of an extruder after extrusion molding comprising:
passing the purging agent of claim 1 through said melt passage.

### Claim 12 (depends on 10)

A method of purging residual thermoplastic resin from a melt passage of an extruder after extrusion molding comprising:
passing the purging agent of claim 10 through said melt passage.

### Claim 13

A method of making a purging agent comprising:
mixing an ethylene-vinyl alcohol copolymer with a composition comprising a compound having a boiling point lower than 300° C.
wherein said purging agent has a value of BT(120) of 0.1-20, and a ratio of BT(250)/BT(120) of 1.5-500.

### Claim 14 (depends on 13)

The method of claim 13, further comprising incorporating into said copolymer, before, after, or simultaneously with said mixing, a metal salt in an amount of 0.005-0.5 wt %, in terms of said metal.

### Claim 15 (depends on 13)

The method of claim 13, wherein said compound having a boiling point lower than 300° C. is water, and said water is present in an amount of 1.0-20 wt %.

### Claim 16 (depends on 13)

The method of claim 13, wherein said composition further comprises a carrier which has absorbed said compound having a boiling point lower than 300° C.

### Claim 17 (depends on 14)

A product produced by the process of claim 14.

### Claim 18 (depends on 1)

A method of extrusion, comprising:
extruding a first ethylene-vinyl alcohol copolymer with an extruder; followed by
purging said extruder with the purging agent of claim 1; followed by:
extruding a second ethylene-vinyl alcohol copolymer with said extruder.

### Claim 19 (depends on 10)

A method of extrusion, comprising:
extruding a first ethylene-vinyl alcohol copolymer with an extruder; followed by
purging said extruder with the purging agent of claim 10; followed by:
extruding a second ethylene-vinyl alcohol copolymer with said extruder.

### Claim 20 (depends on 18)

The method of claim 18, where said first ethylene-vinyl alcohol copolymer and said second ethylene-vinyl alcohol copolymer have the same composition.